Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (3): 54-152    DOI:
Current Issue | Archive | Adv Search |
THE SEM IN SITU OBSERVATION OF TENSILE FRACTURE PROCESSES IN PLAIN CARBON DUAL-PHASE STEELS
SHEN Xianpu;LEI Tingquan;LIU Jianzhuang Harbin Institute of Technology
Cite this article: 

SHEN Xianpu;LEI Tingquan;LIU Jianzhuang Harbin Institute of Technology. THE SEM IN SITU OBSERVATION OF TENSILE FRACTURE PROCESSES IN PLAIN CARBON DUAL-PHASE STEELS. Acta Metall Sin, 1985, 21(3): 54-152.

Download:  PDF(4700KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamic microprocesses of fracture in martensite-ferrite dual-phase steelswere observed by the in situ technique in SEM equipped with tensile platform.The mechanism of crack nucleation has been clarified.The conditions of crack prop-agation and affecting factors have been discussed.It is believed that the propaga-tion of the microcracks depends on the combined effect of both tensile stress andplastic shear strain.The dislocation pile-up model can be successfully used for ex-plaining the effect of the volume fraction of martensite,the carbon content in itand the low temperature tempering on crack nucleation.Furthmore,the factorsaffecting the ductility of dual-phase steels were analyzed according to the specificfeatures of fracture processes.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/54

1 Rashid,M.S.,Formable HSLA and Dual-Phase Steel,Ed.Davenport,A.T.,TMS-AIME,New York,1977,p.1.
2 Speich,G.R.;Miller,R.L.,Structure and Properties of Dual-Phase Steel,Eds.Kot,R.A.;Morris,J.W.,TMS-AIME,New York,1979,p.145.
3 Gerbase,J.;Emburry,J.D.;Hobbs,R.M.,ibid.,p.118.
4 Korzekwa,D.A.;Lawson,R.D.;Matlock,D.K.;Krauss,G.,Scr.Metall.,11(1980) ,1023.
5 Szewzyk,A.F.;Gurland,J.,Metall.Trans.,13A(1982) ,1821.
6 雷廷权;沈显璞;潘杰,钢铁,18(1983) ,№7,46.
7 雷廷权;沈显璞,金属学报,18(1982) ,75.
8 Kim,N.J.;Thomas,G.,Metall.Trans.,12A(1981) ,483.
9 Stevenson,R.,Formable HSLA and Dual-Phase Steel,Ed.Davenport,A.T.,TMS-AIME New York 1977,p.99.
10 徐永波;刘民治,金属学报,18(1982) ,58.
11 Tamura,I.;Tomota,Y.;Akao,A.;Yamaoka,Y.;Ozawa,M.;Kanoton,S.,Trans.Iron Steel Inst.Jpn,13(1973) ,283.
12 Davies,R.G.,Metall.Trans.,9A(1978) ,671.
13 Marder,A.R.;Bramfitt,B.L.,Structure and Properties of Dual-Phase Steel,Eds.Kot,R.A.;Morris,J.W.,TMS-AIME,New York,1979,p.242.
14 Stroh,A.N.,Proc.Phys.Soc.,B66(1953) 1.
15 哈宽富,金属力学性质的微观理论,科学出版社,1983,p.33.
16 Lei,T.C.(雷廷权);Shen,H.P.(深显璞),Paper Presented at the Fourth Risoe Int.Symp.on Metallurgy and Materials Science,Denmark,5-9 Sept.1983.
17 Araki K.;Takada,Y.;Nakaoka,K.,Trans.Iron Steel Inst.Jpn,17(1977) ,710.6
No related articles found!
No Suggested Reading articles found!