THE ELECTRONIC STRUCTURE OF AMORPHOUS ALLOYS Ni-P AND Pd-Ni-P
FENG Pingyi;CHEN Nianyi Shanghai Institute of Metallurgy;Academia Sinica;YU Zhizhong Shanghai Institute of Testing Technics;LIAO Muzhen;GUO Jinliang Tsinghua University;Beijing
Cite this article: 

FENG Pingyi;CHEN Nianyi Shanghai Institute of Metallurgy;Academia Sinica;YU Zhizhong Shanghai Institute of Testing Technics;LIAO Muzhen;GUO Jinliang Tsinghua University;Beijing. THE ELECTRONIC STRUCTURE OF AMORPHOUS ALLOYS Ni-P AND Pd-Ni-P. Acta Metall Sin, 1985, 21(3): 106-114.

Download:  PDF(641KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The study of electronic structure for amorphous alloys Ni-P and Pd-Ni-P wasmade by X-ray photoemission,Auger electron spectroscopy and quantum chemicalcalculation.It was shown that the s and p orbitals on the P atom combinedwith the s and d orbitals of Ni and Pd atoms to form bonding molecular orbit-als(MO).This leads a drop of the den sity ofstates near the Fermi level.Thechanges of band structure are obvious.The“rigid band-charge transfer model”which was used to explain the variation of magnetic and nuclear magnetic prop-erties of amorphous alloys such as Ni-P and Pd-Ni-P seems to be unreliable.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/106

1 Polk,D.E.,Scr.Metall.,4(1970) ,117.
2 Hasegawa,R,;Hines,W.A.;Kabacoff,L.E.;Duwez,P.,Solid State Commun.,20(1976) ,1035.
3 O' Handley,R.C.;Boudreaux,D.S.,Phys.Status Solidi,(a)45(1978) ,607.
4 Hines,W.A.;Kabacoff,L.T.;Hasegawa,R.;Duwez,P.,J.Appl.Phys.,49(1978) ,1724.
5 Fuggle,J.C.,Phys.Rev.,B 27(1983) ,2145.
6 Amamou,A.;Krill,G.,Solid State Commun.,33(1980) ,1087.
7 Bakonyi,I.;Kovacs,I.;Varga,L.;Bagi.T.;Lovas,A.;Tothkader,E.;Tompa,K.,Proc.of the Conf.on Metallic Glasses Science and Technology(Budapest,1980) .
8 Hines.W.A.,Solid State Commun.,39(1981) ,699.
9 Binder,H.;Fluck,E.,Modern Physics in Chemistry,Vol.2,Eds.Fluck,E.;Goldanskii,V.I.,Academic Press,London,1979,p.321.
10 Messmer,R.P.,Phys.Rev.,B 23(1981) ,1616.
11 Hasegawa,R.;O' Handley,R.C.;Mendelson,L.I.,Magnetism and Magnetic Materials,AIP.Conf.Proc.№34,AIP.Publ.,New York,1976,p.298.
12 Hines.W.A.;Lawrence,T.;Kabacoff,L.E.;Hasegawa,R.;Duwez,P.,Amorphous Magnetism,II,Eds.Levy,R.A.;Hasegawa,R.,Plenum Press,New York,1977,p.207.
13 Hines,W.A.;Modzelewski,C.U.;Paolino,R.N.;Chen,H.S.,J.Appl.Phys.,52(1981) ,1814.
14 Hines,W.A.;Clover,K.;Clark,W.G.;Kabacoff,L.T.;Modzelewski,C.U.;Hasegawa,R.;Duwez,P.,Phys.Rev.,B 21(1980) ,3771.
No related articles found!
No Suggested Reading articles found!