THE PARAMAGNETISM-ANTIFERROMAGNETISM TRANSITION OF γ-Fe-Mn-Al-Cr ALLOYS
Cite this article: 

THE PARAMAGNETISM-ANTIFERROMAGNETISM TRANSITION OF γ-Fe-Mn-Al-Cr ALLOYS. 0412-1961. Acta Metall Sin, 1985, 21(4): 35-44.

Download:  PDF(727KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ZHANG Yansheng Institute of Metal Research,Academia Sinica,Shenyang
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/35

1 Fujimori,H.,J.Phys.Soc.Jpn.,21(1966) ,1860.
2 Umebayashi,H.;Ishikawa,Y.,ibid.,21(1966) ,1281.
3 Ishikawa,Y.,Endoh,Y.,ibid.,23(1967) ,205.
4 Hashimoto,T.;Ishikawa,Y.,ibid.,23(1967) ,213.
5 Endoh,Y.;Ishikawa,Y.,ibid.,30(1971) ,1614.
6 Kreachter,H.;Pepperhoff,W.,Arch.Eisenhuettenwes.,39(1968) 541.
7 Shiga,M.,J.Phys.Soc.Jpn.,22(1967) ,539.
8 Hayase,M.;Shiga,M.;Nakamura,Y.,ibid.,30(1971) ,729.
9 张彦生,苏丽娟,金属学报,19(1983) ,A253.
10 张彦生,金属学报,19(1983) ,A262.
11 张彦生,中国金属学会1979-1980年优秀论文选集,第三分册,中国金属学会编,冶金工业出版社,1984年,p.221.
12 张彦生,金属学报,20(1984) ,A313
13 Ohno,H.;Mekata,M.,J.Phys.Soc.Jpn.,31(1971) 102.
14 Sato,H.;Assott,A.,Phys.Rev.,114(1959) ,1420.
15 Sato,H.;Assott,A.,ibid.,114(1959) ,1427.
16 Anderson,P.W.,Phys.Rev.,79(1950) ,350.
17 Anderson,P.W.,ibid.,80(1950) ,922.
18 Warnes,L.A.A.;King,H.W.,Cryogenics,16(1976) ,659.
19 Ledbetter,H.M.;Weston,W.F.;Kaimon,E.R.,J.Appl.Phys.,46(1975) ,3855.
20 Doering,W.,Am.Phys.(Leipz),32(1938) ,465.
21 Hausch,G.;Warlimont,H.,Z.Metallk.,63(1972) ,547.
22 Maeda,T.,J.Phys.Soc.Jpn.,30(1971) ,375.
23 Benkisser,G.,Neue Huette,17(1972) ,475.
24 Shiga,M.;Nakamura,Y.,J.Phys.Soc.Jpn.,26(1969) ,24.
25 Asano,S.;Yamashita,J.,ibid.,31(1971) ,1000.
No related articles found!
No Suggested Reading articles found!