EFFECT OF VANADIUM ON ORDERING PHASE SEPARATION IN Fe-Si ALLOY
by WANG Shidao Lanzhou Railway Institute; DAI Lizhi L. C. Tai Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

by WANG Shidao Lanzhou Railway Institute; DAI Lizhi L. C. Tai Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. EFFECT OF VANADIUM ON ORDERING PHASE SEPARATION IN Fe-Si ALLOY. Acta Metall Sin, 1985, 21(6): 15-110.

Download:  PDF(3042KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The alloying element V has remarkable influence on the ordering phase sepa-ration in the Fe-Si alloy containing 6.5 wt-%Si. The behaviour of V was inves-tigated by magnetic method, X-ray diffraction and electron microseopy. It wasfound that an addition of less amout of V may relax the ordering phase sepa-ration and improve the ductility and magnetic properties of the alloy. An A_2+DO_3 ordering phase separation was observed in the 11.57 at.-%Si-Fe alloy con-taining more V, namely, 0.88 at.-%. Discussion has been made of the effect ofV on the ordering phase separation in the Fe-Si alloy on the basis of analysisof thermodynamic data of three binary alloys of Fe-Si, Fe-V and V-Si.
Received:  18 June 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I6/15

1 Bozorth, R. M., Ferromagnetism, Van Norstrad. New York. 1952, Chap. 2.
2 倪志康;刘玉志,精密合金文集,上海科学技术出版社,1980,p.128.
3 Kernic, A.; Lance. D. H.; Ogden. J. W.; Povlovic. D. M., J Appl. Phys., 38(1967) . 1087.
4 Shewmon. P G., Physical Chemistry in Metallurgy. Proc. of the Conf. Aug. 1976, Eds. Fisher. R. M.; Oriani, R.A.; Turkdogan. E. T. USA Res. Lab., Monroeville. Pa., 1976, p. 375.
5 王世道,戴礼智,钢铁研究总院学报,3(1983) ,341。
6 Lakso, G. E.; Marcinkovski, M. J., Metall, Trans., 5(1974) . 839.
7 43 (1979) . 1415.
8 36 (1973) . 652.
9 Narita. K.; Enokizono, M., IEEE Trans. Magn., MAG-14 (1978) , 258.
10 Navweps Report 7331美国海军武器试验室,国外软磁材料(硅钢及其他软磁材料),上海科技出版社,1973.
11 Stoloff, N.S., Strengthenning Methods in Crystals, Eds. Kelly. A.; Nicholson,R. B., Elsevier Publ, Amsterdam,1971,p.193.
12 Crawford, R.C., Philos Mag., 35(1977) ,567.
13 Beck, P. A., Metall. Trans., 2(1971) , 2015.
14 Swann, P. R.; Granas, L.; Lehtinen, B., Met. Sci., 9(1975) , 90.
15 Thomas, G.; Goringe, M. J., Transmission Electron Microscopy of Materials, Wiley-Interscience Publ. New York, 1979, p. 100.
16 Inden, G.; Pitsch, W., Z. Metallk., 62(1971) ,627.
17 Schlatte, G.; Inden, G.; Pitsch, W., Z. Metallk., 65(1974) ,94.
18 Inden, G.; Z. Metallk, 66(1975) , 577.
19 Kubashewski, O.; Catterall, J. A., Thermochemical Data of Alloys. Pergamon Press, London, 1956, p. 54, 194.
20 Hultgren, R.; Desal, P.D.; Hawkins. D. T.; Gleiser, M.; Kelley, K. K., Setected Values of the Thermodynamic Properties of Binary Alloys, ASM, Metal Park, Ohio, 1973,p. 871, 896.
21 Devereux,O.F., Topics in Metallurgical Thermodynamics, Wiley-Interscience, Publ. New York, 1983, p. 137.
No related articles found!
No Suggested Reading articles found!