| EFFECT OF Ce ON PREFERRED ORIENTATION OF GRAIN IN OXIDE SCALE ON Fe-15Cr ALLOY |
| by GAO Huaisun;LI Bei Baotou Research Institute of Metallurgy |
|
Cite this article:
by GAO Huaisun;LI Bei Baotou Research Institute of Metallurgy. EFFECT OF Ce ON PREFERRED ORIENTATION OF GRAIN IN OXIDE SCALE ON Fe-15Cr ALLOY. Acta Metall Sin, 1985, 21(6): 44-49.
|
|
|
Abstract Study was made of the effect of addition of 0.3% Ce on the preferred ori-entation of grains in oxide scale formed on Fe-15Cr alloy at elevated temperatureby the inverse-pole-figure method. The main orientation is (101 10)_⊥, (1014)_⊥,(1126)_⊥ or (1014)_⊥, (1126)_⊥, (0112)_⊥ for the alloy containing or not respectively.The Ce was found to be accumulated at the interface between the oxide scale andalloy. The presence of Ce appears to have an improving effect over the oxidationresistance of the alloy owing to enhancing and keeping the preferred orientationof grains in oxide scale.
|
|
Received: 18 June 1985
|
1 Wood, G. C.; Boustead, J., Corros. Sci., 8 (1968) , 719. 2 Nagai H.; Okabayashi, M.; Mitani, H., Trans. Jpn Inst Met., 21 (1980) , 341. 3 天野忠昭;矢岛圣使;木村孝;齐藤安俊,防食技术,24(1975) ,19. 4 Stringer, J., Oxid. Met.,5(1972) ,11. 5 李陪;颜玉新;高怀荪;中国腐蚀防护学报,5(1985) ,(待发表). 6 Mueller, M. H.; Chernock, W. P.; Beck, P. A., Trans. Metall. Soc. AIME., 212 (1958) , 39. 7 Klug, H. D.; Alexander, L. E., X-Ray Diffraction Procedure for Poly Crystalline and Amorphous, 2nd ed., Wiley, New York, 1974,p. 360. 8 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸,金属学报,17(1981) ,233. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|