TOPOLOGICALLY CLOSE-PACKED PHASES IN SUPERALLOYS: New Phases and Domain Structures
YE Hengqiang; LI Douxing; GUO Kexin (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

YE Hengqiang; LI Douxing; GUO Kexin (Institute of Metal Research; Academia Sinica; Shenyang). TOPOLOGICALLY CLOSE-PACKED PHASES IN SUPERALLOYS: New Phases and Domain Structures. Acta Metall Sin, 1986, 22(1): 1-43.

Download:  PDF(17580KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  1 Introduction2 Description of topologically close-packed structures2.1 Coordination polyhedra2.2 Atom layers2.3 Structure units2.4 Classification of phases3 Experimental high-resolution electron microscopy3.1 Preparation of specimens3.2 Imaging conditions of HREM images3.3 Micro and convergent beam electron diffraction4 New topologically close-packed metallic phases4.1 σ-related new phases: H, F, K, J phases4.2 Laves-related new phases: C, C_1 phases4.3 Summary5 Microdomain structures5.1 Domain structures in o-related phases: translation domain boundaries- {100}σ, {110}σ, {1(?)0}_H. (001)_H, boundary joints; rotation domains——28°-σ, 28°-H5.2 Domain structures in Laves-related phases: translation domain boundaries-(001)_μ, (001)_L, ((?)1)_L, (111)_μ, ((?)2)_μ, boundary joints; rotation domains; domains in C phase6 Antiprisms with long-range orientational order7 Conclusions
Received:  18 January 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I1/1

1 Bain, F.C.; Griffith, A.A., Trans. AIME, 75 (1927) , 166.
2 Friauf, J.B., J. Am. Chem. Soc., 49 (1927) , 3107. Phys. Rev., 29 (1927) , 34.
3 Laves, F.; Lochberg, K., Nachr. Ges. Wiss, Goettingen, Math. Phys. Kl. Fachgruppe 4, 1, (1934) , No. 6, 59.
4 Arnfelt, H.; Westgren, A., Jernkontorets Ann., 119 (1935) , 185.
5 Shoemaker, D. P; Bergman, B.G., J. Am. Chem. Soc., 72 (1950) , 5793.
6 Rideout, S.; Manly, W.D.; Kamen, E.L.; Lement, B.S.; Beck, P.A., Trans. AIME, 191 (1951) , 872.
7 Shoemaker, D.P.; Shoemaker, C.B.; Wilson, F.C., Acta Cryst., 10 (1957) , 1.
8 Komura, Y.; Sly, W.G.; Shoemaker, D.P., Acta Cryst., 13 (1960) , 575.
9 Shoemaker, C.B.; Shoemaker, D.P., Acta Cryst., 16 (1963) , 997.
10 Shoemaker, C.B.; Shoemaker, D.P., Acta Cryst., 23 (1967) , 231.
11 Hartmann, H.; Fbert, F.; Bretsehneider, O., Z. Anorg, Allg, Chem., 198 (1931) , 116.
12 Wilson, C.G.; Thomas, D.K.; Spooner, F.J., Acta Cryst., 13 (1960) , 56.
13 Frank, F.C.; Kasper, J.S., Acta Cryst., 11 (1958) , 184.
14 Frank, F.C.; Kasper, J.S., Acta Cryst., 12 (1959) , 483.
15 Shoemaker, C.B.; Shoemaker, D.P., Developments in the Strtctural Chemistry of Alloy Phases, ed. Giessen, B.C., Plenum Press, New York, 1969, P. 107.
16 Andersson, S., J. Solid State Chem., 23 (1978) , 191.
17 Marcinkowski, M.J.; Miller, D.S., Philos. Mag., 7 (1962) , 1025.
18 Yagisawa, K.; Fujita, H., Jpn. J. Appl. Phys., 6 (1967) , 827.
19 Allen, C.W.; Delavignette, D.; Amelinckx, S., Phys. Status Solidi (a), 9 (1972) , 237.
20 Stenberg, L.; Andersson, S., J. Solid State Chem., 28 (1979) , 269.
21 Hirabayashi, M., Trans. Jpn. Inst. Metals, 24 (1983) , 315.
22 Komura, Y.; Takeda, S.; Takata, M., Trans. Jpn. Inst. Met., 24 (1983) , 413.
23 Ishimasa, T.; Kitano, Y.; Komura, Y., J. Solid State Chem., 36 (1980) , 74.
24 Ishimasa, T., Kitano, Y.; Komura, Y., Phys. Status Solidi (a) 66 (1981) , 703.
25 Kitano, Y.; Komura, Y.; Kajiwara, H.; Watanabe, E., E., Acta Cryst., A36 (1980) , 16.
26 Stenberg, L., Chem. Scr., 14 (1978/79) , 219.
27 Li, D.X. (李斗星); Stenberg, L.; Andersson, S., J. Solid State Chem., 48 (1983) , 368.
28 Li, D.X. (李斗星); Stenberg, L.; Andersson, S., unpublished work.
29 Hiraga, K.; Yamamoto, T.; Hirabayashi, M., Trans. Jpn. Inst. Met., 24 (1983) , 421.
30 Kasper, J.S., Theory of Alloy Phases, Am. Soc. of Metals Symposium, 1956, p. 264.
31 Pearson, W.B., The Crystal Chemistry and Physics of Metals and Alloys, Wiley-Interscience, New York, p. 44.
32 Sinha, A.K., Topologically close-packed structures of transition metal alloys, Pergamon Press, New York, 1972, p. 81.
33 Ye, H. Q.(叶恒强);Li, D. X.(李斗星);Kuo, K. H.(郭可信),Acta Cryst.,B40 (1984) ,461.
34 Ye, H. Q.(叶恒强);Kuo, K. H.(郭可信),Philos. Mag.,A50 (1984) .117.
35 Li. D. X.(李斗星);Kuo, K. H.(郭可信),Acta Cryst.,B40 (1985) .
36 Bardos, D.I.; Beck, P.A., Trans. Metall. Soc. AIME 236 (1966) , 64.
37 #12
38 Ye, H. Q.(叶恒强);Wang. D. N.(王大能);Kuo. K. H.(郭可信),Proc. of the 3rd APEM, Singapore, 1984,p.170.
39 #12
40 Shoemaker, C.B., Acta Cryst., B39 (1983) , 654.
41 Shoemaker, C.B.; Shoemaker, D.P., Acta Cryst., 23 (1967) , 231.
42 Ishizuka, K., Acta Cryst., A38 (1982) , 773.
43 Cowley, J.M., Diffraction Physics, Amsterdam, North-Holland, (1975) p. 3.
44 Spence, J.H.C., Experimental High-resolution Electron Microscopy, Clarondon Press, Oxford, 1981 p. 250.
45 Ye, H. Q.(叶恒强);Li, D. X.(李斗星);Kuo, K. H.(郭可信),Philos. Mag..A51 (1985) ,829.
46 Ye, H. Q.(叶恒强);Zhang, Z.(张泽);Kuo, K. H.(郭可信),Phys.Status Solidi(a),83 (1984) .77.
47 郭可信,电子显微镜学报,2 (1982) .№2,1.
48 Steeds, J.W., Introduction to Analytical Electron Microscopy, Edited by Hren, J, J.; Godstein, J,I., and Joy, D.C, Plenum Press. New York, (1979) p. 387.
49 Lin, Y.P.; Steeds, J.W., Acta Cryst., B40 (1985) .
50 Buxton, B.F.; Eades, J.A.; Steeds, J.W.; Rackham, G.M., Philos. Trans. R.Soc. A281 (1976) , 171.
51 Ye, H. Q.(叶恒强);Li. D. X.(李斗星);Kuo, K. H.(郭可信),Proc. of the 3rd APEM, Singapore,1984 p.146.
52 Wang, D. N.(王大能);Ye. H. Q.(叶恒强);Kuo, K. H.(郭可信);Acta Cryst.,B40 (1985) .
53 Kuo, K. H.(郭可信);Ye H. Q.(叶恒强);Li, D. X.(李斗星),J. Electron Microscopy Technique, 2 (1985) (in the press).
54 Lj, D. X.(李斗星);Ye, H. Q.(叶恒强);Kuo, K. H.(郭可信),Phil. Mag., A50(1984) ,531.
55 Ye, H. Q.(叶恒强);Li, D. X.(李斗星);Kuo, K. H.(郭可信),Electron Microscopy (1984) ,Budapest (1984) 213.
56 Wang, D. N.(王大能);Ye, H. Q.(叶恒强);Kuo, K. H.(郭可信),ibid (1984) 809.
57 Ye, H. Q.(叶恒强);Wang, D. N.(王大能);Kuo, K. H.(郭可信),Philos. Mag., A51 (1985) ,839.
58 Li, D. X.(李斗星);Kuo, K. H.(郭可信),Philos. Mag.,A51 (1985) ,849.
59 Ye, H, Q.(叶恒强);Wang, D. N.(王大能);Kuo, K. H.(郭可信),Ultramicroscopy, 16(1985) ,273.
60 Ye, H. Q.(叶恒强);Wang, D.N.(王大能);Kuo, K. H.(郭可信),Submitted Phys. Review. Lett. (1985) .
61 Penrose, R., Bull. Inst. Math, Appl. 10 (1974) , 266.
62 Mackay, A.L., Physica 114A (1982) , 609
63 Conway, J.H., unpublished See M. Gardner, Sci. Am., 236 (1977) , 110.
64 Shechtman, D.; Blech, I.; Gratias, D.; Cahn, J.W., Phys. Rev. Lett. 53(1984) , 1951.
65 Hiraga, K.; Hirabayashi, M.; Inoue, A.; Masumoto, T., Sci. Rep. Res. Inst. Tohoku Uni., 32(1985) , №2, 309.
66 Zhang, Z.(张泽);Ye, H. Q.(叶恒强);Kuo, K. H.(郭可信),Submitted to Philos. Mag. Letters.