0412-1961 |
A NOTE ON CONSTANT ELASTIC ALLOY WITH LOW TEMPERATURE COEFFICIENT OF TORSIONRESONANCE FREQUENCY |
|
Cite this article:
A NOTE ON CONSTANT ELASTIC ALLOY WITH LOW TEMPERATURE COEFFICIENT OF TORSIONRESONANCE FREQUENCY. 0412-1961. Acta Metall Sin, 1986, 22(1): 74-148.
|
Abstract TAN Yanchang; HE Bin; ZHAO Yuhua (Northeast Institute of Technology, Shenyang)
|
Received: 18 January 1986
|
1 户井诘哲郎,日本特许公报,昭 44-12265 (1969) . 2 铃木悠一;岡田正法;辺见善三,日本公开特许公报,昭 57-51244(1982) . 3 冥加修;河合淳,日本公开特许公报,昭57-145968(1982) . 4 国家标准GB.2105-80. 金属材料切变模量及泊松比测量方法,北京,1981. 5 谭延昌;刘国禄;何斌,东北工学院学报,27 (1981) ,37 |