EFFECT OF HYDROGEN ON CREEP IN AUSTENITIC STAINLESS STEEL
CHU Wuyang; DING Wei; XIAO Jimei (Beijing University of Iron and Steel Technology)
Cite this article: 

CHU Wuyang; DING Wei; XIAO Jimei (Beijing University of Iron and Steel Technology). EFFECT OF HYDROGEN ON CREEP IN AUSTENITIC STAINLESS STEEL. Acta Metall Sin, 1986, 22(2): 27-30.

Download:  PDF(304KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamic charging does not influence on the creep rate of type 321 austenitic stainless steel if the initial strain was less than 2%, in which the amounts evolving hydrogen after test were below 1.5 ppm (by wt). However, the creep rate increased markedly when the initial strain was larger then 8% or the specimen was precharged for a long time. In the case the corresponding amount evolving hydrogen was 5 to 12 ppm (by wt).
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/27

1 Shin, K.S.; Park, C.G.; Nagakawa, J.; Meshii, M., Scr. Metall., 14 (1980) , 279.
2 Oriani, R.A.; Josephic, P.H., Acta Metall., 27 (1979) , 997; 29 (1981) , 669.
3 Chu,W.Y.(褚武扬);Yao,J.(姚京);Hsiao,C.M.(肖纪美),Metall.Trans.,15A (1984) ,729.
4 姚京;褚武扬;肖纪美,金属学报,20 (1984) ,A124
5 Chu,W.Y.(褚武扬);Wang,H.L.(王核力);Hsiao,C.M.(肖纪美),Corrosion,40 (1984) ,487.
6 乔利杰;褚武扬;肖纪美,奥氏体不锈钢Ⅲ型试样的应力腐蚀与氢致开裂,1984,待发表
7 王燕斌;褚武扬;肖纪美,金属学报,18 (1982) ,673.
8 褚武扬;肖纪美;李世琼,金属学报,17 (1981) ,10.R
No related articles found!
No Suggested Reading articles found!