ESTIMATION OF FRACTURE TOUGHNESS FOR POLYCOMPONENT COMPOSITE MATERIALS
LI Zhonghua (Xi' an jiaotong University)
Cite this article: 

LI Zhonghua (Xi' an jiaotong University). ESTIMATION OF FRACTURE TOUGHNESS FOR POLYCOMPONENT COMPOSITE MATERIALS. Acta Metall Sin, 1986, 22(2): 87-92.

Download:  PDF(453KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The expressions for estimating fracture toughness of the polycomponent composite materials have been derived in terms of the fracture toughnesses and the volume fractions of individual component each is included. The expression, conformed to mixed rule, of upper (n→) or lower (n=1) bound value was also derived on the basis of limit analysis.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/87

1 Kameswararao, C.V.S., Eng. Fract. Mech., 18 (1983) , 35.
2 Patton, V.Z.; Morozov, E.M., Elastic Plastic Frature Mechanics, 1978, p. 74.
3 (叶彦谦等译),微积分学教程,第一卷第一分册,p.59.
4 Hagiwara, Y.; Knott, J, F., 5th Int. Conf. on Fracture, Vol. 2, 1981, 707.
5 Kunio, T.; Shimizu, M.; Yamada, K., Fracture Mechanics of Ductile and Tough Materials Applications to Energy Related Sructure, Eds. Liu, H.W.; Kunio, T., Martinus Nijhoff Publ., The Hague/Boston/London, 1980, p. 221.
6 Harris, B.; Cawthorne, D., Plast. and Polym. 42 (1974) , №161, 209.
7 Cawthorne, D.; Harris, B., Composits, 6 (1975) , p. 115.
8 Kaplan, M.F.; ACI J. Proc., 58 (1961) , 591.
9 Swamy, R.N., Fracture Mechanics Applied to Concrete, In Developments in Concrete Tech-nology, Vol. 1, Ed. Lydon, F.D., Applied Science Publ., London, 1978, p. 221.
No related articles found!
No Suggested Reading articles found!