LIQUIDUS AND INTERMETALLIC COMPOUND IN Al-RICH REGION OF Al-Mg-Ce SYSTEM
ZHENG Chaogui; WU Youyu; QIAN Jiuxin; YE Yupu (Department of Chemistry; Peking University)
Cite this article: 

ZHENG Chaogui; WU Youyu; QIAN Jiuxin; YE Yupu (Department of Chemistry; Peking University). LIQUIDUS AND INTERMETALLIC COMPOUND IN Al-RICH REGION OF Al-Mg-Ce SYSTEM. Acta Metall Sin, 1986, 22(2): 107-155.

Download:  PDF(1238KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The liquidus of the Al-rich corner in Al-Mg-Ce phase diagram and the intermetallic compound, if any, formed in this region have been studied by themal, EMPA, chemical analysis, metallography and X-ray examination. An intermetallic compound in the solid phase was observed to form solid solution with rather extensive range. The pseudo-ternary system Al-Mg_5Al_8-CeAl_4 is of the ternary eutectie type. Three surfaces corresponding to primary crystallization of α-Al, Mg_5Al_8 and CeAl_4 respectively, three univariant curves associated with secondary crystallization and a ternary eutectic with composition about 12.6 wt-%C e and 26.0wt-%Mg at 446℃ were detected.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/107

1 #12
2 Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 105; 78.
3 Mondolfo, L.F., Aluminium Alloys: Structure and Properties, Butterworth, London, 1976, p. 242; 311.
4 郑朝贵;邢娅;钱久信;叶于浦,金属学报,19 (1983) ,A515.
No related articles found!
No Suggested Reading articles found!