Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (3): 76-84    DOI:
Current Issue | Archive | Adv Search |
ACTIVITY OF CaO IN LIQUID CaO-SiO_4-Al_2O_3 SYSTEM
by ZHANG Ziqing (Institute of Metal Research. Academia Sinica; Shenyang); ZHOU Jicheng; ZOU Yuanxi (Chou Yuan-hsi) (Shanghai Institute of Metallurgy; Academia Sinica); TIAN Yanwen (Northeast Institute of Technology; Shenyang)
Cite this article: 

by ZHANG Ziqing (Institute of Metal Research. Academia Sinica; Shenyang); ZHOU Jicheng; ZOU Yuanxi (Chou Yuan-hsi) (Shanghai Institute of Metallurgy; Academia Sinica); TIAN Yanwen (Northeast Institute of Technology; Shenyang). ACTIVITY OF CaO IN LIQUID CaO-SiO_4-Al_2O_3 SYSTEM. Acta Metall Sin, 1986, 22(3): 76-84.

Download:  PDF(691KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  With a view to evaluating the activity of CaO in the liquid system CaO-SiO_2-Al_2O_3, Sn was chosen as solvent for studying the slag-metal eqilibria. The results for 1600℃ thus obtained are believed to be more reasonable and trustworthy than previous investigations. An attempt has also been made to develop a graphical method for the analysis of data. By this means, some relatively accurate iso-activity curves of CaO have been obtained, and values of CaO activities in a wide range of composition in this melt can easily be obtained from the figures derived from experimental data by the authors. Inaddition, the amphoteric behaviour of Al_2O_3 has been determined quantitatively, and the results are believed to have practical significance in blast furnace smelting using high alumina slags.
Received:  18 March 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I3/76

1 Rein, R.H.; Chipman, J., Trans. Metall.Soc. AIME, 233 (1965) , 415.
2 Largenberg, F.C.; Chipman, J., Trans. Metall.Soc. AIME, 215 (1959) , 958.
3 邹元燨;周继程,徐元森,赵彭年;张子青,金属学报,18(1982) ,127.
4 周继程;邹元燨;赵彭年;李鸿明;张子青,中国金属学会1979-1980年优秀论文选集,第四分册,1984,冶金工业出版社,p.83.
5 #12
6 三本木贡治,大森康男,日本金属学会会誌,25(1961) ,139.
7 坂上六郎,铁钢,39(1953) ,587;688;1240.
8 Chou Yuanhsi(邹元燨);Chao Pengnian(赵彭年),Scientia Sinica.11(1962) ,1287.
9 邹元燨,赵彭年,曹兆民,金属学报,6(1963) ,121.
10 Philbrook. W.O.; Goldman, K.M.; Helzel M.H., Trans. AIME, 188 (1950) , 361.
11 邹元燨,赵彭年,第一届全国冶金过程物理化学学术报告会论文集,1965. p.365.
12 Borgianni. C.; Granati, P., Metall. Trans., 8B (1977) , 147.
13 Hgemark, K., J.Phys. Chem., 72 (1968) , 2316.
14 Levin, E,M.; Robbins, C.R.; McMurdie, H,F., Phase Diagrams fot Ceramists, The Am. Ceram. Soc., 1964. p. 219.
No related articles found!
No Suggested Reading articles found!