| BEHAVIOUR OF BORON IN CARBONIZED AND CARBONITRIDED CASE AND CASE-HARDENABILITY OF BORON STEEL |
| CHU Youyi; HE Xinlai (Beijing University of Iron and Steel Technology); FENG Ruilin; CHEN Zhiguo; WU Jinyao (Nanchang Gear Plant) |
|
Cite this article:
CHU Youyi; HE Xinlai (Beijing University of Iron and Steel Technology); FENG Ruilin; CHEN Zhiguo; WU Jinyao (Nanchang Gear Plant). BEHAVIOUR OF BORON IN CARBONIZED AND CARBONITRIDED CASE AND CASE-HARDENABILITY OF BORON STEEL. Acta Metall Sin, 1986, 22(5): 5-15.
|
|
|
Abstract The B is obviously redistributed in B steel within the whole carbonized and carbonitrided case because of the interaction between B with N and C during carbonizing and carbonitriding. The most of all behaviour of B observed in the carbonized case is the enrichment into the surface layer and the depletion from the sub-layer beneath surface, and in the earbonitrided case is the formation of abundant BN in the wide region from surface and the extension of depleted solution B into deep zone. The redistribution of B is remarkably influenced on the hardenability of the case. The carbonized case hardenability is affected not only by the carbon changed in content and influenced on B hardenability effect, but also by the B depletion in sub-layer. The abundant BN particles with solution B depletion deeply into the interior formed in carbonitrided ease is very harmful to the hardenability.
|
|
Received: 18 May 1986
|
1 Jatczak, C. F.; Rowland, E.S., Trans. ASM, 45 (1953) , 771. 2 Grange, R.A.; Mitchell, J.B., Trans. ASM, 46 (1954) , 446. 3 关启标;李林,金属学报,1(1956) ,255. 4 Llewellyn, D.T.; Cook, W.T., Met. Technol., 1(1974) . 517. 5 贺信莱;褚幼义;张秀林;余宗森;李秋萍;尹熙光,会属学报,13(1977) ,235. 6 He, X.L.; Chu, Y.Y., J. Phys, D: Appl. Phys., 16 (1983) , 1145. 7 Rahrer, G.D.; Armstrong, C.D., Trans. ASM, 40 (1948) , 1099. 8 Grossman, M.A., Trans. AIME, 150 (1942) , 227. 9 Kunze, C.T.; Keil, G., Boron in Steel, Eds. Banerji, S.K.; Morral, J.E., AIME, 1980, p. 106. 10 Chatterjee-Fischer, R., Metall. Trans., 9A (1978) , 1553. 11 北京齿轮厂热处理车间;北京钢铁学院金相专业北齿实践队,金属热处理,(1977) ,№ 3. 13. 12 洪觉宏,金属热处理,(1981) ,№ 8,35. 13 Kawasaki, S.; Hishinma, A.; Nagasaki, R., J. Nucl. Mater., 39 (1971) , 166. 14 Smithells, C.J., Metals Reference Book, 5th ed., 1976 |