Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 29-36    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF AUSTENITE ORDERING ON MARTENSITIC TRANSFORMATION IN Fe-Ni ALLOYS
YAN Linfa (Shanghai Iron and Steel Research Institute); XU Zuyao (Shanghai Jiaotong University)
Cite this article: 

YAN Linfa (Shanghai Iron and Steel Research Institute); XU Zuyao (Shanghai Jiaotong University). EFFECT OF AUSTENITE ORDERING ON MARTENSITIC TRANSFORMATION IN Fe-Ni ALLOYS. Acta Metall Sin, 1986, 22(5): 29-36.

Download:  PDF(1707KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Experimental results show that, in Fe-Ni alloys, the M_s or M_b values decrease in two steps with the decrease in quenching temperature below 950℃ with definite grain size of the parent phase. In the first step, i. e., quenching temperature around 800℃, a minimum M_s value appears, and in the second one, i.e., below 700℃ quenching, M_s decreases continueously. The burst aize of martensite transformation corresponding to the lower quenching temperatures is rather smaller than that to the higher ones. These phenomena prove to be related to the ordering of the parent phase. The observation of densely dispersed tine precipitates and superlattice dislocations by TEM comfirms the views that ordering does exist in bulk specimens and markedly affect the martensitic transformation of Fe-Ni alloys.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/29

1 Hsu, T. Y. (Xu Zuyao); Yan Linfah, J. Mater. Sci., 18 (1983) , 3213.
2 徐祖耀;颜林发,金属学报,20(1984) ,A 143.
3 徐祖耀;高明;张寿柏,上海交通大学科学研究报告,1965.
4 Chang, H,; Sastri, S., Metall. Trans., 11A (1980) , 194.
5 Dunne. D,P,; Wayman, C. M,. Metall. Trans., 4 (1973) , 137, 147.
6 Chang, H.; Hahn, S.; Sastri, S.. Metall. Trans,, 7A (1976) , 1796.
7 Ardley, G. W.. Acta Metall., 3 (1955) . 525.
8 Lawley, A.; Vidoz, E.A.; Cahn, R.W., Acta Metall., 9 (1961) , 287.
9 Stoloff, N.S., Strengthening Methods in Crystals, Eds. Kelly. A.; Nicholson, R.B., Elsevier Publ., Amsterdam, 1971, p. 220.
10 Tong, H.C.; Wayman, C.M., Acta Metall., 23 (1975) , 209.
11 徐祖耀,金属学报,l5(1979) ,329;16(1980) ,420.
12 Hsu, T. Y. (Xu Zuyao); Chang Hongbing; Luo Shonfu, J. Mater. Sci., 18 (1983) , 3206.
13 Hsu, T. Y. (Xu Zuyao); Chang Hongbing, Acta Metall., 32 (1984) , 34.
14 Kachi, S.; Bando, Y.; Higuchi, S., J. Appl. Phys., 32 (1962) , 301.
15 Hausch, G.; Warlimont, H., Phys. Lett., 36A (1971) , 415.
16 Hausch, G.; Warlimont, H., Acta Metall., 21 (1973) , 401.
17 Schlosser, W.F., J. Phys. Chem. Solids, 32 (1971) , 939.
18 Rodionov, Yu. L.; Ishandiyarov, G. G.; Sarsendin, O.S., Phys. Met. Metallogr., 48 (1979) , № 567.
19 Stoloff, N.S., Strengthening Methods in Crystals, Eds. Kelly, A.; Nicholson, R. B., Elsevier Publ., Amsterdam, 1971, p. 205.
20 Entwisle, A.R.; Feeney, J. A., The Mechanism of Phase Transformation in Crystalline Solids, Institute of Metals, Monograph № 33, London, 1969, p. 156-61.
21 Owen, E.A.; Liu, Y.H., J. Iron Steel Inst., London, 163 (1949) , 132.
22 Umemoto, M.; Qwen, W.S., Metall. Trans., 5 (1974) , 2041.S
No related articles found!