INFLUENCE OF PROLONGED AGING ON MICROSTPUCTURE AND MECHANICAL PROPERTIES OF K17G CAST Ni-BASE SUPERALLOY
WANG Sukun ZHANG Bingda HU Zhuangqi (Institute of Metal Research.Academia Sinica.Shenyang)
Cite this article: 

WANG Sukun ZHANG Bingda HU Zhuangqi (Institute of Metal Research.Academia Sinica.Shenyang). INFLUENCE OF PROLONGED AGING ON MICROSTPUCTURE AND MECHANICAL PROPERTIES OF K17G CAST Ni-BASE SUPERALLOY. Acta Metall Sin, 1987, 23(1): 6-12.

Download:  PDF(1631KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The K17G cast Ni-base superalloy is the one of low density,high strength and good ductility.Due to the stability of microstructure and lack of harmful a-phase after prolonged aging at 750—950℃,its mechanical properties are slightly lowered only.Although the properties of samples cut and machined from turbine blades subjected also to prolonged aging were been some reduction, in comparison with those of standard precision-cast specimens,their tensile properties and ruptuce strength were still kept at rather high level.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/6

1 Piearcey B J,Smashey R W.Trans Metall Soc,1967;239:451
2 Collins H E,Quigg B J.ASM Trans Q,1968;61:139
3 Collins H E.ASM Trans Q,1969;62:82
4 Sabol G P,Stickler R.Phys Status Solidi,1969;35:11
No related articles found!
No Suggested Reading articles found!