INFLUENCE OF MORPHOLOGY AND DISTRIBUTION OF FERRITE ON FRACTURE BEHAVIOR OF LOW-CARBON STEEL AT LOW TEMPERATURE
HUANG Zheng; YAO Mei; FAN Yinglong (Harbin Institute of Technology); LI Chunzhi (Institute of Aeronautical Materials; Beijing); HAN Yuanlong (Research Institute of Anshan Iron and Steel Company) (Manuscript received 20 January; 1986; revised manuscript 12 July; 1986)
Cite this article: 

HUANG Zheng; YAO Mei; FAN Yinglong (Harbin Institute of Technology); LI Chunzhi (Institute of Aeronautical Materials; Beijing); HAN Yuanlong (Research Institute of Anshan Iron and Steel Company) (Manuscript received 20 January; 1986; revised manuscript 12 July; 1986). INFLUENCE OF MORPHOLOGY AND DISTRIBUTION OF FERRITE ON FRACTURE BEHAVIOR OF LOW-CARBON STEEL AT LOW TEMPERATURE. Acta Metall Sin, 1987, 23(3): 223-313.

Download:  PDF(3144KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In the present investigation, the influence of morphology and distribution of ferrite, especially the acicular ferrite in Widmansttten structure, on fracture behavior of low-carbon steel 16Mn at low temperature was discussed in detail. The microstructures of polygonal ferrite, intersecting aeicuiar ferrite and parallel aeicular ferrite were obtained by using interrupted-cooling procedure.If the arrangement is characterized by intersecting, the steel would possess the superior toughness at low temperature in comparison with that of polygonal ferrite. If the microstructure is mainly composed of parallel acicular ferrite, however, it would deteriorate the steel toughness.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/223

1 Otterberg R, Sandstrom R, Sandberg A. Met Technol, 1980; 10: 397
2 #12
3 #12
4 孙振岩,李春生,李见.魏氏组织论文集,李见主编,东北工学院学报编辑部,1983:57
5 刘继恒.金属热处理,1983;2:6
6 #12
7 黄正.硕士研究生论文,哈尔滨工业大学,1984
8 范莹龙.硕士研究生论文,哈尔滨工业大学,1986
9 李春志.物理学报,1979;28:314
10 姚枚,何裕宽,李道明.钢铁,1984;19(12) :10
11 Yao M, He Y K, Li D M et al. Advances in Fracture Research (ICF-6) , vol. 2, New Delhi, 1984: 1423c
No related articles found!