Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 425-429    DOI:
Current Issue | Archive | Adv Search |
HYDROGEN STORAGE PROPERTIES OF TiMn_(1.5-x)Cr_x
by QIAN Jiuxin; MAO Ying; YE Yupu (Department of Chemistry; Peking University)(Manuscript recevied 10 May; 1986; revised manuscript 8 September; 1986)
Cite this article: 

by QIAN Jiuxin; MAO Ying; YE Yupu (Department of Chemistry; Peking University)(Manuscript recevied 10 May; 1986; revised manuscript 8 September; 1986). HYDROGEN STORAGE PROPERTIES OF TiMn_(1.5-x)Cr_x. Acta Metall Sin, 1987, 23(5): 425-429.

Download:  PDF(318KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The first hydrogen absorption curves of TiMn_(1.5-x)Cr_x have been determined at 40℃ and an initial hydrogen pressure of 4.05MPa. Pressure-composition desorption isotherms for TiMn_(1.5-x)Cr_x-H system have also been determined at 19℃. The results show that hydrogen storage properties improve markedly while Mn was partially substituted by Cr: reducing the VIZ incubation period, enhancing the absorption rate, increasing the absorption capacity and slightly raising the desorption amount of hydrogen.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/425

1 Gamo T, Moriwaki Y, Yanagihara N, Yamashita T, Iwaki T.In: Proc 3rd World Hydrogen. Energy Conf, Vol. 4, Tokyo, June, 1980, Oxford: Pergamon, 1980: 2127
2 李玉凤,徐德明,陈于才.金属学报,1983;19:A403
3 山下敏夫,蒲生孝治,森脇良夫,福田雅太郎.日本金属学会誌,1977;41:148
4 虞心南,张青哲,陈镇国,邓其森,陈荣标,王建荣,于艳蓉,林彰达.物理通讯,1984;2:219
No related articles found!
No Suggested Reading articles found!