FATIGUE RUPTURE OF 55SiMnVB SPRING STEEL
PENG Xinping Department of Materlats Science;Wuhan Iron And Steel University;XU Bofan;LIU Xinmin Wuhan Iron and Steel University
Cite this article: 

PENG Xinping Department of Materlats Science;Wuhan Iron And Steel University;XU Bofan;LIU Xinmin Wuhan Iron and Steel University. FATIGUE RUPTURE OF 55SiMnVB SPRING STEEL. Acta Metall Sin, 1988, 24(2): 126-130.

Download:  PDF(1674KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The results of conventional and high frequency fatigue tests of 55SiMnVB spring steel were reported. The fatigue rupture of the steel concerned hasbeen discussed together with the microstructure and fracture morphology observedand the fracture toughness obtained.
Key words:  55SiMnVB spring steel      fatigue rupture     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/126

1 王承忠,吴素生.理化检验(物理分册),1983;(3) :12
2 航空标准:疲劳裂纹扩展速率标准测试方法,附录3,1981年3月
3 俞学节.上海钢研,1984;(1) :37
4 金达曾,骆竞晞,邓增杰,顾海澄.金属材料强度研究与应用.北京:科学技术文献出版社,1985:51N
No related articles found!
No Suggested Reading articles found!