| MATHEMATICAL MODELS OF NITROGEN CONCENTRATION PROFILE OF ION NITRIDED LAYERS AND COMPUTER SIMULATION |
| XIA Lifang;YAN Mufu Harbin Institute of TechnologyDivision of Metal Materials and Heat treatment; Harbin Institute of Technology; Harbin |
|
Cite this article:
XIA Lifang;YAN Mufu Harbin Institute of TechnologyDivision of Metal Materials and Heat treatment; Harbin Institute of Technology; Harbin. MATHEMATICAL MODELS OF NITROGEN CONCENTRATION PROFILE OF ION NITRIDED LAYERS AND COMPUTER SIMULATION. Acta Metall Sin, 1988, 24(4): 314-321.
|
|
|
Abstract The mathematical models of the kinetics of the layer growth at differ-ent ion nitriding conditions of armco iron, steels 45, 40Cr, 42CrMo and 38CrMoAlhave been established. Based on these models the expression of nitrogen concentra-tion profile of ion nitrided layers have been deduced with profile simulating method.They are C_β=C_(min)~ε+P~4/ξ_(10)(ξ_1-x)+P~5/ξ_(10)~2(ξ_1-x)~2 C_γ~′=C_(min)~γ′+P_1/ξ_(21)(ξ_2-x)+P_2/ξ_(21)~2(ξ_2-x)~2 C_α=C_(min)~α+C_(33)/ξ_(32)~3(ξ_3-x)~3Using these models, the kinetics of layer growth and the nitrogen concentration pro-file of ion nitrided layers were simulated on Apple-Ⅱ computer. Results show thatthe simulated curves coincide quite well with the experimental data.
|
|
Received: 18 April 1988
|
1 杜树芳,黄辉.金属热处理,1980;(1) :7--11 2 曾根匠,纲沢荣二,山中久彦.热处理,1984;24(6) :316--322 3 Marcinik A. In: Proc 4th Int Congress on Heat Treatment of Materials, Vol. I, Berlin: International Federation for the Heat Treatment of Materials, 1985: 591--609 4 山中久彦著,李贻锦,朱雅年译.离子渗氮,北京:机械工业出版社,1985;4,71 5 阎牧夫.离子渗氮工艺过程的数学模型与计算机仿真,哈尔滨工业大学硕士学位论文,1987 6 崔明根,邓中兴.数学模型化处理,哈尔滨工业大学出版社,1985:1--13 7 上海师范大学数学系.回归分析及其实验设计,上海教育出版社,1978:141--19 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|