HIGH T_c SUPERCONDUCTOR YBa_2 Cu_3 O_x PREPARED WITH DIRECT REACTION PROCESS
FAN Zhanguo;JI Chunlin;WANG Kuihan;CUI Chuanmeng;LIU Sulan Northeast University of Technology; Shenyang
Cite this article: 

FAN Zhanguo;JI Chunlin;WANG Kuihan;CUI Chuanmeng;LIU Sulan Northeast University of Technology; Shenyang. HIGH T_c SUPERCONDUCTOR YBa_2 Cu_3 O_x PREPARED WITH DIRECT REACTION PROCESS. Acta Metall Sin, 1989, 25(2): 95-99.

Download:  PDF(371KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A direct reaction process for producing high T_c spuerconductor YBa_2-Cu_3O_x has been proposed. The T_c of it is 90--94.5 K and △T is 1K. The phaseequilibria in system Y_2 BaCuO_5-Y_2Cu_2O_5-CuO-YBa_2Cu_3O_x were studied and discussed.
Key words:  direct reaction process      YBa_2Cu_3Ox      high T_c superconductor     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/95

1 Frase K G, Liniger E G, Clarke D R. J Am Ceram Soc, 1987; 70 (9) : C204
2 Che Guangcan (车广灿), Liang Jingkui (梁敬魁), Chen Wei (陈维) et al. Int J Mod Phys, B, 1987; 1 (2) : 363
No related articles found!
No Suggested Reading articles found!