Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (4): 60-66    DOI:
Current Issue | Archive | Adv Search |
MECHANISM OF INTERGRANULAR FRACTURE OF AS-QUENCHED MARTENSITE IN HIGH CARBON STEELS
LIU Zongchang Baotou Iron and Steel University
Cite this article: 

LIU Zongchang Baotou Iron and Steel University. MECHANISM OF INTERGRANULAR FRACTURE OF AS-QUENCHED MARTENSITE IN HIGH CARBON STEELS. Acta Metall Sin, 1989, 25(4): 60-66.

Download:  PDF(2519KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mechanism of intergranular fracture of as-quenched martensite inhigh carbon steels has been proposed. When coarse grains of austenite transform tomartensite, the grain plays a role of the unit of volume dilation, inhomogeneousstrains necessarily produce and local microscopic stress concentrations create at grainboundaries. This reduces the integration of the grains, sometimes intergranutarcracks may produce. Under the action of first kind hardening stress or externalforce, the intergranular cracks propagated along the grain boundaries will form.This results in the candy-like fracture.
Key words:  as-quench martensite      intergranular fracture      inhomogeneous strain     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/60

1 #12
2 Ogura T. Trans Jpn Inst Met, 1981; 22: 109
3 Brant C L, Banerji S K. Int Metals Rev, 1978: 23 (4) : 164
4 刘宗昌.理化检验(物理分册),1985;19(6) :1
5 贡海.金属热处理,1982;(3) :1
[1] WU Bo WEI Yueguang TAN Jiansong WANG Jianping. NUMERICAL SIMULATIONS OF THE INTERGRANULAR FRACTURE IN NANOCRYSTALLINE Ni[J]. 金属学报, 2009, 45(9): 1077-1082.
[2] XIAO Jimei (HSIAO Chimei) (University of Science and Technology Beijing; Beiing 100083). MATERIALS DESIGN AGAINST FRACTURE[J]. 金属学报, 1997, 33(2): 113-125.
[3] HONG Bande;YI Xiao;MENG Qingchang Harbin Institute of Technology. EFFECT OFδ-Ni_3 Nb ON LOW CYCLE FATIGUE RACTURE OF INCONEL 718[J]. 金属学报, 1991, 27(1): 55-60.
No Suggested Reading articles found!