MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY
HAN Ming;CHEN Fumin;CHEN Jinming;CHEN Yuru;LIU Wenxi Tianjin University professor;Department of Material Science and Engineering;Tianjin University; Tianjin 300072
Cite this article:
HAN Ming;CHEN Fumin;CHEN Jinming;CHEN Yuru;LIU Wenxi Tianjin University professor;Department of Material Science and Engineering;Tianjin University; Tianjin 300072. MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY. Acta Metall Sin, 1990, 26(2): 5-9.
Abstract The bainitic transformation in a Cu-Zn-Al-Mn alloy has been examin-ed with TEM. The results show that the stacking faults and also the bainitic mi-drib are found at the beginning of bainite formation in the alloy. The stack-ing fault planes can pass continuously through the midrib in bainite. The growthledges occur at the broad faces and rims of bainite. The broad and narrow faces ofthe ledges are parallel to the fault plane and habit plane respectively. Both theirMiller indices are {110}_(B_2). The moving direction of ledges is parallel to the faultplane. It may be deduced that bainites in a Cu-Zn-Al-Mn alloy are initially form-ed by shear and the process of growth are governed by propagation of fault planes.
1 陈树川,张骥华,张寿柏,徐祖耀.金属学报,1986;22:A379 2 刘文西,邹美运,马福本.金属学报,1981;17:137 3 Okamoto H, Oka M. Metall Trans, 1986; 17A: 1113 4 Chattopadhyay K, Aaronson H I. Acta Metall, 1986; 34: 695 5 Cornelis I, Wayman C M. Scr Metall, 1973; 7: 579 6 Lorimer G W, Cliff G, Aaronson H I, Kinsman K R. Scr Metall, 1975; 9: 27