PHOSPHORUS SEGREGATION AND EMBRITTLEMENT OF Ni-P AMORPHOUS
QU Zhe;XIE Tiansheng Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

QU Zhe;XIE Tiansheng Institute of Metal Research; Academia Sinica; Shenyang. PHOSPHORUS SEGREGATION AND EMBRITTLEMENT OF Ni-P AMORPHOUS. Acta Metall Sin, 1990, 26(5): 107-111.

Download:  PDF(513KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The surface segregation of P and the embrittlement, also their rela-tions, of Ni-P amorphous annealed at temperatures below crystallization have beeninvestigated. A P-depleted layer was found nearby the surface during annealing.The P-depleted layer became thicken and the depletion of P became severe as theincrease of annealing temperature. The mechanism of elementary redistrib utionand annealing embrittlement during relaxation Was discussed on the viewpoint ofthe activation energy of atomic diffusion in Ni-P amorphous being variables.
Key words:  Ni-P amorphous      element redistribution      annealing embrittlement     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/107

1 Chen H S. Mater Sci Eng, 1976; 26: 79
2 Walter J L, Bacon F, Luborsky F E. Mater Sci Eng, 1976; 24: 239
3 Luborsky F E, Walter J L. J Appl Phys, 1976; 47: 3648
4 Williams R S, Egami T. IEEE Trans Magn, 1976; MAG--12: 927
5 前田康二.日本金属学会会报,1982;21:425
6 Gibbs M R J, Evetts J E, Leake J A. J Mater Sci, 1983; 18: 278
7 Drehman A J, Greer A L. Acta Metall, 1984; 32: 323
[1] HONG Bo; JIANG Chuanhai; WANG Xinjian; WU Jiansheng. Phase transformation behaviour and kinetics of electrodeposition Ni-P amorphous alloys by X-ray analysis[J]. 金属学报, 2006, 42(7): 699-702 .
[2] CHE Xiaozhou; SUN Baode; HU Gengxiang(Shanghai Jiaotong University; Shanghai 200030); CAO Xingguo(Luoyang Institute of Technology; Luoyang 471039); DAI Lizhi(Central Iron & Steel Research Institute; Ministry of Metallurgical Industry;Beijing 100081)(Manuscript received 1995-05-30). MECHANISM OF ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY[J]. 金属学报, 1996, 32(2): 202-206.
[3] CHE Xiaozhou; HU Gengxiang(Shanghai Jiaotong University;Shanghai 200030);CAO Xingguo(Luoyang Institute of Technology;Luoyang 471039);DAI Lizhi (TAI Lichi)(Central Iron Steel Research Institute;Ministry of Metallurgical Industry;Beijing 100081). CHARACTER OF THERMALLY ACTIVATED MOTION OF ATOMS RELATED TO THE DUCTILE-BRITTLE TRANSITION OF AMORPHOUS ALLOYS[J]. 金属学报, 1995, 31(8): 333-339.
[4] CHE Hiaozhou; HU Gengxiang(Shanghai Jiaotong University); CAO Hingguo(Luoyang Institute of Technology); DAI Lizhi(Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS[J]. 金属学报, 1994, 30(24): 532-536.
[5] LIANG Jianduan;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang. APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA[J]. 金属学报, 1989, 25(1): 141-146.
[6] WANG Jingtang;PANG Dexing;DING Bingzhe;BIAN Maoshu;LI Shuling Institute of Metal Research; Academia Sinica; Shenyang. TEMPERATURE DEPENDENCE UPON VISCOSITY OF Ni-P ALLOY ON AMORPHOUS FORMATION[J]. 金属学报, 1988, 24(5): 444-447.
No Suggested Reading articles found!