ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM
ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming
Cite this article: 

ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM. Acta Metall Sin, 1991, 27(3): 147-149.

Download:  PDF(257KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The room temperature and 700℃ isothermal sections for the region containing0--33 at. -%Gd of Gd-Pd-Pt ternary system phase diagram have been determined by X-raydiffraction analysis and optical microscopy. Both sections consist of 5 single phase regions-Pd(Pt) or Pt(Pd), GdPd_3, GdPd_2, GdPt_5 and GdPt_2; 7 bi-phase regions-Pd(Pt)+GdPd_3, Pd(Pt)+GdPt_5, GdPd_3+GdPd_2, GdPd_2+GdPt_2, GdPt_2+GdPd_3, GdPt_2+GdPt_5 and GdPd_3+GdPt_5; and 3tri-phase regions-Pd(Pt)+GdPt_5+GdPd_3, GdPt_5+GdPd_3+GdPt_2 and GdPd_3+GdPd_2+GdPt_2 respe-ctively. No any ternary intermetallic compound is found.
Key words:  Gd-Pd-Pt ternary system      isothermal section      room temperature section     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/147

1 何纯孝,马光辰,王文娜,王永立,赵怀志.贵金属合金相图.北京:冶金工业出版社,1983:111
2 Bronger W. J Less Common Met, 1967; 12: 63
3 1983: 4: 176
4 Loebich O Jr., Raub E. J Less-Common Met, 1973; 30: 47
5 Palenzona A, Iandelli A. J Less-Common Met, 1974; 34: 121
[1] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[2] GONG Fangyue;GOLDSTEIN JI Tianjin University; Lehigh University; Bethlehem; U. S. A. Correspondent associate professor; Department of Materials Science; Tianjin University; Tianjin 300072. 550 AND 450℃ ISOTHERMAL SECTIONS OF Fe-Ni-C PHASE DIAGRAM[J]. 金属学报, 1992, 28(6): 47-51.
[3] ZENG Lingmin;ZHUANG Yinghong;Ll Dexuan;LIN Weibo Guangxi University; Nanning. A 500℃ ISOTHERMAL SECTION OF Ag-Cu-P SYSTEM[J]. 金属学报, 1991, 27(2): 148-150.
[4] CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi. 410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 142-143.
[5] ZHANG Ning;LUO Yang Central Iron and Steel Research Institute; Ministry of Metallurgical Industry Beijing. PHASE DIAGRAM OF Nd-Fe-B TERNARY SYSTEM I. ISOTHERMAL SECTION AT ROOM TEMPERATURE[J]. 金属学报, 1989, 25(2): 116-120.
No Suggested Reading articles found!