Abstract  The buffer layer material itself may be influential to the bond strength between active brazing filler and ceramics. For Ag_(57)Cu_(38)Ti_5 filler metal, Cu or Ta is excellent buffer layer material, but Kovar or Ni-15Cr-15Co is worse. It was important to design a layer of soft buffer, such as Cu, to relax interfacial stress rather than hard buffer layer, such as Mo, to avoid stress. There is an optimum thickness range of soft buffer layer, saying h/L=0.02-0.1. It was a good solution to the interfacial stress problem to use soft/bard buffer layer to increase metal/ceramics joint strength. Finally, an idea of designing gradual materials as buffer layer between metal and ceramics was suggested.
Key words:  ceramic/metal joining      Sialon      40Cr steel      active brazing      interlayer     
Received:  18 June 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I6/133

1 Pask J A. Am Ceram Soc Bull, 1987; 66: 1587
2 Delannay F, Froyen L, Deruyttere A. J Mater Sci, 1987; 22: 1
3 Eigemann B, Scholtes B, Macherauch E. Mater Sci Eng, 1989; A118: 1
4 Xian A P, Si Z Y. J Mater Sci, 1990; 25: 4483
5 Thiemann K H, Weinert H J, Raeuchle W. GB Pat, 2151173 A1, 1985
6 黄莉萍,黄振坤,徐友仁,符锡仁.无机材料学报,1986;1:123
7 Naka M, Okamoto I, Nishino T, Ural S. Trans JWRI, 1989; 18: 189
8 Ruehle M, Evans A G. Mater Sci Eng, 1989; A107: 187
9 冼爱平,斯重遥.计算机与应用化学,1991;8:232
10 冼爱平,斯重遥.第六届全国焊接学术会议论文集,第1卷西安,1990:160
11 Naka M, Tanaka T, Okamoto I. Trans JWRI, 1985; 14: 285
12 Xian A P, S1 Z Y. J Am Ceram Soc, 1990; 73: 3462
[1] REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao. Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition[J]. 金属学报, 2022, 58(2): 206-214.
[2] JIANG Lin, ZHANG Liang, LIU Zhiquan. Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly[J]. 金属学报, 2020, 56(10): 1433-1440.
[3] Shan SU. Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer[J]. 金属学报, 2019, 55(8): 1041-1048.
[4] Zhengrong YU,Xianfei DING,Lamei CAO,Yunrong ZHENG,Qiang FENG. TRANSIENT LIQUID PHASE BONDING OF SECOND AND THIRD GERNERATION Ni-BASED SINGLE CRYSTAL SUPERALLOY WITH Hf-CONTAININGINTERLAYER ALLOY[J]. 金属学报, 2016, 52(5): 549-560.
[5] LIU Yi, JIANG Guofeng, XU Kun, LUO Ximing, CHEN Dengquan, LI Wei. EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING[J]. 金属学报, 2015, 51(2): 209-215.
[6] ;. FABRICATION AND PROPERTIES OF TiN/O’-Sialon ELECTROCONDUCTIVE COMPOSITES[J]. 金属学报, 2007, 43(2): 131-136 .
[7] WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072). MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS[J]. 金属学报, 1997, 33(6): 625-630.
[8] ZHUANG Yanxin; XIAN Aiping; WANG Yikang; ZHANG Hiumu; HU Zhuangqi(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-11-03; in revised form 1996-04-15). WETTING AND JOINING OF Sn-BASED ACTIVE SOLDERS ON SIALON CERAMIC IN ROUGH VACUUM[J]. 金属学报, 1996, 32(7): 735-741.
[9] ZHAI Yang;REN Jialie; ZHUANG Lijun; CAO Yuqing;SUN Lijun(Tsinghua University; Beijing 100084)(Manuscript received 1994-10-09; in revised form 1995-0 1-20). DIFFUSION BONDING OF Si_3N_4 AND 40Cr STEEL WITH AMORPHOUS Cu_(50)Ti_(50)B INTERLAYER[J]. 金属学报, 1995, 31(21): 423-428.
[10] ZHAI Yang;REN Jialie ZHUANG Lijun(Tsighua University). AMORPHOUS Cu_(50)Ti_(50) ALLOYINTERLAYER IN DIFFUSION BONDING OF Si_3N_4 CERAMICS[J]. 金属学报, 1994, 30(20): 361-365.
[11] LIU Changsheng;CAI Qingkui;XU Hao Northeastern University; Shenyang. FATIGUE CRACK INITIATION ON NON-OVERLAPPED LASER HARDENED 40Cr STEEL[J]. 金属学报, 1993, 29(12): 34-38.
No Suggested Reading articles found!