TWO-PHASE EQUILIBRIUM CALCULATION BY THE GRAND POTENTIAL METHOD FOR BINARY ALLOYS
HAO Shiming; JIANG Min (Northeast University of Technology; Shenyang)
Cite this article: 

HAO Shiming; JIANG Min (Northeast University of Technology; Shenyang). TWO-PHASE EQUILIBRIUM CALCULATION BY THE GRAND POTENTIAL METHOD FOR BINARY ALLOYS. Acta Metall Sin, 1992, 28(11): 54-58.

Download:  PDF(317KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new method for phase equilibrium calculation has been proposed in subregular solution model based on the concept of equality of two-phase equilibrium criterion of both the effective chemical potential and the grand potential. Comparing with the optimization for minimum free energy, it seems to be simpler in calculation and no more convergence problem.
Key words:  subregular solution model      phase equilibrium      grand potential     
Received:  18 November 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I11/54

1 Kikuchi R. J Chem Phys, 1974; 60:1071
2 Kikuchi R. Acta Metall,1977; 25:195
3 郝士明,蒋敏.材料科学进展,待发表
4 Murray J L. Bull Alloy Phase Diagrams, 1983; 4:55
[1] LI Hongxiao REN Yuping MA Qianqian JIANG Min QIN Gaowu. PHASE EQUILIBRIUM IN THE LOW-Ca SIDE OF Mg-Zn-Ca SYSTEM AT 400 ℃[J]. 金属学报, 2012, 48(1): 70-75.
[2] LI Hongxiao MA Qianqian REN Yuping JIANG Min QIN Gaowu. TERNARY COMPOUNDS AND RELATIVE PHASE EQUILIBRIA IN THE Mg-RICH SIDE OF THE Mg-Zn-Ca SYSTEM[J]. 金属学报, 2011, 47(4): 385-390.
[3] XIE Yu ZHANG Yan CHEN Rongshi HAN Enhou. RELATIONSHIP OF COMPOSITIONS, PHASE CONSTITUENTS AND SOLIDIFICATION PATHS OF CASTING Mg-Al-Zn ALLOYS[J]. 金属学报, 2009, 45(11): 1396-1401.
[4] ;. Research on the ternary compound T1 with low Nd content in the Mg-Zn-Nd alloys[J]. 金属学报, 2008, 44(4): 385-390 .
[5] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[6] LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM[J]. 金属学报, 1998, 34(9): 897-902.
[7] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[8] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[9] QIN Gaowu;HAO Shiming;ZENG Ninghua (Northeastern University;Shenyang 110006)(Manuscript received 1994-11-04;in revised form 1995-05-04). α(α_2)/γ PHASE EQUILIBRIA IN Ti-Al-Ga AND Ti-Al-Nb-Cr SYSTEMS[J]. 金属学报, 1995, 31(23): 484-488.
[10] LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. 金属学报, 1992, 28(7): 50-54.
No Suggested Reading articles found!