| MICROSTRUCTURE OF Ti_(5)Si_3 PHASE AND ITS ORIENTATIONAL RELATIONSHIPS WITH TiAl AND Ti_(3)Al PHASES |
| HE Lianlong; YE Hengqiang(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang); XU Rengen; YANG Dezhuang (Harbin Institute of Technology)(Manuscript received 12 August; 1993; in revised form 28 September; 1993) |
|
Cite this article:
HE Lianlong; YE Hengqiang(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang); XU Rengen; YANG Dezhuang (Harbin Institute of Technology)(Manuscript received 12 August; 1993; in revised form 28 September; 1993). MICROSTRUCTURE OF Ti_(5)Si_3 PHASE AND ITS ORIENTATIONAL RELATIONSHIPS WITH TiAl AND Ti_(3)Al PHASES. Acta Metall Sin, 1994, 30(4): 145-149.
|
|
|
Abstract Alloying element Si can improve the high-temperature creep resistance of the Ti-rich TiAl intermetallic compound. Numerous Ti_(5)Si_3 phase, precipitated as hexagonal foils along the γ-γ and γ-α_2 interfaces in the lamellar structure, was observed by TEM on the hot isostatic pressing TiAl-V-Si alloy compact. The orientation relationships between this precipitating phase and the TiAl and Ti_(3)Al phase are as follows:[0001]_(Ti_(5)Si_3)Correspondenl: HE Lianlong,research assistant , Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110015
|
|
Received: 18 April 1994
|
| 1LipsittHA,ShechtmanD,SchafrikRE.MetallTrans,1975;6A:19912LipsittHA.MaterResSocSympProc,1985;39:3513浦忠杰,蔡其巩,邹敦叙,朱静,仲增墉.见:仲增墉,叶恒强主编,全国首届金属间化合物学术讨论会文集,1989:1984MitaoS,TsugamaS.Proc2ndJapanInter,SAMPESymp,Vol.I,1991:1855WuJS,BeavenPA,WagnerR.ScrMetall,1990;24:2076WuJS,QinGH.ProclstPacificRimInterConfonAdvancedMaterialsandProcessing,Warrendale,PA:TheMinerals,MetalsandMaterialsSociety,1992:7577HeLLYeHQ,NmgXG,CaoMZ,HanD.PhilosMag,1993;67:11618FleischerRW,ZabalaRJ.MetallTrans,1990;21A:1951 |
| No Suggested Reading articles found! |
|
|