| FOAMING BEHAVIOUR OF CaO-SiO_2-Al_2O_3-FeO SLAGS |
| HUANG Zongze; XIAO Xingguo; XIAO Zeqiang(Department of Ferrous Metallurgy; Northeastern University; Shenyang 110006); Singh S D(National Metallurgical Laboratory; Jamshedpur; India 831007)(Manuscript received 1994-04-26) |
|
Cite this article:
HUANG Zongze; XIAO Xingguo; XIAO Zeqiang(Department of Ferrous Metallurgy; Northeastern University; Shenyang 110006); Singh S D(National Metallurgical Laboratory; Jamshedpur; India 831007)(Manuscript received 1994-04-26). FOAMING BEHAVIOUR OF CaO-SiO_2-Al_2O_3-FeO SLAGS. Acta Metall Sin, 1995, 31(19): 289-294.
|
|
|
Abstract The foaming behaviour of CaO-SiO_2-Al_2O_3-FeO slag system reduced by graphite at 1500℃ was quantitatively studied with the help of X-ray apparatus. Foaming parameters such as foaming ratio and foaming index were determined. It was found that with increase of the basicity of slags, the foaming ratio increased, however, the foaming index was opposite. In addition, the effects of additives like MgO, Na_2O and CaF_2 on the foaming behaviour were also investigated. The result of dimensional analysis showed that the foaming index(∑) of molten slag was determined by where μ is the viscosity of the slag,σis the surface tension, ρis the density of the slag and g is the acceleration of gravity. (Correspondent: HUANG Zongze, Department of Ferrous Metallurgy, Northeastern University, Shenyang110006)
|
|
|
| 1CooperCF,KitchenerJA.JIronSteelInst,1959;193(1):482原茂太,生田昌久,北村光章,荻野和巳.铁钢,1983;69(9):11523ItoK,FruehanRJ.MetallTrans,1989;20B(4):5094YoonJK.IntConfonNewSmeltingReductionandNearNetShapeCastingTechnforSteel,Pohang:TheKoreanInstMetals,1990:975OgawaY,KatayamaH,HirataH,TokumitsuN,YamauchiM.ISIJInt,1992;32(1):876JiangR,FruehanRJ.MetallTrans,1991;22B(4):4817黄宗泽,肖兴国,肖泽强.东北大学学报,1994;15(2):1408KeeneBJ,MillsKC.IntMaterRev,1987;32(1):1059GuthrieRIL.EngineeringinProcessMetallurgy,OxfordScienccPublications,1989:15110NakashimaK,MoriK.ISIJInt,1992;32(1):1111UrbainG.SteelRes,1987;58(3):111 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|