界面水解离调控:水系多价金属离子电池新视角
麦立强, 安琴友, 马鑫泉
Interfacial Water Dissociation Regulation: A New Perspective on Aqueous Multivalent Metal-Ion Batteries
MAI Liqiang, AN Qinyou, MA Xinquan
金属学报 . 2026, (8): 1323 -1330 .  DOI: 10.11900/0412.1961.2026.00090