熔盐堆用镍基合金失效机理与改性策略研究进展
王优, 陈向阳, 王煦嘉, 汤春桃, 沈朝, 曾小勤
Progress in Failure Mechanisms and Modification Strategies of Nickel-Based Alloys for Molten Salt Reactors
WANG You, CHEN Xiangyang, WANG Xujia, TANG Chuntao, SHEN Zhao, ZENG Xiaoqin
金属学报
.
2026, (8): 1331
-1346
.
DOI: 10.11900/0412.1961.2025.00407