面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径
吕昭平, 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊
High-Entropy Alloys in Extreme Environments: A Perspective on Advantages, Challenges, and Breakthroughs
LU Zhaoping, SHEN Yaozu, WANG Xianzhen, CHEN Qiang, TANG Jianguo, ZHANG Xiaobin, YU Yong, JIANG Suihe, LIU Xiongjun, WANG Hui, WU Yuan
金属学报 . 2026, (5): 743 -755 .  DOI: 10.11900/0412.1961.2025.00322