可降解镁基复合材料的制备及其在骨科领域的研究进展
欧阳思慧, 佘加, 陈先华, 潘复生
Preparation of Biodegradable Mg-Based Composites and Their Recent Advances in Orthopedic Applications
OUYANG Sihui, SHE Jia, CHEN Xianhua, PAN Fusheng
金属学报 . 2025, (3): 455 -474 .  DOI: 10.11900/0412.1961.2024.00362