合金元素对 α-Fe中H原子溶解及扩散影响的第一性原理研究
宝尔根, 王建韬, 徐文静, 马会, 陈星秋
First-Principles Study on the Influence of Alloying Elements on the Dissolution and Diffusion of Hydrogen Atoms in α-Fe
BAO Ergen, WANG Jiantao, XU Wenjing, MA Hui, CHEN Xing-qiu
金属学报 . 2026, (3): 489 -496 .  DOI: 10.11900/0412.1961.2024.00240