Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 共晶高熵合金快速凝固行为及组织调控
卢健麟, 任化永, 谢桉, 王建潼, 何峰
Rapid Solidification Behavior and Microstructure Regulation of Ni43.5Co19Cr10Fe10Al15Ti2Mo0.5 Eutectic High-Entropy Alloy
LU Jianlin, REN Huayong, XIE An, WANG Jiantong, HE Feng
金属学报
.
2025, (1): 191
-202
.
DOI: 10.11900/0412.1961.2024.00271