固溶后处理对GH4706合金时效析出相演化及力学性能的影响
王冲, 王磊, 段然, 田强, 黄烁, 赵光普
Effects of Solution Post-Treatment on Precipitation Evolution During Aging of GH4706 Alloy and Its Mechanical Properties
WANG Chong, WANG Lei, DUAN Ran, TIAN Qiang, HUANG Shuo, ZHAO Guangpu
金属学报 . 2025, (11): 1638 -1652 .  DOI: 10.11900/0412.1961.2024.00090