MB15镁合金的相组成及其微观形态
张少卿
PHASE CONSTITUTION AND MORPHOLOGIES OF Mg-Zn-Zr ALLOY (MB15)
ZHANG Shaoqing Institute of Aeronautical Materials; Beijing ZHANG Shaoqing; Institute of Aeronautical Materlols. P. O. Box No.81; 100095 Beijing