基于空间站的金属材料研究进展
收稿日期: 2026-03-02
修回日期: 2026-03-31
网络出版日期: 2026-04-16
基金资助
国家自然科学基金项目(52088101);国家重点研发计划项目(2025YFF0520200);载人空间站空间科学与应用项目(KJZ-YY-NCL401);载人空间站空间科学与应用项目(KJZ-YY-NCL0501)
Research Progress of Metallic Materials Under Space Station Conditions
Received date: 2026-03-02
Revised date: 2026-03-31
Online published: 2026-04-16
Supported by
National Natural Science Foundation of China(52088101);National Key Research and Development Program of China(2025YFF0520200);Space Utilization Program of China Manned Space Project(KJZ-YY-NCL401);Space Utilization Program of China Manned Space Project(KJZ-YY-NCL0501)
胡亮 , 王海鹏 , 魏炳波 . 基于空间站的金属材料研究进展[J]. 金属学报, 2026 , 62(5) : 685 -704 . DOI: 10.11900/0412.1961.2026.00062
Outer space provides unique environmental conditions for investigating the physical and chemical properties of metallic materials, the mechanisms of phase transformation processes, and the regulation of microstructure and performance. In particular, it has considerable scientific significance and application value for the preparation of high-temperature, highly active metallic materials, as well as for the implementation of in situ resource utilization and space manufacturing. This study reviews the main research on metallic materials conducted under space experimental conditions since the 1960s and summarizes the materials science experimental platforms and their main functions on the Chinese Space Station, the International Space Station, and the Mir Space Station. Research progress in aspects such as melt flow, liquid properties, solidification structure, and extravehicular exposure is analyzed. The special phenomena and new laws unveiled through space experiments are clarified. Finally, the research and development trends of metallic materials for space manufacturing are prospected.
| [1] | Walter H U, translated by Ge P W, Wang J T. Fluid Sciences and Materials Science in Space [M]. Beijing: China Science and Technology Press, 1991: 243 |
| 瓦尔特著, 葛培文, 王景涛 译. 空间流体科学与空间材料科学 [M]. 北京: 中国科学技术出版社, 1991: 243 | |
| [2] | Ruan Y, Hu L, Yan N, et al. Recent advances and future perspectives of space materials science [J]. Sci. Sin. Technol., 2020, 50: 603 |
| 阮 莹, 胡 亮, 闫 娜 等. 空间材料科学研究进展与未来趋势 [J]. 中国科学: 技术科学, 2020, 50: 603 | |
| [3] | Kurz W, Rappaz M, Trivedi R. Progress in modelling solidification microstructures in metals and alloys. Part II: Dendrites from 2001 to 2018 [J]. Int. Mater. Rev., 2021, 66: 30 |
| [4] | Zhai W, Chang J, Geng D L, et al. Progress and prospect of solidification research for metallic materials [J]. Chin. J. Nonferrous Met., 2019, 29: 1953 |
| 翟 薇, 常 健, 耿德路 等. 金属材料凝固过程研究现状与未来展望 [J]. 中国有色金属学报, 2019, 29: 1953 | |
| [5] | Mohr M, Dong Y, Bracker G P, et al. Electromagnetic levitation containerless processing of metallic materials in microgravity: Thermophysical properties [J]. npj Microgravity, 2023, 9: 34 |
| [6] | Matson D M, Battezzati L, Galenko P K, et al. Electromagnetic levitation containerless processing of metallic materials in microgravity: Rapid solidification [J]. npj Microgravity, 2023, 9: 65 |
| [7] | Gu Y D, Gao M, Zhao G H, et al. Recent progress in space science and applications on Chinese Space Station in 2022-2024 [J]. Chin. J. Space Sci., 2024, 44: 607 |
| [8] | Yu J D, Zhang W, Yang S, et al. Recent advances and future prospects of Space Materials Science [J]. Rev. Mater. Res., 2025, 1: 100065 |
| [9] | Da D A, Huang L P, Xie X, et al. First material processing experiment in space microgravity made by China [J]. Chin. Space Sci. Technol., 1988, 8(6): 4 |
| 达道安, 黄良甫, 谢 燮 等. 我国首次空间微重力下的材料加工试验 [J]. 中国空间科学技术, 1988, 8(6): 4 | |
| [10] | Ge P W, Nishinaga T, Li C R, et al. Growth of GaSb single crystal in space [J]. Sci. China, 2001, 31A: 56 |
| 葛培文, 西永颂, 李超荣 等. GaSb单晶空间生长 [J]. 中国科学, 2001, 31A: 56 | |
| [11] | Yin Z G, Zhang X W, Pan X H. Crystal growth from melts: Materials science program in the SJ-10——Recoverable scientific experiment satellite [J]. Physics, 2016, 45: 213 |
| 尹志岗, 张兴旺, 潘秀红. 空间熔体材料科学: 实践十号返回式科学实验卫星 [J]. 物理, 2016, 45: 213 | |
| [12] | Zhang X W, Yin Z G, Yu J D, et al. Space materials science in China: I. Experiment studies under microgravity [J]. Chin. J. Space Sci., 2020, 40: 946 |
| [13] | Zhang P, Zhang Y, Wang Z L, et al. 1D and 3D co-simulation and self-adaptive position control of electrostatic levitation in China's Space Station [J]. npj Microgravity, 2022, 8: 29 |
| [14] | Wang D S, Lv H Y, Hu M, et al. In-orbit flight tests of operational behavior of space lubricated bearings [J]. Bearing, 2025, (4): 80 |
| 王德生, 吕宏宇, 胡 明 等. 空间润滑轴承运转行为的在轨飞行试验 [J]. 轴承, 2025, (4): 80 | |
| [15] | Enz T, Steinbach S, Simicic D, et al. First experiments using the materials science laboratory on board the International Space Station [J]. Microgravity Sci. Technol., 2011, 23: 345 |
| [16] | Jarvis D J, Voss D. IMPRESS Integrated Project—An overview paper [J]. Mater. Sci. Eng., 2005, A413-414: 583 |
| [17] | Zimmermann G, Sturz L, Billia B, et al. Investigation of columnar-to-equiaxed transition in solidification processing of AlSi alloys in microgravity—The CETSOL project [J]. J. Phys. Conf. Ser., 2011, 327: 012003 |
| [18] | Friedrich J, Dagner J, Hainke M, et al. Numerical modeling of crystal growth and solidification experiments carried out under microgravity conditions [J]. Cryst. Res. Technol., 2003, 38: 726 |
| [19] | Seidel A, Soellner W, Stenzel C. EML—An electromagnetic levitator for the International Space Station [J]. J. Phys. Conf. Ser., 2011, 327: 012057 |
| [20] | Soellner W, Seidel A, Stenzel C, et al. EML-containerless processing facility for material science research onboard the ISS [J]. J. Japan Soc. Microgravity Appl., 2010, 27: 183 |
| [21] | Hu L, Lu X Y, Hou Z M. Progress in electrostatic levitation technology [J]. Physics, 2007, 36: 944 |
| 胡 亮, 鲁晓宇, 侯智敏. 静电悬浮技术研究进展 [J]. 物理, 2007, 36: 944 | |
| [22] | Paradis P F, Ishikawa T, Lee G W, et al. Materials properties measurements and particle beam interactions studies using electrostatic levitation [J]. Mater. Sci. Eng., 2014, R76: 1 |
| [23] | Rhim W K, Chung S K, Barber D, et al. An electrostatic levitator for high-temperature containerless materials processing in 1-g [J]. Rev. Sci. Instrum., 1993, 64: 2961 |
| [24] | Meister T, Lohoefer G, Unbehauen H, Development of an electrostatic levitator for containerless processing [J]. Acta Photonica Sin., 1999, 28: 14 |
| [25] | Sung Y S, Takeya H, Togano K. Containerless solidification of Si, Zr, Nb, and Mo by electrostatic levitation [J]. Rev. Sci. Instrum., 2001, 72: 4419 |
| [26] | Hu L, Wang H P, Xie W J, et al. Electrostatic levitation under the single-axis feedback control condition [J]. Sci. China Phys. Mech. Astron., 2010, 53: 1438 |
| [27] | Lee G W, Jeon S, Park C, et al. Crystal-liquid interfacial free energy and thermophysical properties of pure liquid Ti using electrostatic levitation: Hypercooling limit, specific heat, total hemispherical emissivity, density, and interfacial free energy [J]. J. Chem. Thermodyn., 2013, 63: 1 |
| [28] | Ishikawa T, Okada J T, Watanebe Y, et al. Thermophysical property measurements of oxide melts at high temperature by electrostatic levitation furnace on the ISS [J]. Int. J. Microgravity Sci. Appl., 2015, 32: 320410 |
| [29] | Tamaru H, Koyama C, Saruwatari H, et al. Status of the electrostatic levitation furnace (ELF) in the ISS-KIBO [J]. Microgravity Sci. Technol., 2018, 30: 643 |
| [30] | Grugel R N, Luz P, Smith G, et al. Materials research conducted aboard the International Space Station: Facilities overview, operational procedures, and experimental outcomes [J]. Acta Astronaut., 2008, 62: 491 |
| [31] | Nguyen-Thi H, Reinhart G, Salloum Abou Jaoude G, et al. XRMON-GF: A novel facility for solidification of metallic alloys with in situ and time-resolved X-ray radiographic characterization in microgravity conditions [J]. J. Cryst. Growth, 2013, 374: 23 |
| [32] | Murphy A G, Mathiesen R H, Houltz Y, et al. Direct observation of spatially isothermal equiaxed solidification of an Al-Cu alloy in microgravity on board the MASER 13 sounding rocket [J]. J. Cryst. Growth, 2016, 454: 96 |
| [33] | Schlagheck R A, Trach B L. Microgravity research results and experiences from the NASA/MIR space station program [J]. Acta Astronaut., 2003, 53: 983 |
| [34] | Shirkhanzadeh M. Analysis of the data obtained from liquid metal diffusion experiments conducted on the MIR space station [J]. Acta Astronaut., 2009, 64: 256 |
| [35] | Stoichev N V, Yaneva S B, Regel L L, et al. Eutectic solidification of Al-Cu alloys influenced by convection [J]. Adv. Space Res., 1988, 8: 171 |
| [36] | Bewersdorff A, G?rler G P, Otto G, et al. Solidification of silver-germanium alloys in an amorphous matrix aboard the Space Station Mir [J]. Acta Astronaut., 1993, 29: 547 |
| [37] | Weiβ A, Zimmermann G, Camel D. Investigation on solidification structures in the TITUS furnace onboard the MIR station [A]. Proceedings of the First International Symposium on Microgravity Research and Applications in Physical Sciences and Biotechnology [C]. Sorrento, Italy: European Space Agency, 2000: 683 |
| [38] | Napolitano L G. Marangoni convection in space microgravity environments [J]. Science, 1984, 225: 197 |
| [39] | Arafune K, Hirata A. Thermal and solutal Marangoni convection in In-Ga-Sb system [J]. J. Cryst. Growth, 1999, 197: 811 |
| [40] | Okano Y, Umemura S, Enomoto Y, et al. Numerical study of Marangoni convection effect on the melting of GaSb/InSb/GaSb [J]. J. Cryst. Growth, 2002, 235: 135 |
| [41] | Matson D M, Xiao X, Rodriguez J E, et al. Use of thermophysical properties to select and control convection during rapid solidification of steel alloys using electromagnetic levitation on the space station [J]. JOM, 2017, 69: 1311 |
| [42] | Hyers R W, Trapaga G, Abedian B. Laminar-turbulent transition in an electromagnetically levitated droplet [J]. Metall. Mater. Trans., 2003, 34B: 29 |
| [43] | Song S P, Li B Q. Free surface profiles and thermal convection in electrostatically levitated droplets [J]. Int. J. Heat Mass Transfer., 2000, 43: 3589 |
| [44] | Hyers R W. Fluid flow effects in levitated droplets [J]. Meas. Sci. Technol., 2005, 16: 394 |
| [45] | Chang J, Wang H P, Liao H, et al. Remarkable undercooling capability and metastable thermophysical properties of liquid Nb84.1Si15.9 alloy revealed by electrostatic levitation in outer space [J]. Rev. Sci. Instrum., 2024, 95: 034501 |
| [46] | Wang H P, Hu L, Xie W J, et al. Metastable liquid properties and surface flow patterns of ultrahigh temperature alloys explored in outer space [J]. Angew. Chem. Int. Ed., 2024, 63: e202400312 |
| [47] | Zhao J Z, Sun H, Zhang L L, et al. In-situ composite microstructure formation of immiscible alloy solidified in space [J]. Natl. Sci. Rev., 2023, 10: nwac261 |
| [48] | Hibiya T, Egry I. Thermophysical property measurements of high temperature melts: Results from the development and utilization of space [J]. Meas. Sci. Technol., 2005, 16: 317 |
| [49] | Bracker G P, Luo Y, Damaschke B, et al. Examining the influence of turbulence on viscosity measurements of molten germanium under reduced gravity [J]. npj Microgravity, 2022, 8: 53 |
| [50] | Xiao X, Brillo J, Lee J, et al. Impact of convection on the damping of an oscillating droplet during viscosity measurement using the ISS-EML facility [J]. npj Microgravity, 2021, 7: 36 |
| [51] | Nawer J, Ishikawa T, Oda H, et al. Uncertainty analysis and performance evaluation of thermophysical property measurement of liquid Au in microgravity [J]. npj Microgravity, 2023, 9: 38 |
| [52] | Hu J L, Wang P, Huang F Q, et al. Gravitational effects and key issues in melt diffusion measurements [J]. Sci. Sin. Technol., 2025, 55: 2041 |
| 胡金亮, 王 鹏, 黄非奇 等. 熔体扩散测量中的重力效应与关键问题 [J]. 中国科学: 技术科学, 2025, 55: 2041 | |
| [53] | Frohberg G, Kraatz K H, Wever H. Selfdiffusion of Sn112 and Sn124 in liquid tin [A]. Proceedings of the 5th European Symposium on Materials Sciences Under Microgravity [C]. Schlo? Elmau: European Space Agency, 1984: 201 |
| [54] | Mohr M, Fecht H J. Investigating thermophysical properties under microgravity: A review [J]. Adv. Eng. Mater., 2021, 23: 2170006 |
| [55] | Mohr M, Wunderlich R, Dong Y, et al. Thermophysical properties of advanced Ni-based superalloys in the liquid state measured on board the International Space Station [J]. Adv. Eng. Mater., 2020, 22: 1901228 |
| [56] | Nawer J, Stanford B, Kolbe M, et al. Thermodynamic assessment of evaporation during molten steel testing onboard the International Space Station [J]. npj Microgravity, 2024, 10: 77 |
| [57] | Watanabe M, Onodera K, Tanaka K, et al. Interfacial phenomena and thermophysical properties of molten steel and oxides [J]. Int. J. Microgravity Sci. Appl., 2016, 33: 330212 |
| [58] | Ishikawa T, Oda H, Koyama C, et al. Density of a molten stainless Steel-B4C Alloy measured in the electrostatic levitation furnace onboard the International Space Station [J]. Int. J. Microgravity Sci. Appl., 2025, 42: 420202 |
| [59] | Seimiya Y, Kobatake H, Tono-Oka K, et al. Thermophysical properties of molten Fe-Cu alloy measured using the electrostatic levitation furnace aboard the International Space Station (ISS-ELF) under microgravity conditions [J]. ISIJ Int., 2024, 64: 2253 |
| [60] | Hu L, Xie W J, Wan Z X, et al. Space station based experimental research on thermophysical properties and solidification mechanisms of Fe-19%Si alloy [J]. Rev. Mater. Res., 2025, 1: 100005 |
| [61] | Mohr M, Wunderlich R, Novakovic R, et al. Precise measurements of thermophysical properties of liquid Ti-6Al-4V (Ti64) alloy on board the International Space Station [J]. Adv. Eng. Mater., 2020, 22: 2000169 |
| [62] | Wunderlich R K, Mohr M, Dong Y, et al. Thermophysical properties of the TiAl-2Cr-2Nb alloy in the liquid phase measured with an electromagnetic levitation device on board the International Space Station, ISS-EML [J]. Int. J. Mater. Res., 2021, 112: 770 |
| [63] | Wunderlich R K, Hecht U, Hediger F, et al. Surface Tension, Viscosity, and selected thermophysical properties of Ti48Al48Nb2Cr2, Ti46Al46Nb8, and Ti46Al46Ta8 from microgravity experiments [J]. Adv. Eng. Mater., 2018, 20: 1800346 |
| [64] | Liu D N, Wang H P, Liao H, et al. Wrinkled shrinkage on surface monophasic structure of floating refractory alloy droplets solidified in space environment [J]. Adv. Funct. Mater., 2025, 35: 2415364 |
| [65] | Snyder R S. Second International Microgravity Laboratory (IML-2) final report [R]. Washington: National Aeronautics and Space Administration, 1997 |
| [66] | Robinson M B. Microgravity Science Laboratory (MSL-1) final report [R]. Huntsville, Alabama: NASA Marshall Space Flight Center, 1998 |
| [67] | Wunderlich R K, Fecht H J. Thermophysical properties of bulk metallic glass forming alloys in the stable and undercooled liquid—A microgravity investigation [J]. Mater. Trans., 2001, 42: 565 |
| [68] | Mohr M, Wunderlich R K, Zweiacker K, et al. Surface tension and viscosity of liquid Pd43Cu27Ni10P20 measured in a levitation device under microgravity [J]. npj Microgravity, 2019, 5: 4 |
| [69] | Mohr M, Wunderlich R K, Koch S, et al. Surface tension and viscosity of Cu50Zr50 measured by the oscillating drop technique on board the International Space Station [J]. Microgravity Sci. Technol., 2019, 31: 177 |
| [70] | Van Hoesen D C, Gangopadhyay A K, Loh?fer G, et al. Resistivity saturation in metallic liquids above a dynamical crossover temperature observed in measurements aboard the international space station [J]. Phys. Rev. Lett., 2019, 123: 226601 |
| [71] | Mohr M, Wunderlich R K, Hofmann D C, et al. Thermophysical properties of liquid Zr52.5Cu17.9Ni14.6Al10Ti5—Prospects for bulk metallic glass manufacturing in space [J]. npj Microgravity, 2019, 5: 24 |
| [72] | Mohr M, Hofmann D C, Fecht H J. Thermophysical properties of an Fe57.75Ni19.25Mo10C5B8 glass-forming alloy measured in microgravity [J]. Adv. Eng. Mater., 2021, 23: 2001143 |
| [73] | Nawer J, Matson D M. Quantifying facility performance during thermophysical property measurement of liquid Zr using Electrostatic Levitation [J]. High Temp.-High Pressures, 2023, 52: 123 |
| [74] | Nawer J, Ishikawa T, Oda H, et al. Uncertainty quantification of thermophysical property measurement in space and on earth: A study of liquid platinum using electrostatic levitation [J]. J. Astron. Space Sci., 2023, 40: 93 |
| [75] | Wang H P, Liao H, Wang Y B, et al. Solidification mechanism and microstructure evolution of refractory Nb-Si and Nb-Si-Zr alloys aboard China Space Station [J]. Sci. Sin. Technol., 2025, 55: 1989 |
| 王海鹏, 廖 晖, 王彦博 等. 中国空间站难熔Nb-Si和Nb-Si-Zr合金凝固组织形成机理研究 [J]. 中国科学: 技术科学, 2025, 55: 1989 | |
| [76] | Nguyen Thi H, Dabo Y, Drevet B, et al. Directional solidification of Al-1.5 wt% Ni alloys under diffusion transport in space and fluid-flow localisation on earth [J]. J. Cryst. Growth, 2005, 281: 654 |
| [77] | Nabavizadeh S A, Upadhyay S, Eshraghi M, et al. Spurious grain formation due to Marangoni convection during directional solidification of alloys in μ-g environment of International Space Station [J]. J. Cryst. Growth, 2021, 574: 126334 |
| [78] | Ghods M, Upadhyay S R, Rajamure R S, et al. Primary dendrite array morphology in Al-7 wt% Si alloy samples directionally solidified aboard the International Space Station [J]. J. Cryst. Growth, 2021, 562: 126077 |
| [79] | Li Y Z, Mangelinck-No?l N, Zimmermann G, et al. Modification of the microstructure by rotating magnetic field during the solidification of Al-7 wt.% Si alloy under microgravity [J]. J. Alloys Compd., 2020, 836: 155458 |
| [80] | Jia Y L, Zhang Y J, Shi Z K, et al. Review of the formation mechanism and control technology for freckle defects in directionally solidified superalloys [J]. Acta Metall. Sin., 2026, 62: 309 |
| 贾玉亮, 张勇佳, 史泽楷 等. 高温合金定向凝固雀斑形成机理及控制技术研究进展 [J]. 金属学报, 2026, 62: 309 | |
| [81] | Liu D R, Mangelinck-No?l N, Gandin C A, et al. Structures in directionally solidified Al-7 wt.% Si alloys: Benchmark experiments under microgravity [J]. Acta Mater., 2014, 64: 253 |
| [82] | Mirihanage W U, Browne D J, Zimmermann G, et al. Simulation of international space station microgravity directional solidification experiments on columnar-to-equiaxed transition [J]. Acta Mater., 2012, 60: 6362 |
| [83] | Li Y Z, Mangelinck-No?l N, Zimmermann G, et al. Comparative study of directional solidification of Al-7?wt% Si alloys in Space and on Earth: Effects of gravity on dendrite growth and Columnar-to-equiaxed transition [J]. J. Cryst. Growth, 2019, 513: 20 |
| [84] | Murphy A G, Reinhart G, Nguyen-Thi H, et al. Meso-scale modelling of directional solidification and comparison with in situ X-ray radiographic observations made during the MASER-12 XRMON microgravity experiment [J]. J. Alloys Compd., 2013, 573: 170 |
| [85] | Abou-Khalil L, Salloum-Abou-Jaoude G, Reinhart G, et al. Influence of gravity level on columnar-to-equiaxed transition during directional solidification of Al-20 wt.% Cu alloys [J]. Acta Mater., 2016, 110: 44 |
| [86] | Ngomesse F, Reinhart G, Soltani H, et al. In situ investigation of the columnar-to-equiaxed transition during directional solidification of Al-20 wt.%Cu alloys on Earth and in microgravity [J]. Acta Mater., 2021, 221: 117401 |
| [87] | Pan M X, Li S P, Zhao D Q, et al. Directional growth of Al-Mg2Si eutectic alloy in the SZ2 unmanned spaceship [J]. Sci. China, 2003, 46A: 158 |
| 潘明祥, 李顺朴, 赵德乾 等. Al-Mg2Si共晶合金在“神舟2号”飞船上定向复合生长 [J]. 中国科学, 2002, 32A: 725 | |
| [88] | Luo X H, Huang Q, Liu B D, et al. Al-Al3Ni eutectic alloy and Al/WC(Ni) composite directionally solidified under microgravity and normal gravity [J]. Adv. Space Res., 2003, 32: 225 |
| [89] | Bottin-Rousseau S, Witusiewicz V T, Hecht U, et al. Coexistence of rod-like and lamellar eutectic growth patterns [J]. Scr. Mater., 2022, 207: 114314 |
| [90] | Hofmeister W H, Bayuzick R J, Hyers R, et al. Cavitation-induced nucleation of zirconium in low earth orbit [J]. Appl. Phys. Lett., 1999, 74: 2711 |
| [91] | Bracker G P, Schneider S, Wunderlich R, et al. Confirmation of anomalous nucleation in zirconium [J]. JOM, 2020, 72: 3140 |
| [92] | Gangopadhyay A K, Sellers M E, Bracker G P, et al. Demonstration of the effect of stirring on nucleation from experiments on the International Space Station using the ISS-EML facility [J]. npj Microgravity, 2021, 7: 31 |
| [93] | Gangopadhyay A K, Sheng Y, Bracker G P, et al. Slower nucleation kinetics with stirring in a supercooled Zr80Pt20 liquid-Terrestrial and microgravity experiments on the International Space Station [J]. J. Chem. Phys., 2025, 162: 134502 |
| [94] | Hermann R, L?ser W, Lindenkreuz H G, et al. Metastable phase formation in undercooled Fe-Co melts under terrestrial and parabolic flight conditions [J]. Microgravity Sci. Technol., 2007, 19: 5 |
| [95] | L?ser W, Woodcock T G, Shuleshova O, et al. Metastable solidification in undercooled liquid droplets of Fe-Ni based soft-magnetic alloys under terrestrial and microgravity conditions [J]. J. Phys. Conf. Ser., 2011, 327: 012005 |
| [96] | Galenko P K, Alexandrov D V, Toropova L V. Dendrite growth under a forced convective flow: A review [J]. Phys. Rep., 2024, 1085: 1 |
| [97] | Galenko P K, Toropova L V, Alexandrov D V, et al. Anomalous kinetics, patterns formation in recalescence, and final microstructure of rapidly solidified Al-rich Al-Ni alloys [J]. Acta Mater., 2022, 241: 118384 |
| [98] | Binder S. Undercooling and solidification of tetragonal Ni2B under different convective flow conditions [D]. Bochum: Ruhr University Bochum, 2010 |
| [99] | Galenko P K, Wonneberger R, Koch S, et al. Bell-shaped “dendrite velocity-undercooling” relationship with an abrupt drop of solidification kinetics in glass forming Cu-Zr(-Ni) melts [J]. J. Cryst. Growth, 2020, 532: 125411 |
| [100] | Wang H P, Liao H, Chang J, et al. Decoupling effect stimulated independent dendrite growth of eutectic phases under microgravity and containerless states [J]. Mater. Today, 2024, 75: 386 |
| [101] | Wang H P, Zheng C H, Hu L, et al. Outer space cultivated regular eutectic cells with anomalous internal microstructures for rapidly solidifying Zr50V50 hypereutectic alloy [J]. J. Appl. Phys., 2025, 137: 045104 |
| [102] | Wang H P, Li H Z, Zheng C H, et al. Eutectic growth kinetics and microscopic mechanical property of refractory Zr57V43 alloy under space and ground conditions [J]. Acta Mater., 2025, 295: 121213 |
| [103] | Zhu B F, Li C Y, Zhang S J, et al. Numerical simulation of the dynamic contraction of dendrite solidification in the Al-4.7%Cu alloy [J]. Acta Metall. Sin., 2026, 62: 509 |
| 朱宝丰, 李晨宇, 张士杰 等. Al-4.7%Cu合金枝晶凝固动态收缩的数值模拟 [J]. 金属学报, 2026, 62: 509 | |
| [104] | Wang H P, Liao H, Hu L, et al. Freezing shrinkage dynamics and surface dendritic growth of floating refractory alloy droplets in outer space [J]. Adv. Mater., 2024, 36: 2313162 |
| [105] | Wang H P, Liu D N, Zheng C H, et al. Spiral eutectic growth dynamics facilitated by space Marangoni convection and liquid surface wave [J]. Phys. Fluids, 2024, 36: 047137 |
| [106] | Jiang H X, Li W, Zhang L L, et al. Progress in the solidification of monotectic alloys under the microgravity condition of space [J]. Sci. Sin. Phys. Mech. Astron., 2020, 50: 047005 |
| 江鸿翔, 黎 旺, 张丽丽 等. 空间微重力条件下偏晶合金凝固研究进展 [J]. 中国科学: 物理学 力学 天文学, 2020, 50: 047005 | |
| [107] | Li W, Jiang H X, Zhang L L, et al. Solidification of Al-Bi-Sn immiscible alloy under microgravity conditions of space [J]. Scr. Mater., 2019, 162: 426 |
| [108] | Samwel S W. Low earth orbital atomic oxygen erosion effect on spacecraft materials [J]. Space Res. J., 2014, 7: 1 |
| [109] | Polturak E, Koren G, Ayalon M, et al. Design and performance of a space based high temperature superconductivity experiment [J]. Appl. Phys. Lett., 1999, 75: 1293 |
| [110] | Su Y, Li Y X, Zeng X Q. Progress in the study of radiation-resistant high-strength magnesium alloys for space station extravehicular exposure [J]. Sci. Sin. Technol., 2025, 55: 2101 |
| 苏 阳, 李扬欣, 曾小勤. 抗辐射高强韧镁合金的空间站舱外暴露研究进展 [J]. 中国科学: 技术科学, 2025, 55: 2101 | |
| [111] | Wang X L, Zhou F, Liu W M. Effects of atomic oxygen and ultraviolet in low earth orbit on low surface energy polymer film [J]. J. Appl. Polym. Sci., 2011, 120: 329 |
| [112] | Gao X M, Hu M, Sun J Y, et al. Changes in the structure and tribological property of Ag film by LEO space environment exposure [J]. Appl. Surf. Sci., 2014, 320: 466 |
| [113] | Liu R P, Zhang X Y, Zhao J H, et al. Solute distribution characteristics of Pd40Ni40P20 alloy solidified in microgravity and gravity conditions [J]. Acta Phys. Sin., 1997, 46: 819 |
| 刘日平, 张湘义, 赵建华 等. 重力及微重力条件下Pd40Ni40P20合金凝固组织中溶质原子的分布特征 [J]. 物理学报, 1997, 46: 819 | |
| [114] | Wen P, Wang B B, Ding D W, et al. Research progress on some basic problems of bulk metallic glass under microgravity [J]. Mater. China, 2017, 36: 880 |
| 闻 平, 王彬彬, 丁大伟 等. 微重力条件下块体金属玻璃的若干基础问题研究进展 [J]. 中国材料进展, 2017, 36: 880 | |
| [115] | Olive J R, Hofmeister W H, Bayuzick R J, et al. Formation of tetragonal YBa2Cu3O7 - δ from an undercooled melt [J]. J. Mater. Res., 1994, 9: 1 |
| [116] | Bitterlich H, L?ser W, Lindenkreuz H G, et al. Superconducting YNi2B2C- and YPd2B2C-phase formation from undercooled melts [J]. J. Alloys Compd., 2001, 325: 285 |
| [117] | Feng J C, Wang H Q, Zhang B G, et al. Research status and prospect of space welding technology [J]. Trans. China Weld. Inst., 2015, 36(6): 107 |
| 冯吉才, 王厚勤, 张秉刚 等. 空间焊接技术研究现状及展望 [J]. 焊接学报, 2015, 36(6): 107 | |
| [118] | Zhang Y Y, Zhang W, Wang G. Discussion on the technical demands and application modes of additive manufacturing in space [J]. Mater. China, 2017, 36: 503 |
| 张颖一, 张 伟, 王 功. 太空增材制造的技术需求和应用模式探索 [J]. 中国材料进展, 2017, 36: 503 | |
| [119] | Zocca A, Lüchtenborg J, Mühler T, et al. Enabling the 3D printing of metal components in μ-gravity [J]. Adv. Mater. Technol., 2019, 4: 1900506 |
| [120] | Kovalchuk D, Melnyk V, Melnyk I. A coaxial wire-feed additive manufacturing of metal components using a profile electron beam in space application [J]. J. Mater. Eng. Perform., 2022, 31: 6069 |
| [121] | Li B B, Wang B W, Zhu G, et al. Low-roughness-surface additive manufacturing of metal-wire feeding with small power [J]. Materials, 2021, 14: 4265 |
| [122] | Gradl P, Mireles O R, Katsarelis C, et al. Advancement of extreme environment additively manufactured alloys for next generation space propulsion applications [J]. Acta Astronaut., 2023, 211: 483 |
| [123] | Hoffmann M, Ye J H, Elwany A. Selective deposition and fusion of AISI 316L: An additive manufacturing process for space environments via direct ink writing and laser processing [J]. J. Manuf. Sci. Eng., 2024, 146: 121006 |
| [124] | Roberts C, McGill P, Foreman L, et al. Material characterization of additively manufactured Ti-6Al-4V parts for an environmental control and life support system in space flight hardware [J]. Mater. Perform. Charact., 2020, 9: 714 |
| [125] | Mohammed S M A K, Li Z H, Orikasa K, et al. Neutron radiation induced transmutation of boron to lithium in aluminum-boron nitride composite [J]. Mater. Today Adv., 2025, 25: 100551 |
| [126] | Meng S K, Zhu R S, Zheng H L, et al. Property evolution and service life prediction of novel metallic materials for future lunar bases [J]. Rare Met., 2024, 43: 5318 |
| [127] | Jiang X, Xue D Z, Bai Y, et al. AI4Materials: Transforming the landscape of materials science and enigneering [J]. Rev. Mater. Res., 2025, 1: 100010 |
/
| 〈 |
|
〉 |