综述

跨尺度协同增强铝基复合材料研究进展

  • 欧阳求保 ,
  • 苏楠 ,
  • 王瑞安 ,
  • 刘侃 ,
  • 张荻
展开
  • 上海交通大学 材料科学与工程学院 金属基复合材料全国重点实验室 上海 200240
欧阳求保,男,1967年生,教授,博士
张 荻,zhangdi@sjtu.edu.cn,主要从事金属基复合材料研究

收稿日期: 2025-10-20

  修回日期: 2026-02-10

  网络出版日期: 2026-04-16

基金资助

国家重点研发计划项目(2023YFB4606200);国家自然科学基金项目(52192595);上海交通大学2030计划项目

Research Progress on Cross-Scale Synergistically Reinforced Aluminum Matrix Composites

  • OUYANG Qiubao ,
  • SU Nan ,
  • WANG Ruian ,
  • LIU Kan ,
  • ZHANG Di
Expand
  • National Key Laboratory of Metal Matrix Composites, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
ZHANG Di, professor, Tel: 13501719680, E-mail: zhangdi@sjtu.edu.cn

Received date: 2025-10-20

  Revised date: 2026-02-10

  Online published: 2026-04-16

Supported by

National Key Research and Development Program of China(2023YFB4606200);National Natural Science Foundation of China(52192595);Shanghai Jiao Tong University 2030 Initiative

摘要

铝基复合材料因其高比强度、高比模量、良好的导热性及可控的热膨胀系数等优点,在航空航天、汽车工业和电子封装等领域展现出广阔的应用前景。然而,传统的单一尺度增强体在提升材料强度的同时,往往导致塑性、韧性显著下降,这一强韧性矛盾制约了其进一步发展。近年来,受自然生物材料多级结构启发的“跨尺度协同增强”策略为解决这一瓶颈提供了新思路。该策略通过将微米尺度和纳米尺度增强体进行协同复合,构建多级结构,旨在同时实现材料高强度、高模量及良好塑韧性的结合。本文系统综述了跨尺度协同增强铝基复合材料的研究进展,阐述了跨尺度协同的设计理念,讨论了主要的材料体系及关键制备技术,剖析了跨尺度协同增强的机理,并对未来研究方向进行了展望,旨在为高性能铝基复合材料的设计和开发提供理论参考。

本文引用格式

欧阳求保 , 苏楠 , 王瑞安 , 刘侃 , 张荻 . 跨尺度协同增强铝基复合材料研究进展[J]. 金属学报, 2026 , 62(5) : 733 -742 . DOI: 10.11900/0412.1961.2025.00321

Abstract

Aluminum matrix composites, due to their high specific strength and modulus, excellent thermal conductivity, and controllable thermal expansion coefficient, show prospective broad applications in aerospace, automotive, and electronic packaging. However, traditional single-scale reinforcements often enhance material strength while reducing plasticity and toughness. This strength-toughness trade-off limits further material development. This bottleneck can potentially be overcome through an approach based on the recently developed “cross-scale synergistically reinforcement” strategy, inspired by the multiscale structures of natural biological materials. By the synergistic combination of micron- and nano-scale reinforcements into multiscale structures, the strategy aims to simultaneously enhance strength, modulus, plasticity, and toughness. This paper systematically reviews the research progress on cross-scale synergistic reinforcement in aluminum matrix composites. Additionally, this paper elucidates the design philosophy of cross-scale synergy, discusses the primary material systems, key fabrication techniques, and underlying mechanisms of cross-scale synergistic reinforcement, and outlines future research directions. Finally, this paper aims to provide theoretical guidance for the design and development of high-performance aluminum matrix composites.

参考文献

[1] Wang X S, Wang X Z, Liu K, et al. Effect of the CNTs into SiCp-Al interfacial micro-zones on ageing precipitation behavior, microstructure and mechanical properties of SiCp(CNT)/Al-Zn-Mg-Cu composites [J]. Composites, 2023, 259B: 110708
[2] Li S S, Su Y S, Zhu X H, et al. Enhanced mechanical behavior and fabrication of silicon carbide particles covered by in-situ carbon nanotube reinforced 6061 aluminum matrix composites [J]. Mater. Des., 2016, 107: 130
[3] Guan L C R, Cao H, Su Y, et al. Enhanced strength-ductility synergy of SiC particles reinforced aluminum matrix composite via dual configuration design of reinforcement and matrix [J]. Mater. Des., 2024, 245: 113186
[4] Ma Z Y, Xiao B L, Zhang J F, et al. Overview of research and development for aluminum matrix composites driven by aerospace equipment demand [J]. Acta Metall. Sin., 2023, 59: 457
  马宗义, 肖伯律, 张峻凡 等. 航天装备牵引下的铝基复合材料研究进展与展望 [J]. 金属学报, 2023, 59: 457
[5] Wu Z Y, Shao H F, Cai C C, et al. Tensile and fracture behaviors of stitched twill carbon fabric structure reinforced aluminum matrix composites at elevated temperature [J]. Acta Metall. Sin., 2025, 61: 1387
  吴志勇, 邵徽凡, 蔡长春 等. 斜纹碳布缝合织物结构增强铝基复合材料的高温拉伸及断裂行为 [J]. 金属学报, 2025, 61: 1387
[6] Cai Y P, Su Y S, Liu K, et al. Effect of Sc microalloying on fabrication, microstructure and mechanical properties of SiCp/Al-Cu-Mg-Sc composites via powder metallurgy [J]. Mater. Sci. Eng., 2023, A877: 145152
[7] Hua A D, Su Y S, Cai Y P, et al. Fabrication, microstructure characterization and mechanical properties of B4C microparticles and SiC nanowires hybrid reinforced aluminum matrix composites [J]. Mater. Charact., 2022, 193: 112243
[8] Zhang Z M, Fan G L, Tan Z Q, et al. Towards the strength-ductility synergy of Al2O3/Al composite through the design of roughened interface [J]. Composites, 2021, 224B: 109251
[9] Liu K, Su Y S, Wang X Z, et al. Achieving simultaneous enhancement of strength and ductility in Al matrix composites by employing the synergetic strengthening effect of micro- and nano-SiCps [J]. Composites, 2023, 248B: 110350
[10] Wang X S, Su Y S, Qiu C H, et al. Mechanical behavior and interfacial micro-zones of SiCp(CNT) hybrid reinforced aluminum matrix composites [J]. Mater. Charact., 2022, 189: 111982
[11] Ma Y, Chen H, Zhang M X, et al. Break through the strength-ductility trade-off dilemma in aluminum matrix composites via precipitation-assisted interface tailoring [J]. Acta Mater., 2023, 242: 118470
[12] Yi C L, Chen X M, Gou F L, et al. Direct measurements of the mechanical strength of carbon nanotube-aluminum interfaces [J]. Carbon, 2017, 125: 93
[13] Zhou T, Lei M, Xu J. Recent progress in the development and properties of aluminum matrix composites reinforced with graphene: A review [J]. Mater. Today Sustain., 2024, 25: 100674
[14] Zhang X, Li S F, Pan B, et al. A novel strengthening effect of in-situ nano Al2O3w on CNTs reinforced aluminum matrix nanocomposites and the matched strengthening mechanisms [J]. J. Alloys Compd., 2018, 764: 279
[15] He H Y, Fan G L, Saba F, et al. Enhanced distribution and mechanical properties of high content nanoparticles reinforced metal matrix composite prepared by flake dispersion [J]. Composites, 2023, 252B: 110514
[16] Bakshi S R, Lahiri D, Agarwal A. Carbon nanotube reinforced metal matrix composites—A review [J]. Int. Mater. Rev., 2010, 55: 41
[17] Jiang L, Li Z Q, Fan G L, et al. Strong and ductile carbon nanotube/aluminum bulk nanolaminated composites with two-dimensional alignment of carbon nanotubes [J]. Scr. Mater., 2012, 66: 331
[18] Li S S, Su Y S, Ouyang Q B, et al. In-situ carbon nanotube-covered silicon carbide particle reinforced aluminum matrix composites fabricated by powder metallurgy [J]. Mater. Lett., 2016, 167: 118
[19] Li S S, Su Y S, Jin H L, et al. Effects of carbon nanotube content on morphology of SiCp(CNT) hybrid reinforcement and tensile mechanical properties of SiCp(CNT)/Al composites [J]. J. Mater. Res., 2017, 32: 1239
[20] Liu K, Cui Q F, Shi L, et al. Tuning lamella spacings for simultaneous strength-ductility improvements in heterogeneous lamella SiCp/2024Al composites [J]. Mater. Des., 2025, 249: 113510
[21] Cao L, Chen B, Jia Z D, et al. Research progress and aerospace applications of aluminum matrix composite [J]. Foundry Technol., 2023, 44: 685
  曹 遴, 陈 彪, 贾振东 等. 铝基复合材料研究进展及其航空航天应用 [J]. 铸造技术, 2023, 44: 685
[22] Li P Y. Research progress in high-performance aluminum matrix composites [J]. J. Mater. Eng, 2023, 51(4): 67
  李沛勇. 高性能铝基复合材料研究进展 [J]. 材料工程, 2023, 51(4): 67
[23] Ye X P, Li Y L, Weng J D, et al. Research status on strengthening mechanism of particle-reinforced metal matrix composites [J]. J. Mater. Eng., 2018, 46(12): 28
  叶想平, 李英雷, 翁继东 等. 颗粒增强金属基复合材料的强化机理研究现状 [J]. 材料工程, 2018, 46(12): 28
[24] Ma G N, Zhu S Z, Wang D, et al. Aging behaviors and mechanical properties of SiC/Al-Zn-Mg-Cu Composites [J]. Acta Metall. Sin., 2023, 59: 1655
  马国楠, 朱士泽, 王 东 等. SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能 [J]. 金属学报, 2023, 59: 1655
[25] Sun T T, Wang H Z, Wu Y, et al. Effect of in situ 2%TiB2 particles on microstructure and mechanical properties of 2024Al additive manufacturing alloy [J]. Acta Metall. Sin., 2023, 59: 169
  孙腾腾, 王洪泽, 吴 一 等. 原位自生2%TiB2颗粒对2024Al增材制造合金组织和力学性能的影响 [J]. 金属学报, 2023, 59: 169
[26] Nie J F, Wu Y L, Xie K W, et al. Microstructure and thermal stability of heterostructured Al-AlN nanocomposite [J]. Acta Metall. Sin., 2022, 58: 1497
  聂金凤, 伍玉立, 谢可伟 等. Al-AlN异构纳米复合材料的组织构型与热稳定性 [J]. 金属学报, 2022, 58: 1497
[27] Jiang Z H, Qiu W T, Gong S, et al. Preparation and properties of lightweight HfO2@CNT/polymer/CuAlMn composite with high strength and high damping [J]. Acta Metall. Sin., 2024, 60: 287
  蒋招汉, 邱文婷, 龚 深 等. 轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能 [J]. 金属学报, 2024, 60: 287
[28] Senthilraj K, Rajamurugan G. Influence of Al2TiO5 particles on AA6061 composites fabricated by bottom pouring stir casting technique [J]. Mater. Lett., 2023, 338: 134085
[29] Cui S, Shao G S, Zhang K, et al. Microstructure and mechanical properties of graphene reinforced Al-matrix composites prepared by stirring casting [J]. Nonferrous Met. Mater. Eng., 2022, 43(2): 19
  崔 松, 邵国森, 张 柯 等. 搅拌铸造法制备石墨烯增强铝基复合材料的组织和力学性能研究 [J]. 有色金属材料与工程, 2022, 43(2): 19
[30] Bai Y L, Zhang Z F, Fan J Z, et al. Preparation of particle reinforced aluminum matrix composites by semi-solid stirring [J]. Spec. Cast. Nonferrous Alloys, 2021, 41: 402
  白月龙, 张志峰, 樊建中 等. 半固态搅拌制备颗粒增强铝基复合材料 [J]. 特种铸造及有色合金, 2021, 41: 402
[31] El-Sabbagh A M, Soliman M, Taha M A, et al. Effect of rolling and heat treatment on tensile behaviour of wrought Al-SiCp composites prepared by stir-casting [J]. J. Mater. Process. Technol., 2013, 213: 1669
[32] Samal P, Vundavilli P R, Meher A, et al. Recent progress in aluminum metal matrix composites: A review on processing, mechanical and wear properties [J]. J. Manuf. Process., 2020, 59: 131
[33] Yang W S, Zhao Q Q, Xin L, et al. Microstructure and mechanical properties of graphene nanoplates reinforced pure Al matrix composites prepared by pressure infiltration method [J]. J. Alloys Compd., 2018, 732: 748
[34] Ma G J, Ding Y T, Jin P P, et al. Research on powder metallurgy processing for preparing Al matrix composites [J]. Mater. Rep., 2013, 27(15): 149
  马国俊, 丁雨田, 金培鹏 等. 粉末冶金法制备铝基复合材料的研究 [J]. 材料导报, 2013, 27(15): 149
[35] Liu R X, Wu C D, Zhang J, et al. Microstructure and mechanical behaviors of the ultrafine grained AA7075/B4C composites synthesized via one-step consolidation [J]. J. Alloys Compd., 2018, 748: 737
[36] Bi J, Lei Z L, Chen Y B, et al. Microstructure and mechanical properties of a novel Sc and Zr modified 7075 aluminum alloy prepared by selective laser melting [J]. Mater. Sci. Eng., 2019, A768: 138478
[37] Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys [J]. Nature, 2017, 549: 365
[38] Fan J L, Han Y, Li P F, et al. Micro/Nano composited tungsten material and its high thermal loading behavior [J]. J. Nucl. Mater., 2014, 455: 717
[39] Jiang L, Ma K K, Yang H, et al. The microstructural design of trimodal aluminum composites [J]. JOM, 2014, 66: 898
[40] Jiang L, Yang H, Yee J K, et al. Toughening of aluminum matrix nanocomposites via spatial arrays of boron carbide spherical nanoparticles [J]. Acta Mater., 2016, 103: 128
[41] Zhang Z M, Fan G L, Tan Z Q, et al. Bioinspired multiscale Al2O3-rGO/Al laminated composites with superior mechanical properties [J]. Composites, 2021, 217B: 108916
[42] Wang X, Jiang X S, Sun H L, et al. Microstructures and mechanical properties of Al nanocomposites hybrid-reinforced with B4C, carbon nanotubes and graphene nanoplatelets [J]. Mater. Sci. Eng., 2023, B293: 116457
[43] ?enel M C, Gürbüz M, Ko? E. Fabrication and characterization of synergistic Al-SiC-GNPs hybrid composites [J]. Composites, 2018, 154B: 1
[44] Wang X, Jiang X S, Sun H L, et al. Microstructure and mechanical properties of bioinspired laminated Al matrix hybrid reinforced with B4C and graphene nanoplatelets [J]. Mater. Charact., 2022, 193: 112307
[45] Herzallah H, Elsayd A, Shash A, et al. Effect of carbon nanotubes (CNTs) and silicon carbide (SiC) on mechanical properties of pure Al manufactured by powder metallurgy [J]. J. Mater. Res. Technol., 2020, 9: 1948
[46] Van Trinh P, Lee J, Kang B, et al. Mechanical and wear properties of SiCp/CNT/Al6061 hybrid metal matrix composites [J]. Diam. Relat. Mater., 2022, 124: 108952
[47] Guo B S, Zhang X M, Cen X, et al. Ameliorated mechanical and thermal properties of SiC reinforced Al matrix composites through hybridizing carbon nanotubes [J]. Mater. Charact., 2018, 136: 272
[48] Qiu F, Tong H T, Gao Y Y, et al. Microstructures and compressive properties of Al matrix composites reinforced with bimodal hybrid in-situ nano-/micro-sized TiC particles [J]. Materials, 2018, 11: 1284
[49] David Raja Selvam J, Dinaharan I, Vibin Philip S, et al. Microstructure and mechanical characterization of in situ synthesized AA6061/(TiB2 + Al2O3) hybrid aluminum matrix composites [J]. J. Alloys Compd., 2018, 740: 529
[50] Li S S. Prepare SiCp (in situ CNT) reinforced aluminum matrix composites and study on its properties [D]. Shanghai: Shanghai Jiao Tong University, 2017
  李士胜. 碳化硅颗粒原位自生碳纳米管增强铝基复合材料的制备与性能研究 [D]. 上海: 上海交通大学, 2017
[51] Liu Z Y, Xiao B L, Wang W G, et al. Modelling of carbon nanotube dispersion and strengthening mechanisms in Al matrix composites prepared by high energy ball milling-powder metallurgy method [J]. Composites, 2017, 94A: 189
[52] Cao L, Chen B, Wan J, et al. Unraveling the dispersion mechanism of carbon nanotubes in aluminum powder particles during high energy ball milling by FIB-TEM study [J]. Powder Technol., 2023, 419: 118339
[53] Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59
  肖伯律, 黄治冶, 马 凯 等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59
[54] Zhao N Q, Liu X H, Pu B W. Progress on multi-dimensional carbon nanomaterials reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin., 2019, 55: 1
  赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展 [J]. 金属学报, 2019, 55: 1
[55] Oh S I, Lim J Y, Kim Y C, et al. Fabrication of carbon nanofiber reinforced aluminum alloy nanocomposites by a liquid process [J]. J. Alloys Compd., 2012, 542: 111
[56] Ding H, Cui X P, Xu C S, et al. Fabrication and mechanical characteristics of multi-laminated aluminum matrix composites reinforced by continuous basalt fibers [J]. Acta Metall. Sin., 2018, 54: 1171
  丁 浩, 崔喜平, 许长寿 等. 连续玄武岩纤维增强铝基层状复合材料的制备与力学特性 [J]. 金属学报, 2018, 54: 1171
[57] Sharma A, Narsimhachary D, Sharma V M, et al. Surface modification of Al6061-SiC surface composite through impregnation of graphene, graphite & carbon nanotubes via FSP: A tribological study [J]. Surf. Coat. Technol., 2019, 368: 175
[58] Geng K, Li S F, Yang Y F, et al. 3D printing of Al matrix composites through in situ impregnation of carbon nanotubes on Al powder [J]. Carbon, 2020, 162: 465
[59] Zhu Z G, Hu Z H, Seet H L, et al. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: Microstructure, properties, and applications [J]. Int. J. Mach. Tools Manuf., 2023, 190: 104047
[60] Aikin R M, Christodoulou L. The role of equiaxed particles on the yield stress of composites [J]. Scr. Metall. Mater., 1991, 25: 9
[61] Le Roy G, Embury J D, Edwards G, et al. A model of ductile fracture based on the nucleation and growth of voids [J]. Acta Metall., 1981, 29: 1509
[62] Ryu H J, Cha S I, Hong S H. Generalized shear-lag model for load transfer in SiC/Al metal-matrix composites [J]. J. Mater. Res., 2003, 18: 2851
[63] Hansen N. Hall-Petch relation and boundary strengthening [J]. Scr. Mater., 2004, 51: 801
[64] Liu K, Cui Q F, Shi L, et al. Grain structure tailoring strategy for heterogeneous lamella SiCp/2024Al composites with exceptional strength-ductility synergy [J]. Composites, 2024, 280B: 111491
[65] Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties [J]. Mater. Res. Lett., 2017, 5: 527
[66] Han Q H, Asgari A, Hodgson P D, et al. Strain partitioning in dual-phase steels containing tempered martensite [J]. Mater. Sci. Eng., 2014, A611: 90
[67] Zhu Y T, Wu X L. Perspective on hetero-deformation induced (HDI) hardening and back stress [J]. Mater. Res. Lett., 2019, 7: 393
[68] Wang G, Ouyang H, Su Y S, et al. Heterostructured bulk aluminum with controllable gradient structure: Fabrication strategy and deformation mechanisms [J]. Scr. Mater., 2021, 196: 113762
文章导航

/