基于同步辐射原位表征技术的镁合金研究进展
收稿日期: 2025-09-28
修回日期: 2025-12-02
网络出版日期: 2026-03-30
基金资助
国家自然科学基金项目(52371005);国家自然科学基金项目(52531001);国家自然科学基金项目(52534009)
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
Received date: 2025-09-28
Revised date: 2025-12-02
Online published: 2026-03-30
Supported by
National Natural Science Foundation of China(52371005);National Natural Science Foundation of China(52531001);National Natural Science Foundation of China(52534009)
镁合金具有低密度、高比强度、生物相容性好等特点,被广泛应用于航空航天、交通运输和生物医疗等领域。阐明制备过程和服役过程中材料微观结构的动态演变规律,是材料成分设计与加工工艺优化,以及服役性能提升的重要基础。同步辐射光源可产生高通量、高分辨率及高相干性的X射线光束,能够实现合金在制备加工全流程及模拟服役环境中微观结构演化的原位动态表征。本文简要介绍了国内外基于同步辐射光源的原位样品环境装置建设现状,系统总结了近年来利用同步辐射先进表征技术研究镁合金微观组织演化机制的相关工作,内容涵盖凝固、变形与损伤、腐蚀与防护等。最后对同步辐射技术在镁合金研究领域的未来发展方向进行了展望。
郭恩宇 , 杜泽龙 , 李炳志 , 王同敏 . 基于同步辐射原位表征技术的镁合金研究进展[J]. 金属学报, 2026 , 62(5) : 890 -904 . DOI: 10.11900/0412.1961.2025.00297
Magnesium alloys are widely employed in lightweight applications such as aerospace, transportation, and biomedical devices due to their low density, high specific strength, and good biocompatibility. Elucidating the dynamic evolution of microstructures during preparation and service is essential for alloy compositional design, processing optimization, and performance enhancement. Synchrotron radiation sources, which generate X-ray beams with high flux, high resolution, and high coherence, enable in situ dynamic characterization of microstructural evolution in magnesium alloys throughout the entire processing chain and under simulated service conditions. This paper briefly overviews the development of in situ sample environment devices at synchrotron facilities worldwide. It also systematically outlines recent research on the microstructural evolution mechanisms of magnesium alloys investigated using this advanced technology, covering solidification, deformation and damage, as well as corrosion and protection. Finally, future directions for the application of synchrotron radiation technology in magnesium alloy research are discussed.
| [1] | Zhu Q C, Li Y X, Cao F Y, et al. Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film [J]. Nat. Commun., 2022, 13: 5838 |
| [2] | Yu M D, Li Y F, Guo H, et al. Anomalous strain hardening via manipulating basal/pyramidal dislocation interactions in the Mg-Y-Ca alloy [J]. Acta Mater., 2025, 296: 121309 |
| [3] | Guru M K, Bohlen J, Aydin R C, et al. Machine learning pipeline for structure-property modeling in Mg-alloys using microstructure and texture descriptors [J]. Acta Mater., 2025, 295: 121132 |
| [4] | Ma C, Yu W, Zhang Z, et al. The effect of slow shot speed and casting pressure on the 3D microstructure of high pressure die casting AE44 magnesium alloy [J]. J. Magnes. Alloy., 2023, 11: 753 |
| [5] | Paliwal M, Jung I H. The evolution of the growth morphology in Mg-Al alloys depending on the cooling rate during solidification [J]. Acta Mater., 2013, 61: 4848 |
| [6] | Ni R, Boehlert C J, Chen B, et al. Temperature-dependent interplay of intra- and inter-granular deformation mechanisms in Mg-10Y: Statistical analysis from an HRDIC perspective [J]. Acta Mater., 2025, 296: 121256 |
| [7] | Jeong J, Alfreider M, Konetschnik R, et al. In-situ TEM observation of 10 1 ˉ 2 twin-dominated deformation of Mg pillars: Twinning mechanism, size effects and rate dependency [J]. Acta Mater., 2018, 158: 407 |
| [8] | Fan X Q, Fleming T G, Clark S J, et al. Magnetic modulation of keyhole instability during laser welding and additive manufacturing [J]. Science, 2025, 387: 864 |
| [9] | Ajayi T M, Shirato N, Rojas T, et al. Characterization of just one atom using synchrotron X-rays [J]. Nature, 2023, 618: 69 |
| [10] | Guo E Y, Du Z L, Chen X B, et al. Development of magnesium alloys: Advanced characterization using synchrotron radiation techniques [J]. J. Mater. Sci. Technol., 2024, 195: 93 |
| [11] | Mathiesen R H, Arnberg L, Mo F, et al. Time resolved X-ray imaging of dendritic growth in binary alloys [J]. Phys. Rev. Lett., 1999, 83: 5062 |
| [12] | Abou-Khalil L, Da Cruz K S, Reinhart G, et al. Influence of growth velocity on fragmentation during directional solidification of Al-14 wt.% Sn alloy studied by in-situ synchrotron X-radiography [J]. Acta Mater., 2022, 241: 118370 |
| [13] | Azeem M A, Lee P D, Phillion A B, et al. Revealing dendritic pattern formation in Ni, Fe and Co alloys using synchrotron tomography [J]. Acta Mater., 2017, 128: 241 |
| [14] | Buffiere J Y, Maire E, Adrien J, et al. In situ experiments with X ray tomography: An attractive tool for experimental mechanics [J]. Exp. Mech., 2010, 50: 289 |
| [15] | Bale H A, Haboub A, MacDowell A A, et al. Real-time quantitative imaging of failure events in materials under load at temperatures above 1, 600? oC [J]. Nat. Mater., 2013, 12: 40 |
| [16] | Zhang K, Wigger T, Pineda R, et al. Unravelling dynamic recrystallisation in a microalloyed steel during rapid high temperature deformation using synchrotron X-rays [J]. Acta Mater., 2024, 278: 120265 |
| [17] | Wang T M, Cao F, Zhou P, et al. Study on diffusion behavior and microstructural evolution of Al/Cu bimetal interface by synchrotron X-ray radiography [J]. J. Alloys Compd., 2014, 616: 550 |
| [18] | Wang T M, Xu J J, Xiao T Q, et al. Evolution of dendrite morphology of a binary alloy under an applied electric current: An in situ observation [J]. Phys. Rev., 2010, 81E: 042601 |
| [19] | Zhang W, Simpson C A, Leitner T, et al. The effect of anisotropic microstructure on the crack growth and fatigue overload behaviour of ultrafine-grained nickel [J]. Acta Mater., 2020, 184: 225 |
| [20] | Wu Z K, Wu S C, Kruzic J J, et al. Critical damage events of 3D printed AlSi10Mg alloy via in situ synchrotron X-ray tomography [J]. Acta Mater., 2025, 282: 120464 |
| [21] | Lin Y, Qian W J, Lei L M, et al. Structural integrity issues of composite materials and structures in future transportation equipment [J]. Compos. Struct., 2025, 358: 118943 |
| [22] | Casari D, Mirihanage W U, Falch K V, et al. α-Mg primary phase formation and dendritic morphology transition in solidification of a Mg-Nd-Gd-Zn-Zr casting alloy [J]. Acta Mater., 2016, 116: 177 |
| [23] | Du J, Zhang A, Guo Z, et al. Effect of additional solute elements (X = Al, Ca, Y, Ba, Sn, Gd and Zn) oncrystallographic anisotropy during the dendritic growth of magnesium alloys [J]. J. Alloys Compd., 2019, 775: 322 |
| [24] | Tang Y, Wu Y, Zhang Y, et al. Intermittent nucleation and periodic growth of grains under thermo-solutal convection during directional solidification of Al-Cu alloy [J]. Acta Mater., 2021, 212: 116861 |
| [25] | Wang M Y, Jing T, Liu B C. Phase-field simulations of dendrite morphologies and selected evolution of primary α-Mg phases during the solidification of Mg-rich Mg-Al-based alloys [J]. Scr. Mater., 2009, 61: 777 |
| [26] | Yang M, Xiong S M, Guo Z. Characterisation of the 3-D dendrite morphology of magnesium alloys using synchrotron X-ray tomography and 3-D phase-field modelling [J]. Acta Mater., 2015, 92: 8 |
| [27] | Yang M, Xiong S M, Guo Z. Effect of different solute additions on dendrite morphology and orientation selection in cast binary magnesium alloys [J]. Acta Mater., 2016, 112: 261 |
| [28] | Shuai S S, Guo E Y, Wang J, et al. Synchrotron tomographic quantification of the influence of Zn concentration on dendritic growth in Mg-Zn alloys [J]. Acta Mater., 2018, 156: 287 |
| [29] | Shuai S S, Guo E Y, Phillion A B, et al. Fast synchrotron X-ray tomographic quantification of dendrite evolution during the solidification of Mg Sn alloys [J]. Acta Mater., 2016, 118: 260 |
| [30] | Guo E Y, Phillion A B, Cai B, et al. Dendritic evolution during coarsening of Mg-Zn alloys via 4D synchrotron tomography [J]. Acta Mater., 2017, 123: 373 |
| [31] | Aagesen L K, Johnson A E, Fife J L, et al. Universality and self-similarity in pinch-off of rods by bulk diffusion [J]. Nat. Phys., 2010, 6: 796 |
| [32] | Gu L D, Shang X Q, Wang J, et al. The influence of SiC-Al2O3 reinforcements on the deformation and fracture mechanism of thixomolded Mg-based composite [J]. J. Mater. Sci., 2024, 59: 9892 |
| [33] | Huang S J, Subramani M, Ali A N, et al. The effect of micro-SiCp content on the tensile and fatigue behavior of AZ61 magnesium alloy matrix composites [J]. Int. J. Metalcast., 2021, 15: 780 |
| [34] | Wang P B, Shen J, Chen T J, et al. Simultaneously improving the strength and ductility of AZ91/GNPs composites through decorating graphene nanoplatelets with MgO [J]. J. Mater. Sci. Technol., 2024, 183: 133 |
| [35] | Pu Z P, Wang S F, Yan Q, et al. Grain refinement mechanism of SiC nanoparticles/Mg-9 wt.% Al composite investigated by sharp interface model at microscale and nanoscale [J]. J. Alloys Compd., 2022, 922: 166269 |
| [36] | Guo E Y, Shuai S S, Kazantsev D, et al. The influence of nanoparticles on dendritic grain growth in Mg alloys [J]. Acta Mater., 2018, 152: 127 |
| [37] | Du Z L, Wang C, Liu F Y, et al. Unraveling the individual and synergistic effects of copper and gadolinium on the microstructure and mechanical properties of Mg-6Zn-0.5Ca alloy [J]. J. Alloys Compd., 2025, 1036: 181421 |
| [38] | Du Z L, Yang X Q, Wang Q, et al. A synergetic approach to enhancing mechanical properties of trace TiB2 particles reinforced AZ91D composites through α-Mg grain refinement and β-Mg17Al12 manipulation [J]. Composites, 2025, 198: 109114 |
| [39] | Yang X Q, Du Z L, Guo E Y, et al. Achieving simultaneous refinement of α-Mg grains and β-Mg17Al12 phases via trace multi-scale TiB2 for strength-ductility synergy in AZ91D composites [J]. J. Alloys Compd., 2025, 1048: 185116 |
| [40] | Wu H Z, Du Z L, An Y K, et al. Grain refinement and mechanical property enhancement of AM60B magnesium alloy via TiB2 particle regulation [J]. Mater. Today Commun., 2025, 47: 112999 |
| [41] | Ma C S, Yu W B, Zhang T T, et al. The effect of slow shot speed and casting pressure on the 3D microstructure of high pressure die casting AE44 magnesium alloy [J]. J. Magnes. Alloy., 2023, 11: 753 |
| [42] | Walmsley I A. Quantum optics: Science and technology in a new light [J]. Science, 2015, 348: 525 |
| [43] | Trang T T T, Zhang J H, Kim J H, et al. Designing a magnesium alloy with high strength and high formability [J]. Nat. Commun., 2018, 9: 2522 |
| [44] | Offerman S E, van Dijk N H, Sietsma J, et al. Grain nucleation and growth during phase transformations [J]. Science, 2002, 298: 1003 |
| [45] | Zhou X L, Feng Z Q, Zhu L L, et al. High-pressure strengthening in ultrafine-grained metals [J]. Nature, 2020, 579: 67 |
| [46] | Zhang D S, Liu W, Li Y X, et al. In situ observation of crystal rotation in Ni-based superalloy during additive manufacturing process [J]. Nat. Commun., 2023, 14: 2961 |
| [47] | Schmidt S, Nielsen S F, Gundlach C, et al. Watching the growth of bulk grains during recrystallization of deformed metals [J]. Science, 2004, 305: 229 |
| [48] | Oddershede J, Camin B, Schmidt S, et al. Measuring the stress field around an evolving crack in tensile deformed Mg AZ31 using three-dimensional X-ray diffraction [J]. Acta Mater., 2012, 60: 3570 |
| [49] | Huang Z H, Wang L Y, Zhou B J, et al. Observation of non-basal slip in Mg-Y by in situ three-dimensional X-ray diffraction [J]. Scr. Mater., 2018, 143: 44 |
| [50] | Zhang N B, Zhang Y Y, Chen S, et al. Onset of detwinning in Mg-3Al-1Zn alloy: A synchrotron-based X-ray diffraction study [J]. Scr. Mater., 2021, 190: 113 |
| [51] | Yi S B, Davies C H J, Brokmeier H G, et al. Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loading [J]. Acta Mater., 2006, 54: 549 |
| [52] | Wang W Y, Tang B, Shang S L, et al. Local lattice distortion mediated formation of stacking faults in Mg alloys [J]. Acta Mater., 2019, 170: 231 |
| [53] | Garces G, Morris D G, Mu?oz-Morris M A, et al. Plasticity analysis by synchrotron radiation in a Mg97Y2Zn1 alloy with bimodal grain structure and containing LPSO phase [J]. Acta Mater., 2015, 94: 78 |
| [54] | Garces G, Medina J, Perez P, et al. The effect of temperature on load partitioning evolution in magnesium metal matrix composite reinforced with Ti particles using in-situ synchrotron radiation diffraction experiments [J]. J. Magnes. Alloy., 2023, 11: 706 |
| [55] | Arul Kumar M, Clausen B, Capolungo L, et al. Deformation twinning and grain partitioning in a hexagonal close-packed magnesium alloy [J]. Nat. Commun., 2018, 9: 4761 |
| [56] | Bong H J, Hu X H, Sun X, et al. Mechanism-based constitutive modeling of ZEK100 magnesium alloy with crystal plasticity and in-situ HEXRD experiment [J]. Int. J. Plast., 2019, 113: 35 |
| [57] | Zhang H J, Jérusalem A, Salvati E, et al. Multi-scale mechanisms of twinning-detwinning in magnesium alloy AZ31B simulated by crystal plasticity modeling and validated via in situ synchrotron XRD and in situ SEM-EBSD [J]. Int. J. Plast., 2019, 119: 43 |
| [58] | Wang H, Clausen B, Tomé C N, et al. Studying the effect of stress relaxation and creep on lattice strain evolution of stainless steel under tension [J]. Acta Mater., 2013, 61: 1179 |
| [59] | Hu X H, Sun X, Hector L G, et al. Individual phase constitutive properties of a TRIP-assisted QP980 steel from a combined synchrotron X-ray diffraction and crystal plasticity approach [J]. Acta Mater., 2017, 132: 230 |
| [60] | Jia N, Cong Z H, Sun X, et al. An in situ high-energy X-ray diffraction study of micromechanical behavior of multiple phases in advanced high-strength steels [J]. Acta Mater., 2009, 57: 3965 |
| [61] | Abdolvand H, Daymond M R, Mareau C. Incorporation of twinning into a crystal plasticity finite element model: Evolution of lattice strains and texture in Zircaloy-2 [J]. Int. J. Plast., 2011, 27: 1721 |
| [62] | Agnew S R, Singh A, Calhoun C A, et al. In-situ neutron diffraction of a quasicrystal-containing Mg alloy interpreted using a new polycrystal plasticity model of hardening due to {10.2} tensile twinning [J]. Int. J. Plast., 2018, 100: 34 |
| [63] | Agnew S R, Mulay R P, Polesak F J, et al. In situ neutron diffraction and polycrystal plasticity modeling of a Mg-Y-Nd-Zr alloy: Effects of precipitation on individual deformation mechanisms [J]. Acta Mater., 2013, 61: 3769 |
| [64] | Neil C J, Wollmershauser J A, Clausen B, et al. Modeling lattice strain evolution at finite strains and experimental verification for copper and stainless steel using in situ neutron diffraction [J]. Int. J. Plast., 2010, 26: 1772 |
| [65] | Wang H M, Wu P D, Kurukuri S, et al. Strain rate sensitivities of deformation mechanisms in magnesium alloys [J]. Int. J. Plast., 2018, 107: 207 |
| [66] | Lee S, Pilipchuk M, Yildirim C, et al. Three-dimensional nucleation and growth of deformation twins in magnesium [J]. Science, 2025, 389: 632 |
| [67] | Wang C, Du Z L, Guo E Y, et al. Mechanical behavior of SiC reinforced ZA63 Mg matrix composites: Experiments and 3D finite element modelling [J]. J. Magnes. Alloy., 2025, 13: 1294 |
| [68] | Hu Y N, Wu S C, Guo Y, et al. Inhibiting weld cracking in high-strength aluminium alloys [J]. Nat. Commun., 2022, 13: 5816 |
| [69] | An Y K, Guo E Y, Xia D Y, et al. A new strategy for fabricating Mg-Al alloys with excellent strength-ductility synergy via pulse-coupled wire-arc directed energy deposition [J]. Int. J. Plast., 2026, 196: 104550 |
| [70] | Kondori B, Morgeneyer T F, Helfen L, et al. Void growth and coalescence in a magnesium alloy studied by synchrotron radiation laminography [J]. Acta Mater., 2018, 155: 80 |
| [71] | Wang Z Y, Wu S C, Kang G Z, et al. In-situ synchrotron X-ray tomography investigation of damage mechanism of an extruded magnesium alloy in uniaxial low-cycle fatigue with ratchetting [J]. Acta Mater., 2021, 211: 116881 |
| [72] | Karagadde S, Lee P D, Cai B, et al. Transgranular liquation cracking of grains in the semi-solid state [J]. Nat. Commun., 2015, 6: 8300 |
| [73] | Azghandi S H M, Weiss M, Arhatari B D, et al. A rationale for the influence of grain size on failure of magnesium alloy AZ31: An in situ X-ray microtomography study [J]. Acta Mater., 2020, 200: 619 |
| [74] | Kumar R, Lhuissier P, Villanova J, et al. Elementary growth mechanisms of creep cavities in AZ31 alloy revealed by in situ X-ray nano-tomography [J]. Acta Mater., 2022, 228: 117760 |
| [75] | Zeller-Plumhoff B, Robisch A L, Pelliccia D, et al. Nanotomographic evaluation of precipitate structure evolution in a Mg-Zn-Zr alloy during plastic deformation [J]. Sci. Rep., 2020, 10: 16101 |
| [76] | Pollock T M. Weight loss with magnesium alloys [J]. Science, 2010, 328: 986 |
| [77] | Yang G F, Kim Y C, Han H S, et al. In vitro dynamic degradation behavior of new magnesium alloy for orthopedic applications [J]. J. Biomed. Mater. Res., 2015, 103B: 807 |
| [78] | Esmaily M, Svensson J E, Fajardo S, et al. Fundamentals and advances in magnesium alloy corrosion [J]. Prog. Mater. Sci., 2017, 89: 92 |
| [79] | Ro?ňáková I, Montufar E B, Horynová M, et al. Assessment of localized corrosion under simulated physiological conditions of magnesium samples with heterogeneous microstructure: Value of X-ray computed micro-tomography platform [J]. Corros. Sci., 2016, 104: 187 |
| [80] | Zhang C, Liu C, Li X, et al. Quantifying the influence of secondary phases on corrosion in multicomponent Mg alloys using X-ray computed microtomography [J]. Corros. Sci., 2022, 195: 110010 |
| [81] | Tian G Y, Wang J S, Zhang C, et al. Quantifying the influence of microstructure on the corrosion of Mg-Li alloys by using X-ray CT [J]. Corros. Sci., 2024, 229: 111848 |
| [82] | Wang X J, Chen Z N, Guo E Y, et al. Corrosion process of Mg-Sn alloys revealed via in situ synchrotron X-ray radiography [J]. Mater. Lett., 2022, 308: 131139 |
| [83] | Liu X Q, Wang X J, Guo E Y, et al. Influence of deformation on the corrosion behavior of LZ91 Mg-Li alloy [J]. Int. J. Miner. Metall. Mater., 2023, 30: 72 |
| [84] | Chen Z N, Ji H T, Geng X Q, et al. 3-D distribution characteristics of the micro-defects in the PEO coating on ZM6 Mg-alloy during corrosion [J]. Corros. Sci., 2020, 174: 108821 |
| [85] | Li B Z, Ouyang Y B, Guo E Y, et al. Mao-based solid-like slippery composite coating with superior corrosion resistance and robust machinery performance upon magnesium-lithium alloy LA81 [J]. Chem. Eng. J., 2024, 497: 154801 |
| [86] | Fischerauer S F, Kraus T, Wu X, et al. In vivo degradation performance of micro-arc-oxidized magnesium implants: A micro-CT study in rats [J]. Acta Biomater., 2013, 9: 5411 |
| [87] | Hou X R, Li B Z, Zhou Z H, et al. Superhydrophobic and corrosion-resistant coating on magnesium-lithium alloys [J]. J. Taiwan Inst. Chem. Eng., 2025, 176: 106319 |
| [88] | Ouyang Y B, Zhou Z H, Guo E Y, et al. Boosting corrosion resistance of Mg-Li alloy: Implanting bioinspired superhydrophobic surfaces into MAO matrix for enhanced protection [J]. Ceram. Int., 2024, 50: 48425 |
| [89] | Li B Z, Liu B C, Guo E Y, et al. MAO-based self-healing phase-change solid-like slippery composite coating with superior corrosion resistance and robust machinery performance [J]. J. Mater. Sci. Technol., 2026, 253: 298 |
/
| 〈 |
|
〉 |