研究论文

直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制

  • 王明飞 ,
  • 陶美悦 ,
  • 宫臣 ,
  • 彭博 ,
  • 李廷举 ,
  • 接金川
展开
  • 1 大连理工大学 材料科学与工程学院 大连 116024
    2 大连理工大学 宁波研究院 宁波 315000
王明飞,男,1995年生,博士生
接金川,jiejc@dlut.edu.cn,主要从事物理场作用下铜合金凝固组织控制及高品质金属基复合材料制备研究

收稿日期: 2025-11-14

  修回日期: 2026-03-01

  网络出版日期: 2026-03-18

基金资助

国家自然科学基金项目(U23A20611);国家自然科学基金项目(52071050);宁波市科技创新项目(2024Z077);宁波市科技创新项目(2023Z100);中国博士后科学基金项目(2024M750312);中国博士后科学基金项目(GZB20240091);辽宁省博士后科研基金项目(2025-BS-0043)

Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing

  • WANG Mingfei ,
  • TAO Meiyue ,
  • GONG Chen ,
  • PENG Bo ,
  • LI Tingju ,
  • JIE Jinchuan
Expand
  • 1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
    2 Ningbo Research Institute of Dalian University of Technology, Ningbo 315000, China
JIE Jinchuan, professor, Tel: 15941130325, E-mail: jiejc@dlut.edu.cn

Received date: 2025-11-14

  Revised date: 2026-03-01

  Online published: 2026-03-18

Supported by

National Natural Science Foundation of China(U23A20611);National Natural Science Foundation of China(52071050);Science and Technology Innovation Project of Ningbo(2024Z077);Science and Technology Innovation Project of Ningbo(2023Z100);China Postdoctoral Science Foundation(2024M750312);China Postdoctoral Science Foundation(GZB20240091);Liaoning Province Doctoral Research Start-up Fund Program Project(2025-BS-0043)

摘要

针对铸态Cu-Ni-Si/1010钢双金属复合材料微观组织粗大及力学性能不足的问题,本工作旨在通过后处理工艺实现其组织调控和性能优化。本工作对比研究了直接退火与冷轧+退火复合工艺对铸态Cu-Ni-Si/1010钢双金属复合材料显微组织和力学行为的影响。结果表明,铸态Cu-Ni-Si合金微观组织呈现粗大柱状晶和少量β-Ni3Si相,直接退火诱导α-Cu基体析出纳米级δ-Ni2Si强化相;冷轧+退火工艺通过引入高密度位错并抑制部分晶粒再结晶,使组织呈现细化的纤维状特征。力学测试结果表明,冷轧+退火样品的抗拉强度由铸态的379 MPa显著提高至613 MPa,这归因于析出强化、加工硬化及异质变形诱导强化的协同效应。此外,得益于1010钢的回复作用,冷轧+退火样品在保持高强度的同时,延伸率仍达18.4%。

本文引用格式

王明飞 , 陶美悦 , 宫臣 , 彭博 , 李廷举 , 接金川 . 直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制[J]. 金属学报, 2026 , 62(6) : 1091 -1104 . DOI: 10.11900/0412.1961.2025.00368

Abstract

High-performance materials are in strong demand in the electronics and automotive industries. Cu-Ni-Si alloys are widely used owing to their excellent combination of strength and electrical conductivity, whereas 1010 steel provides superior formability, high elastic modulus, and cost-effectiveness. Integrating these materials into laminated bimetallic composites represents a promising strategy for achieving structural-functional integration, thereby overcoming the trade-offs inherent in single-component metals. However, fabrication of such composites remains challenging, primarily due to poor wettability and limited mutual solubility between Cu and Fe, which often result in weak interfacial bonding and coarse as-cast microstructures. Therefore, the development of effective fabrication methods and appropriate post-processing routes to tailor microstructure and optimize mechanical properties is essential for industrial application. In this study, Cu-Ni-Si/1010 steel laminated bimetallic composite was successfully fabricated via continuous solid-liquid bonding method. To investigate the effects of annealing and cold rolling followed by annealing on microstructural evolution and mechanical behavior, the composites were subjected to four conditions: as-cast (sample S1), direct annealing at 450 °C (sample S2), 70% cold rolling followed by annealing at 450 °C (sample S3), and 70% cold rolling (sample S4). Microstructural and mechanical characterization was performed using OM, SEM, TEM, and tensile testing to elucidate the relationships among processing parameters, interfacial characteristics, and strengthening mechanisms. The Cu-Ni-Si layer in sample S1 exhibits coarse columnar grains, with a minor β-Ni3Si phase located at α-Cu grain boundaries. Direct annealing promotes the formation of nanoscale δ-Ni2Si precipitates within the α-Cu matrix, contributing to strengthening. In contrast, the combined cold rolling and annealing treatment induces more pronounced microstructural evolution: severe plastic deformation increases dislocation density and refines the grain structure into the fibrous morphology due to incomplete recrystallization. No brittle intermetallic compounds are observed at the interface under any condition. Samples S3 and S4 exhibit wavy, well-bonded interfaces, indicating enhanced interfacial diffusion and metallurgical bonding. Tensile testing shows that sample S3 achieves the highest ultimate tensile strength (613 MPa), significantly exceeding those of sample S1 (379 MPa) and sample S2 (415 MPa), which is attributed to the synergistic effects of work hardening, precipitation strengthening, and hetero-deformation induced strengthening. Although ductility decreases slightly in sample S3, the elongation remains relatively high at 18.4%, whereas sample S4 exhibits the lowest elongation (12.6%), which is detrimental to subsequent forming. Importantly, all samples fracture within the matrix without interfacial delamination, confirming robust metallurgical bonding. These results indicate that direct annealing enhances both strength and ductility in Cu-Ni-Si/1010 steel laminated bimetallic composites, while cold rolling followed by annealing is an effective strategy for substantially increasing strength while preserving interfacial integrity.

参考文献

[1] Wang C S, Fu H D, Zhang H T, et al. Effect of cold-rolling deformation on microstructure, properties, and precipitation behavior of high-performance Cu-Ni-Si alloys[J]. Acta Metall. Sin., 2023, 59: 585
  王长胜, 付华栋, 张洪涛 等. 冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响[J]. 金属学报, 2023, 59: 585
[2] Yi J, Jia Y L, Zhao Y Y, et al. Precipitation behavior of Cu-3.0Ni-0.72Si alloy[J]. Acta Mater., 2019, 166: 261
[3] Mohammad-Nejad D, Jamshidi Aval H, Jamaati R. Development of gradient microstructures in AISI 1010 steel using integrated surface thermomechanical treatment and cold rolling[J]. Results Mater., 2025, 28: 100794
[4] Li S, Luo H, Hao P F, et al. Innovative data-driven design of titanium bimetal with superior strength-ductility synergy[J]. J. Alloys Compd., 2025, 1039: 183004
[5] Wang Y Y, Lu Y Y, Zhao Y, et al. Laser directed energy deposition of Ti6Al4V/M50 steel bimetals: Comparative study of Nb/Cu and Nb/Cu/Ni interlayers[J]. Mater. Des., 2025, 257: 114383
[6] Wang M F, Peng B, Sun J, et al. Simultaneously enhancing mechanical and bonding property of Cu-Ni-Si/1010 steel bimetal laminated composites via annealing[J]. Mater. Charact., 2025, 223: 114908
[7] Wang M F, Sun J, Peng B, et al. Interfacial bonding mechanism and mechanical properties of Cu-Ni-Si/1010 steel bimetallic laminated composites prepared by continuous solid/liquid bonding[J]. Mater. Today Commun., 2024, 40: 109803
[8] Dong B W, Jie J C, Wang S H, et al. Fabrication of Cu-24Pb-2Sn/C10 laminar composite by solid-liquid continuous casting compositing[J]. Mater. Lett., 2020, 262: 127174
[9] Zhang D K, Xiu S H, Wang K H, et al. Liquid-solid composite bonding of femtosecond laser surface modified SiC ceramics and 7A52 aluminum alloy[J]. Mater. Charact., 2024, 217: 114327
[10] He J, Zhao J Z. Microstructures of rapidly solidified Cu-Fe immiscible alloy[J]. Acta Metall. Sin., 2005, 41: 407
  何 杰, 赵九洲. 快速凝固Cu-Fe难混溶合金的显微组织[J]. 金属学报, 2005, 41: 407
[11] Fu Y X, Liu J X, Huang W Q, et al. Formation mechanisms of defects in additively manufactured GH4169/cast iron bimetal via a multiphysics coupling model[J]. J. Manuf. Process., 2025, 152: 805
[12] Peng B, Liu S C, Jie J C, et al. Direct elimination of Fe-oxides assists the preparation of Cu/1010 steel bimetal laminated composites with oxides-free interface[J]. Mater. Charact., 2025, 228: 115386
[13] Gu L M, Zhang J F, Liu Y, et al. Macroscopic and microscopic residual stress relief in SiC/Al composites: Effects of annealing and cryogenic treatment[J]. J. Mater. Sci. Technol., 2026, 254: 106
[14] Zheng J B, Shu X D, Xu Y C, et al. The coordinated evolution behavior of interface microstructure regulation and bonding strength of hot-spinning Mg/Al composite tubes under annealing[J]. J. Magnes. Alloy., 2026, 16: 101891
[15] Zhang R, Zhu S Z, Liu Z Y, et al. Influence of aging temperatures on precipitation behaviors of SiC/Al-Zn-Mg-Cu composites[J]. Acta Metall. Sin., 2024, 60: 1043
  张 冉, 朱士泽, 刘振宇 等. 时效温度对SiC/Al-Zn-Mg-Cu复合材料时效析出行为的影响[J]. 金属学报, 2024, 60: 1043
[16] An X L, Li Y, Ni S, et al. Grain refinement process in a cold-rolled polycrystalline cobalt[J]. Mater. Charact., 2020, 164: 110360
[17] Niu H, Wang T, Ji C, et al. Enhanced interfacial bonding strength via multi-scale microstructure formation in 304SS/TA2 composite tubes fabricated by three-roll skew rolling[J]. J. Mater. Sci. Technol., 2026, 249: 275
[18] Xiang H L, Hua L L, Li Z X, et al. High interfacial bonding strength aluminum alloy bimetallic composite plate fabricated by additive manufacturing and rolling hybrid process[J]. J. Alloys Compd., 2025, 1041: 183778
[19] Yu G A, Zhang H M, Yu Z X, et al. Effect of annealing temperature on interface diffusion behavior of ultra-thin Cu/Al composite sheet by secondary micro-rolling[J]. Mater. Lett., 2024, 377: 137308
[20] Wei Z X, Huang P, Su X X, et al. Effect of bell annealing on the interface microstructure and mechanical properties of titanium/steel composite plates prepared by hot rolling[J]. Mater. Sci. Eng., 2025, A919: 147485
[21] Li X H, Yan H, Chen R S. Microstructure, texture and mechanical properties of Y2O3p/ZG21 composites after rolling and subsequent annealing[J]. J. Alloys Compd., 2021, 889: 161683
[22] Xu J J, Fu J Y, Li S J, et al. Effect of annealing and cold rolling on interface microstructure and properties of Ti/Al/Cu clad sheet fabricated by horizontal twin-roll casting[J]. J. Mater. Res. Technol., 2022, 16: 530
[23] Xu H Q, Zhang W J, Qi X N, et al. Achieving high-strength joining with superior metallurgical bonding in tungsten/steel via in-situ element-selective directional diffusion[J]. J. Mater. Process. Technol., 2025, 345: 119064
[24] Wang W, Chen Z N, Guo E Y, et al. Influence of cryorolling on the precipitation of Cu-Ni-Si alloys: An in situ X-ray diffraction study[J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 1089
[25] Hu T, Chen J H, Liu J Z, et al. The crystallographic and morphological evolution of the strengthening precipitates in Cu-Ni-Si alloys[J]. Acta Mater., 2013, 61: 1210
[26] Liu S S, Huang G S, Gupta M, et al. Microstructures, mechanical properties and deformation mechanism of heterogeneous metal materials: A review[J]. J. Mater. Sci. Technol., 2026, 248: 1
[27] Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy[J]. Acta Mater., 2014, 62: 141
[28] Wen H M, Topping T D, Isheim D, et al. Strengthening mechanisms in a high-strength bulk nanostructured Cu-Zn-Al alloy processed via cryomilling and spark plasma sintering[J]. Acta Mater., 2013, 61: 2769
[29] Baheti V A, Kashyap S, Kumar P, et al. Effect of Ni on growth kinetics, microstructural evolution and crystal structure in the Cu(Ni)-Sn system[J]. Philos. Mag., 2017, 97: 1782
[30] Fang X T, Li Z K, Wang Y F, et al. Achieving high hetero-deformation induced (HDI) strengthening and hardening in brass by dual heterostructures[J]. J. Mater. Sci. Technol., 2022, 98: 244
[31] Lei Q, Li Z, Gao Y, et al. Microstructure and mechanical properties of a high strength Cu-Ni-Si alloy treated by combined aging processes[J]. J. Alloys Compd., 2017, 695: 2413
[32] Wen Y, Guan B, Xin Y C, et al. Solute atom mediated Hall-Petch relations for magnesium binary alloys[J]. Scr. Mater., 2022, 210: 114451
[33] Lu X C, Ran H, Fan J C, et al. Cryogenic amplification of the HDI effect enhances strength-ductility synergy in layered heterostructures[J]. Scr. Mater., 2026, 271: 116990
[34] Li Z K, Fang X T, Wang Y F, et al. Tuning heterostructures with powder metallurgy for high synergistic strengthening and hetero-deformation induced hardening[J]. Mater. Sci. Eng., 2020, A777: 139074
文章导航

/