金属凝固作为先进制造的关键基础过程,对工件微观组织和服役性能具有决定性影响。定向凝固是高温合金单晶构件制备的重要技术,但精确控制凝固组织仍面临诸多难点。为系统梳理定向凝固枝晶生长模拟的研究现状和发展趋势,揭示多尺度模拟在预测枝晶形貌、枝晶竞争及缺陷形成中的关键作用,本文以枝晶生长为切入点,系统归纳了凝固成分过冷理论、枝晶生长模型和典型定向凝固工艺,重点综述了有限元、有限差分、元胞自动机和相场法等多尺度模拟方法,并论述了这些方法从宏观物理场模拟到微观枝晶生长建模中的适用性及其代表性成果。最后,本文归纳了定向凝固枝晶生长数值模拟当前面临的挑战,并展望了未来的发展方向。
董洪标 , 郝文硕 . 综述:定向凝固枝晶生长的数值模拟[J]. 金属学报, 2026 , 62(5) : 756 -769 . DOI: 10.11900/0412.1961.2025.00301
Solidification is a fundamental process in advanced manufacturing, playing a pivotal role in determining the microstructure and performance of components. Directional solidification is a critical technique for producing single-crystal superalloy components; however, precise control of dendritic structure remains challenging. This article aims to systematically review the current status and future trends of dendrite growth simulations in directional solidification. In addition, it seeks to elucidate the key role of multiscale modeling in predicting dendritic morphology, dendrite competition, and defect formation. This article focuses on dendritic growth and summarizes the constitutional undercooling theory, dendrite growth models, and typical directional solidification processes. Multiscale numerical simulation methods, including finite element, finite difference, cellular automaton, and phase-field approaches, are emphasized, with an analysis of their applicability and a discussion of their representative achievements from macroscopic physical-field simulation to microscopic dendrite growth modeling. Finally, the key challenges are outlined, and prospective advancements in the numerical simulation of dendrite growth in directional solidification are delineated.
| [1] | Zhou Y H, Hu Z Q, Jie W Q. Solidification technology [M]. Beijing: China Machine Press, 1998: 1 |
| 周尧和, 胡壮麒, 介万奇. 凝固技术 [M]. 北京: 机械工业出版社, 1998: 1 | |
| [2] | Hao W S, Ma S D, Dong Z H, et al. Atomic characteristics of heterogeneous nucleation during solidification of aluminum alloys: A critical review [J]. Mater. Genome Eng. Adv., 2025, 3: e65 |
| [3] | Zhang D Y, Qiu D, Gibson M A, et al. Additive manufacturing of ultrafine-grained high-strength titanium alloys [J]. Nature, 2019, 576: 91 |
| [4] | Ren N, Li J, Zhang R Y, et al. Solute trapping and non-equilibrium microstructure during rapid solidification of additive manufacturing [J]. Nat Commun, 2023, 14: 7990 |
| [5] | Kurz W, Fisher D J, Trivedi R. Progress in modelling solidification microstructures in metals and alloys: Dendrites and cells from 1700 to 2000 [J]. Int. Mater. Rev., 2019, 64: 311 |
| [6] | Kurz W, Rappaz M, Trivedi R. Progress in modelling solidification microstructures in metals and alloys. Part II: Dendrites from 2001 to 2018 [J]. Int Mater Rev, 2021, 66: 30 |
| [7] | Dong H, Dai H. Single-crystal casting/directional solidification [J]. Compr. Mater. Process., 2014, 5: 89 |
| [8] | Dai H J, D'Souza N, Dong H B. Grain selection in spiral selectors during investment casting of single-crystal turbine blades: Part I. Experimental investigation [J]. Metall. Mater. Trans., 2011, 42A: 3430 |
| [9] | Dai H J, Dong H B, D'Souza N, et al. Grain selection in spiral selectors during investment casting of single-crystal components: Part II. Numerical modeling [J]. Metall. Mater. Trans., 2011, 42A: 3439 |
| [10] | Yang L W, Ren N, Li J, et al. Thermal-solutal convection-induced low-angle grain boundaries in single-crystal nickel-based superalloy solidification [J]. J. Mater. Sci. Technol., 2025, 208: 214 |
| [11] | Yang X L, Dong H B, Wang W, et al. Microscale simulation of stray grain formation in investment cast turbine blades [J]. Mater. Sci. Eng., 2004, A386: 129 |
| [12] | Aveson J W, Tennant P A, Foss B J, et al. On the origin of sliver defects in single crystal investment castings [J]. Acta Mater., 2013, 61: 5162 |
| [13] | Liu Y, Wang F, Ma D X, et al. Freckle prediction model incorporating geometrical effects for Ni-based single-crystal superalloy components [J]. Acta Mater., 2024, 266: 119702 |
| [14] | Ren N, Li J, Panwisawas C, et al. Insight into the sensitivities of freckles in the directional solidification of single-crystal turbine blades [J]. J. Manuf. Processes, 2022, 77: 219 |
| [15] | Perry S J, D'Souza N, Collins D M, et al. An in situ resistance-based method for tracking the temporal evolution of recovery and recrystallization in Ni-base single-crystal superalloy at super-solvus temperatures [J]. Metall. Mater. Trans., 2023, 54A: 1582 |
| [16] | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 |
| [17] | Xu Q Y, Yang C, Yan X W, et al. Development of numerical simulation in nickel-based superalloy turbine blade directional solidification [J]. Acta Metall. Sin., 2019, 55: 1175 |
| 许庆彦, 杨 聪, 闫学伟 等. 高温合金涡轮叶片定向凝固过程数值模拟研究进展 [J]. 金属学报, 2019, 55: 1175 | |
| [18] | Xu Q Y, Yang C, Zhang H, et al. Multiscale modeling and simulation of directional solidification process of Ni-based superalloy turbine blade casting [J]. Metals, 2018, 8: 632 |
| [19] | Rappaz M, Gandin C A. Probabilistic modelling of microstructure formation in solidification processes [J]. Acta Metall. Mater., 1993, 41: 345 |
| [20] | Kobayashi R. A numerical approach to three-dimensional dendritic solidification [J]. Exp. Math., 1994, 3: 59 |
| [21] | Swope W C, Andersen H C. 106-particle molecular-dynamics study of homogeneous nucleation of crystals in a supercooled atomic liquid [J]. Phys. Rev., 1990, 41B: 7042 |
| [22] | Hao W S, Ma S D, Hu Y W, et al. Solute adsorption energy criterion for discovering effective grain refiners in high-Si Al-Si alloys [J]. J. Mater. Res. Technol., 2025, 39: 506 |
| [23] | Feng S, Zhou H Y, Dong H B. Using deep neural network with small dataset to predict material defects [J]. Mater. Des., 2019, 162: 300 |
| [24] | Bai X P, Zhang X C. Artificial intelligence-powered materials science [J]. Nano-Micro Lett., 2025, 17: 135 |
| [25] | Jiang X, Xue D Z, Bai Y, et al. AI4Materials: Transforming the landscape of materials science and enigneering [J]. Rev. Mater. Res., 2025, 1: 100010 |
| [26] | Xu X W, Ren N, Lu Z Q, et al. A data-driven approach for the fast prediction of macrosegregation [J]. Metall. Mater. Trans., 2024, 55A: 2083 |
| [27] | Udu A G, Lecchini-Visintini A, Dong H B. Feature selection for aero-engine fault detection [A]. Database and Expert Systems Applications: 34th International Conference [C]. Penang: Springer, 2023: 522 |
| [28] | Dai H J, Dong H B, Atkinson H V, et al. Simulation of the columnar-to-equiaxed transition in alloy solidification—The effect of nucleation undercooling, density of nuclei in bulk liquid and alloy solidification range on the transition [J]. Solid State Phenom., 2008, 139: 129 |
| [29] | Strickland J, Nenchev B, Dong H B. On directional dendritic growth and primary spacing—A review [J]. Crystals, 2020, 10: 627 |
| [30] | Hunt J D. Steady state columnar and equiaxed growth of dendrites and eutectic [J]. Mater. Sci. Eng., 1984, 65: 75 |
| [31] | Kurz W, Fisher D J. Fundamentals of Solidification [M]. Uetikon-Zuerich: Trans Tech Publications, 1998: 67 |
| [32] | Wang W, Lee P D, McLean M. A model of solidification microstructures in nickel-based superalloys: Predicting primary dendrite spacing selection [J]. Acta Mater., 2003, 51: 2971 |
| [33] | Kermanpur A, Varahraam N, Engilehei E, et al. Directional solidification of Ni base superalloy IN738LC to improve creep properties [J]. Mater. Sci. Technol., 2000, 16: 579 |
| [34] | Hunt J D, Lu S Z. Numerical modeling of cellular/dendritic array growth: Spacing and structure predictions [J]. Metall. Mater. Trans., 1996, 27A: 611 |
| [35] | Dong H B. Evolution of dendritic patterns during directional solidification of Ni-base alloys: Towards hexagonally ordered, close-packed dendrite arrays [J]. Metall. Mater. Trans., 2026, 57A: 1709 |
| [36] | Strickland J, Nenchev B, Perry S, et al. On the nature of hexagonality within the solidification structure of single crystal alloys: Mechanisms and applications [J]. Acta Mater., 2020, 200: 417 |
| [37] | Strickland J, Nenchev B, Tassenberg K, et al. On the origin of mosaicity in directionally solidified Ni-base superalloys [J]. Acta Mater., 2021, 217: 117180 |
| [38] | Walton D, Chalmers B. The origin of the preferred orientation in the columnar zone of ingots [J]. Trans. Metall. Soc. AIME, 1959, 215: 447 |
| [39] | Takaki T, Ohno M, Shimokawabe T, et al. Two-dimensional phase-field simulations of dendrite competitive growth during the directional solidification of a binary alloy bicrystal [J]. Acta Mater., 2014, 81: 272 |
| [40] | Takaki T, Sakane S, Ohno M, et al. Large-scale phase-field studies of three-dimensional dendrite competitive growth at the converging grain boundary during directional solidification of a bicrystal binary alloy [J]. ISIJ Int., 2016, 56: 1427 |
| [41] | Ge H H, Li J, Han X J, et al. Dendritic model for macrosegregation prediction of large scale castings [J]. J. Mater. Process. Technol., 2016, 227: 308 |
| [42] | Yang L W, Ren N, Panwisawas C, et al. Melt flow-induced mechanical deformation of dendrites in alloy solidification: A coupled thermal fluid-solid mechanics approach [J]. J. Mater. Res. Technol., 2023, 25: 4094 |
| [43] | Yang L W, Ren N, Panwisawas C, et al. Melt flow-induced mechanical deformation and fracture behaviour of dendrites in alloy solidification [J]. Metall. Mater. Trans., 2023, 54A: 4612 |
| [44] | Zhou Y Z, Sun X F. Effect of solidification rate on competitive grain growth in directional solidification of a nickel-base superalloy [J]. Sci. China Technol. Sci., 2012, 55: 1327 |
| [45] | Xie X L, Zhou L P, Yu J B, et al. Effect of weak transverse magnetic field on the competitive grain growth of Ni-based superalloy with divergent bi-crystals[J]. Acta Metall. Sin., 2025, 61: 1203 |
| 谢信亮, 周丽萍, 余建波 等. 横向弱磁场对镍基高温合金发散双晶竞争生长行为的影响 [J]. 金属学报, 2025, 61: 1203 | |
| [46] | Li J J, Wang Z J, Wang Y Q, et al. Phase-field study of competitive dendritic growth of converging grains during directional solidification [J]. Acta Mater., 2012, 60: 1478 |
| [47] | Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades [J]. Acta Metall. Sin., 2015, 51: 1179 |
| 马德新. 高温合金叶片单晶凝固技术的新发展 [J]. 金属学报, 2015, 51: 1179 | |
| [48] | Hofmeister M, Franke M M, Koerner C, et al. Single crystal casting with fluidized carbon bed cooling: A process innovation for quality improvement and cost reduction [J]. Metall. Mater. Trans., 2017, 48B: 3132 |
| [49] | Wang F, Ma D X, Zhang J, et al. Effect of local cooling rates on the microstructures of single crystal CMSX-6 superalloy: A comparative assessment of the Bridgman and the downward directional solidification processes [J]. J. Alloys Compd., 2014, 616: 102 |
| [50] | Giamei A F, Tschinkel J G. Liquid metal cooling: A new solidification technique [J]. Metall. Trans., 1976, 7A: 1427 |
| [51] | Elliott A J, Pollock T M, Tin S, et al. Directional solidification of large superalloy castings with radiation and liquid-metal cooling: A comparative assessment [J]. Metall. Mater. Trans., 2004, 35A: 3221 |
| [52] | Liu L. The progress of investment casting of nickel-based superalloys [J]. Foundry, 2012, 61: 1273 |
| 刘 林. 高温合金精密铸造技术研究进展 [J]. 铸造, 2012, 61: 1273 | |
| [53] | Bondarenko Y A, Kablov E N, Surova V A, et al. Effect of high-gradient directed crystallization on the structure and properties of rhenium-bearing single-crystal alloy [J]. Met. Sci. Heat Treat., 2006, 48: 360 |
| [54] | Brundidge C L, Miller J D, Pollock T M. Development of dendritic structure in the liquid-metal-cooled, directional-solidification process [J]. Metall. Mater. Trans., 2011, 42A: 2723 |
| [55] | Miller J D, Yuan L, Lee P D, et al. Simulation of diffusion-limited lateral growth of dendrites during solidification via liquid metal cooling [J]. Acta Mater., 2014, 69: 47 |
| [56] | Miller J D, Pollock T M. Stability of dendrite growth during directional solidification in the presence of a non-axial thermal field [J]. Acta Mater., 2014, 78: 23 |
| [57] | Liu L, Huang T W, Qu M, et al. High thermal gradient directional solidification and its application in the processing of nickel-based superalloys [J]. J. Mater. Process. Technol., 2010, 210: 159 |
| [58] | Liu L, Sun D J, Huang T W, et al. Directional solidification under high thermal gradient and its application in superalloys processing [J]. Acta Metall. Sin., 2018, 54: 615 |
| 刘 林, 孙德建, 黄太文 等. 高梯度定向凝固技术及其在高温合金制备中的应用 [J]. 金属学报, 2018, 54: 615 | |
| [59] | Franke M M, Hilbinger R M, Lohmüller A, et al. The effect of liquid metal cooling on thermal gradients in directional solidification of superalloys: Thermal analysis [J]. J. Mater. Process. Technol., 2013, 213: 2081 |
| [60] | Napolitano R E, Schaefer R J. The convergence-fault mechanism for low-angle boundary formation in single-crystal castings [J]. J. Mater. Sci., 2000, 35: 1641 |
| [61] | Goulette M J, Spilling P D, Arthey R P. Cost effective single crystals [A]. Superalloys 1984: Fifth International Symposium [C]. TMS, 1984: 167 |
| [62] | D'Souza N, Jennings P A, Yang X L, et al. Seeding of single-crystal superalloys—Role of constitutional undercooling and primary dendrite orientation on stray-grain nucleation and growth [J]. Metall. Mater. Trans., 2005, 36B: 657 |
| [63] | Dantzig J A, Rappaz M. Solidification [M]. Lausanne: EPFL Press, 2016: 209 |
| [64] | Dai H J, Gebelin J C, Newell M, et al. Grain selection during solidification in spiral grain selector [A]. Superalloys 2008 [M]. Pittsburgh, PA. TMS, 2008: 367 |
| [65] | Ren N, Li J, Wang B Q, et al. Design of variable withdrawal rate for superalloy single-crystal blade fabrication [J]. Mater. Des., 2021, 198: 109347 |
| [66] | Pan D, Xu Q Y, Liu B C. Modelling on directional solidification of superalloy blades with furnace wall temperature evolution [J]. Acta Metall. Sin., 2010, 46: 294 |
| 潘 冬, 许庆彦, 柳百成. 考虑炉壁温度变化的高温合金叶片定向凝固过程模拟 [J]. 金属学报, 2010, 46: 294 | |
| [67] | Li Z L. Experimental research and numerical simulation on primary recrystallization of nickel-based single crystal superalloy [D]. Beijing: Tsinghua University, 2016 |
| 李忠林. 镍基单晶高温合金静态再结晶实验研究及数值模拟 [D]. 北京: 清华大学, 2016 | |
| [68] | Ren N, Li J, Panwisawas C, et al. Thermal-solutal-fluid flow of channel segregation during directional solidification of single-crystal nickel-based superalloys [J]. Acta Mater., 2021, 206: 116620 |
| [69] | Ren N, Panwisawas C, Li J, et al. Solute enrichment induced dendritic fragmentation in directional solidification of nickel-based superalloys [J]. Acta Mater., 2021, 215: 117043 |
| [70] | Rappaz M, Gandin C A, Desbiolles J L, et al. Prediction of grain structures in various solidification processes [J]. Metall. Mater. Trans., 1996, 27A: 695 |
| [71] | Gandin C A, Rappaz M. A coupled finite element-cellular automaton model for the prediction of dendritic grain structures in solidification processes [J]. Acta Metall. Mater., 1994, 42: 2233 |
| [72] | Gandin C A, Rappaz M, Tintillier R. 3-dimensional simulation of the grain formation in investment castings [J]. Metall. Mater. Trans., 1994, 25A: 629 |
| [73] | Meng X B, Li J G, Jin T, et al. Evolution of grain selection in spiral selector during directional solidification of nickel-base superalloys [J]. J. Mater. Sci. Technol., 2011, 27: 118 |
| [74] | Meng X B, Lu Q, Li J G, et al. Modes of grain selection in spiral selector during directional solidification of nickel-base superalloys [J]. J. Mater. Sci. Technol., 2012, 28: 214 |
| [75] | Zhang R L, Chen L N, Li C H, et al. Influence of spiral crystal selector on crystal orientation of single crystal superalloy [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 1092 |
| [76] | Wang N, Liu L, Gao S F, et al. Simulation of grain selection during single crystal casting of a Ni-base superalloy [J]. J. Alloys Compd., 2014, 586: 220 |
| [77] | Carter P, Cox D C, Gandin C A, et al. Process modelling of grain selection during the solidification of single crystal superalloy castings [J]. Mater. Sci. Eng., 2000, A280: 233 |
| [78] | Dai H J, Gebelin J C, D'Souza N, et al. Effect of spiral shape on grain selection during casting of single crystal turbine blades [J]. Int. J. Cast Met. Res., 2009, 22: 54 |
| [79] | Gao S F, Liu L, Zhang J, et al. Simulation of stray grain formation at the platform during Ni-base single crystal superalloy DD403 casting [J]. China Foundry, 2015, 12: 118 |
| [80] | Li Y F. Study on stray grain formation in the platform of Ni-based single crystal superalloys turbine blade [D]. Xi'an: Northwestern Polytechnical University, 2018 |
| 李亚峰. 镍基单晶高温合金涡轮叶片平台杂晶缺陷研究 [D]. 西安: 西北工业大学, 2018 | |
| [81] | Ma D X, Wang F, Sun H Y, et al. Study on sliver defects in single crystal castings of superalloys [J]. Foundry, 2019, 68: 567 |
| 马德新, 王 富, 孙洪元 等. 高温合金单晶铸件中条纹晶缺陷的试验研究 [J]. 铸造, 2019, 68: 567 | |
| [82] | Meng X B, Li J G, Chen Z Q, et al. Effect of platform dimension on the dendrite growth and stray grain formation in a Ni-base single-crystal superalloy [J]. Metall. Mater. Trans., 2013, 44A: 1955 |
| [83] | Sa S P, Yang W C, Qin J R, et al. Numerical simulation of blade arrangement on stray grains in a fourth-generation single crystal superalloy blade [J]. Mater. China, 2024, 43: 871 |
| 撒世鹏, 杨文超, 秦嘉润 等. 叶片排列方式对一种第四代单晶高温合金叶片杂晶影响的数值模拟研究 [J]. 中国材料进展, 2024, 43: 871 | |
| [84] | Yang W C, Sa S P, Hao W S, et al. Temperature field and microstructure simulation of directional solidification process of single crystal blade prepared efficiently with different module structures [J]. Rare Met. Mater. Eng., 2023, 52: 3847 |
| 杨文超, 撒世鹏, 郝文硕 等. 不同模组结构高效制备单晶叶片定向凝固过程的温度场及组织模拟 [J]. 稀有金属材料与工程, 2023, 52: 3847 | |
| [85] | Gandin C A, Rappaz M. A 3D Cellular Automaton algorithm for the prediction of dendritic grain growth [J]. Acta Mater., 1997, 45: 2187 |
| [86] | Thévoz P, Desbiolles J L, Rappaz M. Modeling of equiaxed microstructure formation in casting [J]. Metall. Trans., 1989, 20A: 311 |
| [87] | Kurz W, Giovanola B, Trivedi R. Theory of microstructural development during rapid solidification [J]. Acta Metall., 1986, 34: 823 |
| [88] | Dong H B, Lee P D. Simulation of the columnar-to-equiaxed transition in directionally solidified Al-Cu alloys [J]. Acta Mater., 2005, 53: 659 |
| [89] | Karma A. Phase-field model of eutectic growth [J]. Phys. Rev., 1994, 49E: 2245 |
| [90] | Takaki T. Phase-field modeling and simulations of dendrite growth [J]. ISIJ Int., 2014, 54: 437 |
| [91] | Warren J A, Boettinger W J. Prediction of dendritic growth and microsegregation patterns in a binary alloy using the phase-field method [J]. Acta Metall. Mater., 1995, 43: 689 |
| [92] | Karma A, Rappel W J. Quantitative phase-field modeling of dendritic growth in two and three dimensions [J]. Phys. Rev., 1998, 57E: 4323 |
| [93] | Steinbach I, Apel M. Multi phase field model for solid state transformation with elastic strain [J]. Physica, 2006, 217D: 153 |
| [94] | Ginzburg V L, Landau L D. On the theory of superconductivity [A]. On Superconductivity and Superfluidity: A Scientific Autobiography [M]. Berlin, Heidelberg: Springer, 2009: 113 |
| [95] | Yang C, Xu Q Y, Liu B C. Study of dendrite growth with natural convection in superalloy directional solidification via a multiphase-field-lattice Boltzmann model [J]. Comput. Mater. Sci., 2019, 158: 130 |
| [96] | Xia H, Yang Y, Feng Q, et al. Generation mechanism and motion behavior of sliver defect in single crystal Ni-based superalloy [J]. J. Mater. Sci. Technol., 2023, 137: 232 |
/
| 〈 |
|
〉 |