金属材料晶界结构的拓扑性质与表征
收稿日期: 2025-10-10
修回日期: 2025-12-24
网络出版日期: 2026-02-12
基金资助
国家自然科学基金项目(T2293691);中央高校基本科研业务费项目(NJ2024001);江苏省自然科学基金项目(BK20243065);江苏省自然科学基金项目(BK20243044);江苏省自然科学基金项目(BK20251410);机械结构力学及控制国家重点实验室研究基金项目(MCAS-L-0525K01)
Topological Properties and Characteristics of Grain Boundary Structure in Metallic Materials
Received date: 2025-10-10
Revised date: 2025-12-24
Online published: 2026-02-12
Supported by
National Natural Science Foundation of China(T2293691);Fundamental Research Funds for the Central Universities(NJ2024001);Natural Science Foundation of Jiangsu Province(BK20243065);Natural Science Foundation of Jiangsu Province(BK20243044);Natural Science Foundation of Jiangsu Province(BK20251410);Research Fund of State Key Laboratory of Mechanics and Control for Aerospace Structures(MCAS-L-0525K01)
朱思瑛 , 易敏 , 郭万林 . 金属材料晶界结构的拓扑性质与表征[J]. 金属学报, 2026 , 62(5) : 705 -720 . DOI: 10.11900/0412.1961.2025.00317
The topological properties of metallic grain boundaries are crucial in determining their mechanical, electrical, and chemical behaviors, making them a major focus of grain boundary engineering. This study systematically reviews recent advancements in understanding the topological characteristics of metallic grain boundary structures at various scales, including atomic-scale topological configurations and mesoscale grain boundary network topology. It begins by summarizing current research on the topology of grain boundary atomic structures, including the coincidence site lattice model, displacement shift complete lattice theory, topological characterisation of grain boundary dislocation networks, and analysis of topological defects. It then introduces characterisation methods for mesoscale grain boundary networks, emphasising a research framework based on discrete cell complexes and systematically examining the topological properties of these networks. Finally, potential applications of grain boundary topology research in materials design are discussed.
Key words: metallic material; grain boundary; topology; microstructure
| [1] | Zhu S Y, Borodin E, Jivkov A P. Topological characteristics of grain boundary networks during severe plastic deformations of copper alloys [J]. Acta Mater., 2023, 259: 119290 |
| [2] | Devulapalli V, Chen E Z, Brink T, et al. Topological grain boundary segregation transitions [J]. Science, 2024, 386: 420 |
| [3] | Rohrer G S. Grain boundary energy anisotropy: A review [J]. J. Mater. Sci., 2011, 46: 5881 |
| [4] | Gleiter H. On the structure of grain boundaries in metals [J]. Mater. Sci. Eng., 1982, 52: 91 |
| [5] | Priester L. Grain Boundaries: From Theory to Engineering [M]. New York: Springer, 2012: 1 |
| [6] | Randle V. The Measurement of Grain Boundary Geometry [M]. Boca Raton: CRC Press, 2017: 1 |
| [7] | Han J, Thomas S L, Srolovitz D J. Grain-boundary kinetics: A unified approach [J]. Prog. Mater. Sci., 2018, 98: 386 |
| [8] | Schuh C A, Lu K. Stability of nanocrystalline metals: The role of grain-boundary chemistry and structure [J]. MRS Bull., 2021, 46: 225 |
| [9] | Palumbo G, Aust K T. Structure-dependence of intergranular corrosion in high purity nickel [J]. Acta Metall. Mater., 1990, 38: 2343 |
| [10] | Liu G H, Wang W G, Rohrer G S, et al. {111}/{111} near singular boundaries in a dynamically recrystallized Al-Zn-Mg-Cu alloy compressed at elevated temperature [J]. Acta Metall. Sin., 2024, 60: 1165 |
| 刘光辉, 王卫国, Rohrer G S 等. 高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界 [J]. 金属学报, 2024, 60: 1165 | |
| [11] | Wang G J, Vitek V. Relationships between grain boundary structure and energy [J]. Acta Metall., 1986, 34: 951 |
| [12] | Bulatov V V, Reed B W, Kumar M. Grain boundary energy function for fcc metals [J]. Acta Mater., 2014, 65: 161 |
| [13] | Ratanaphan S, Olmsted D L, Bulatov V V, et al. Grain boundary energies in body-centered cubic metals [J]. Acta Mater., 2015, 88: 346 |
| [14] | Chen K T, Srolovitz D J, Han J. Grain-boundary topological phase transitions [J]. Proc. Natl. Acad. Sci. USA, 2020, 117: 33077 |
| [15] | Wang J W, Chen Y B, Zhu Q, et al. Grain boundary dominated plasticity in metallic materials [J]. Acta Metall. Sin., 2022, 58: 726 |
| 王江伟, 陈映彬, 祝 祺 等. 金属材料的晶界塑性变形机制 [J]. 金属学报, 2022, 58: 726 | |
| [16] | Reed B W, Kumar M, Minich R W, et al. Fracture roughness scaling and its correlation with grain boundary network structure [J]. Acta Mater., 2008, 56: 3278 |
| [17] | Gao Y, Liu X, Wang Y Q, et al. The role of special grain boundaries in enhancing creep performance in the welded joint of a novel Fe-Ni-based superalloy through aging treatment [J]. Mater. Charact., 2025, 224: 115010 |
| [18] | Zheng X Y, Chen X, He M L, et al. Multi-scale simulation of mechanical properties of 6XXX aluminum alloy based on crystal plasticity [J]. Acta Metall. Sin., 2025, 61: 1758 |
| 郑潇禹, 陈 辛, 何美玲 等. 基于晶体塑性的6XXX铝合金力学性能多尺度计算 [J]. 金属学报, 2025, 61: 1758 | |
| [19] | Hu C Z, Li Y W, Yu Z Y, et al. Computing grain boundary diagrams of thermodynamic and mechanical properties [J]. npj Comput. Mater., 2021, 7: 159 |
| [20] | Marquardt K, Rohrer G S, Morales L, et al. The most frequent interfaces in olivine aggregates: The GBCD and its importance for grain boundary related processes [J]. Contrib. Mineral. Petrol., 2015, 170: 40 |
| [21] | Chookajorn T, Murdoch H A, Schuh C A. Design of stable nanocrystalline alloys [J]. Science, 2012, 337: 951 |
| [22] | Garner A, Euesden R, Yao Y C, et al. Multiscale analysis of grain boundary microstructure in high strength 7xxx Al alloys [J]. Acta Mater., 2021, 202: 190 |
| [23] | Wilde G, Divinski S. Grain boundaries and diffusion phenomena in severely deformed materials [J]. Mater. Trans., 2019, 60: 1302 |
| [24] | Leitner K, Lutz D, Knabl W, et al. Grain boundary segregation engineering in as-sintered molybdenum for improved ductility [J]. Scr. Mater., 2018, 156: 60 |
| [25] | Zhu Y L, Cao Y, Tian W, et al. New insights into ductility improvement of a nickel-based superalloy through grain boundary engineering [J]. Mater. Sci. Eng., 2024, A908: 146786 |
| [26] | Tikhonova M, Kaibyshev R, Belyakov A. Microstructure and mechanical properties of austenitic stainless steels after dynamic and post-dynamic recrystallization treatment [J]. Adv. Eng. Mater., 2018, 20: 1700960 |
| [27] | Zhuo Z, Xia S, Bai Q, et al. The effect of grain boundary character distribution on the mechanical properties at different strain rates of a 316L stainless steel [J]. J. Mater. Sci., 2018, 53: 2844 |
| [28] | Naydenkin E V, Ratochka I V, Mishin I P, et al. The effect of interfaces on mechanical and superplastic properties of titanium alloys [J]. J. Mater. Sci., 2017, 52: 4164 |
| [29] | Li L L, Zhang P, Zhang Z J, et al. Strain localization and fatigue cracking behaviors of Cu bicrystal with an inclined twin boundary [J]. Acta Mater., 2014, 73: 167 |
| [30] | Jin Y J, Lu H, Yu C, et al. Study on grain boundary character and strain distribution of intergranular cracking in the CGHAZ of T23 steel [J]. Mater. Charact., 2013, 84: 216 |
| [31] | Das A. Grain boundary engineering: fatigue fracture [J]. Philos. Mag., 2017, 97: 867 |
| [32] | Lu K. Stabilizing nanostructures in metals using grain and twin boundary architectures [J]. Nat. Rev. Mater., 2016, 1: 16019 |
| [33] | Van Swygenhoven H. Grain boundaries and dislocations [J]. Science, 2002, 296: 66 |
| [34] | Hirth J P. The influence of grain boundaries on mechanical properties [J]. Metall. Trans., 1972, 3: 3047 |
| [35] | Palumbo G, Lehockey E M, Lin P. Applications for grain boundary engineered materials [J]. JOM, 1998, 50(2): 40 |
| [36] | Randle V, Ralph B. Grain boundary structure and mechanical properties [J]. Rev. Phys. Appl., 1988, 23: 501 |
| [37] | Kheradmand N, Barnoush A, Vehoff H. Investigation of the role of grain boundary on the mechanical properties of metals [J]. J. Phys.: Conf. Ser., 2010, 240: 012017 |
| [38] | Randle V, Owen G. Mechanisms of grain boundary engineering [J]. Acta Mater., 2006, 54: 1777 |
| [39] | Randle V. ‘Special’ boundaries and grain boundary plane engineering [J]. Scr. Mater., 2006, 54: 1011 |
| [40] | Randle V. Grain boundary engineering: An overview after 25 years [J]. Mater. Sci. Technol., 2010, 26: 253 |
| [41] | Watanabe T. Grain boundary engineering: Historical perspective and future prospects [J]. J. Mater. Sci., 2011, 46: 4095 |
| [42] | Raabe D, Herbig M, Sandl?bes S, et al. Grain boundary segregation engineering in metallic alloys: A pathway to the design of interfaces [J]. Curr. Opin. Solid State Mater. Sci., 2014, 18: 253 |
| [43] | Xu X M, Zhong Y J, Wajrak M, et al. Grain boundary engineering: An emerging pathway toward efficient electrocatalysis [J]. InfoMat, 2024, 6: e12608 |
| [44] | Tiamiyu A A, Pang E L, Chen X, et al. Nanotwinning-assisted dynamic recrystallization at high strains and strain rates [J]. Nat. Mater., 2022, 21: 786 |
| [45] | Figueiredo R B, Langdon T G. Fabricating ultrafine-grained materials through the application of severe plastic deformation: A review of developments in brazil [J]. J. Mater. Res. Technol., 2012, 1: 55 |
| [46] | Panzarino J F, Pan Z L, Rupert T J. Plasticity-induced restructuring of a nanocrystalline grain boundary network [J]. Acta Mater., 2016, 120: 1 |
| [47] | Fu H L, Zhou X, Gao Z P, et al. Effect of grain geometry on the stability of polycrystalline Pt at the nanoscale [J]. Phys. Rev. Lett., 2025, 134: 056101 |
| [48] | Zhang L, Lu C, Tieu K. A review on atomistic simulation of grain boundary behaviors in face-centered cubic metals [J]. Comput. Mater. Sci., 2016, 118: 180 |
| [49] | Pan X L, Zhou L C, Wang C X, et al. Microstructure and residual stress modulation of 7075 aluminum alloy for improving fatigue performance by laser shock peening [J]. Int. J. Mach. Tools Manuf., 2023, 184: 103979 |
| [50] | Abdeljawad F, Foiles S M, Moore A P, et al. The role of the interface stiffness tensor on grain boundary dynamics [J]. Acta Mater., 2018, 158: 440 |
| [51] | Randle V. The Role of the Coincidence Site Lattice in Grain Boundary Engineering [M]. London: CRC Press, 2024: 1 |
| [52] | Lee D S, Ryoo H S, Hwang S K. A grain boundary engineering approach to promote special boundaries in Pb-base alloy [J]. Mater. Sci. Eng., 2003, A354: 106 |
| [53] | Warren P, Raju N, Prasad A, et al. Grain and grain boundary segmentation using machine learning with real and generated datasets [J]. Comput. Mater. Sci., 2024, 233: 112739 |
| [54] | Zhu Q, Samanta A, Li B X, et al. Predicting phase behavior of grain boundaries with evolutionary search and machine learning [J]. Nat. Commun., 2018, 9: 467 |
| [55] | Huber L, Hadian R, Grabowski B, et al. A machine learning approach to model solute grain boundary segregation [J]. npj Comput. Mater., 2018, 4: 64 |
| [56] | Zhang J N, Koneru A, Sankaranarayanan S K R S, et al. Graph neural network guided evolutionary search of grain boundaries in 2D materials [J]. ACS Appl. Mater. Interfaces, 2023, 15: 20520 |
| [57] | van Beers P R M, Kouznetsova V G, Geers M G D, et al. A multiscale model of grain boundary structure and energy: From atomistics to a continuum description [J]. Acta Mater., 2015, 82: 513 |
| [58] | Song X Y, Deng C. Atomic energy in grain boundaries studied by machine learning [J]. Phys. Rev. Mater., 2022, 6: 043601 |
| [59] | Patala S. Topological analysis of the grain boundary space [D]. Cambridge: Massachusetts Institute of Technology, 2011 |
| [60] | Wakai F, Shinoda Y, Ishihara S, et al. Topological transformation of grains in three-dimensional normal grain growth [J]. J. Mater. Res., 2001, 16: 2136 |
| [61] | Gao N N, Zhao Y, Xia W Q, et al. Phase-field crystal studies on grain boundary migration, dislocation behaviors, and topological transition under tension of square polycrystals [J]. Crystals, 2023, 13: 777 |
| [62] | Narang P, Garcia C A C, Felser C. The topology of electronic band structures [J]. Nat. Mater., 2021, 20: 293 |
| [63] | Gupta S, Saxena A. A topological twist on materials science [J]. MRS Bull., 2014, 39: 265 |
| [64] | Hirth J P, Balluffi R W. On grain boundary dislocations and ledges [J]. Acta Metall., 1973, 21: 929 |
| [65] | Gleiter H. Nanostructured materials: Basic concepts and microstructure [J]. Acta Mater., 2000, 48: 1 |
| [66] | Zhu Q, Zhao Q K, Huang Q S, et al. Grain boundary plasticity initiated by excess volume [J]. Proc. Natl. Acad. Sci. USA, 2024, 121: e2400161121 |
| [67] | Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141 |
| [68] | Hellman O C, Vandenbroucke J A, Rüsing J, et al. Analysis of three-dimensional atom-probe data by the proximity histogram [J]. Microsc. Microanal., 2000, 6: 437 |
| [69] | Wagih M, Larsen P M, Schuh C A. Learning grain boundary segregation energy spectra in polycrystals [J]. Nat. Commun., 2020, 11: 6376 |
| [70] | Wei C Z, Thomas S L, Han J, et al. A continuum multi-disconnection-mode model for grain boundary migration [J]. J. Mech. Phys. Solids, 2019, 133: 103731 |
| [71] | Wang L H, Zhang Y, Zeng Z, et al. Tracking the sliding of grain boundaries at the atomic scale [J]. Science, 2022, 375: 1261 |
| [72] | Lu K. Gradient nanostructured materials [J]. Acta Metall. Sin., 2015, 51: 1 |
| 卢 柯. 梯度纳米结构材料 [J]. 金属学报, 2015, 51: 1 | |
| [73] | Fu H L, Zhou X, Gao Z P, et al. Pt Schwarz crystals stabilized by minimal-surface grain boundaries and twins at the grain size limit [J]. Acta Mater., 2024, 276: 120007 |
| [74] | Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422 |
| [75] | Zhu Q, Huang Q S, Guang C, et al. Metallic nanocrystals with low angle grain boundary for controllable plastic reversibility [J]. Nat. Commun., 2020, 11: 3100 |
| [76] | Cantwell P R, Tang M, Dillon S J, et al. Grain boundary complexions [J]. Acta Mater., 2014, 62: 1 |
| [77] | Cantwell P R, Frolov T, Rupert T J, et al. Grain boundary complexion transitions [J]. Annu. Rev. Mater. Res., 2020, 50: 465 |
| [78] | Zhang Z B, Yang Z B, Lu S, et al. Strain localisation and failure at twin-boundary complexions in nickel-based superalloys [J]. Nat. Commun., 2020, 11: 4890 |
| [79] | Krause A R, Cantwell P R, Marvel C J, et al. Review of grain boundary complexion engineering: Know your boundaries [J]. J. Am. Ceram. Soc., 2019, 102: 778 |
| [80] | Grimmer H, Bollmann W, Warrington D H. Coincidence-site lattices and complete pattern-shift in cubic crystals [J]. Acta Cryst., 1974, 30A: 197 |
| [81] | Bollmann W. Crystal Defects and Crystalline Interfaces [M]. Berlin: Springer, 2012: 1 |
| [82] | Pond R C, Bollmann W. The symmetry and interfacial structure of bicrystals [J]. Philos. Trans. Roy. Soc., 1979, 292A: 449 |
| [83] | Warrington D H, Bollmann W. Dislocation networks in high-angle grain boundaries [J]. Philos. Mag., 1972, 25: 1195 |
| [84] | Bollmann W. On the geometry of grain and phase boundaries: I. General theory [J]. Philos. Mag., 1967, 16: 363 |
| [85] | Randle V, Rohrer G S, Miller H M, et al. Five-parameter grain boundary distribution of commercially grain boundary engineered nickel and copper [J]. Acta Mater., 2008, 56: 2363 |
| [86] | Ratanaphan S, Yoon Y, Rohrer G S. The five parameter grain boundary character distribution of polycrystalline silicon [J]. J. Mater. Sci., 2014, 49: 4938 |
| [87] | An D, Griffiths T A, Konijnenberg P, et al. Correlating the five parameter grain boundary character distribution and the intergranular corrosion behaviour of a stainless steel using 3D orientation microscopy based on mechanical polishing serial sectioning [J]. Acta Mater., 2018, 156: 297 |
| [88] | Brandon D G. The structure of high-angle grain boundaries [J]. Acta Metall., 1966, 14: 1479 |
| [89] | Bollmann W. The basic concepts of the 0-lattice theory [J]. Surf. Sci., 1972, 31: 1 |
| [90] | Bollmann W. O‐lattice calculation of an F.C.C.-B.C.C. interface [J]. Phys. Status Solidi, 1974, 21A: 543 |
| [91] | Li M, Xu T. Topological and atomic scale characterization of grain boundary networks in polycrystalline and nanocrystalline materials [J]. Prog. Mater. Sci., 2011, 56: 864 |
| [92] | Jin Z H, Li X Y, Lu K. Formation of stable schwarz crystals in polycrystalline copper at the grain size limit [J]. Phys. Rev. Lett., 2021, 127: 136101 |
| [93] | Xu W, Zhang B, Li X Y, et al. Suppressing atomic diffusion with the Schwarz crystal structure in supersaturated Al-Mg alloys [J]. Science, 2021, 373: 683 |
| [94] | Gu J L, Duan F H, Liu S D, et al. Phase engineering of nanostructural metallic materials: Classification, structures, and applications [J]. Chem. Rev., 2024, 124: 1247 |
| [95] | Meiners T, Frolov T, Rudd R E, et al. Observations of grain-boundary phase transformations in an elemental metal [J]. Nature, 2020, 579: 375 |
| [96] | Zhu S Y, Jivkov A P, Borodin E, et al. Triple junction disclinations in severely deformed Cu-0.4%Mg alloys [J]. Acta Mater., 2024, 264: 119600 |
| [97] | Bollmann W. Triple lines in polycrystalline aggregates as disclinations [J]. Philos. Mag., 1984, 49A: 73 |
| [98] | Bollmann W. Triple-line disclinations representations, continuity and reactions [J]. Philos. Mag., 1988, 57A: 637 |
| [99] | Liu Y, Leung S, Li F F, et al. Bulk-disclination correspondence in topological crystalline insulators [J]. Nature, 2021, 589: 381 |
| [100] | Wu M S, Zhou K, Nazarov A A. Crack nucleation at disclinated triple junctions [J]. Phys. Rev., 2007, 76B: 134105 |
| [101] | Barnett A K, Hussein O, Alghalayini M, et al. Triple junction segregation dominates the stability of nanocrystalline alloys [J]. Nano Lett., 2024, 24: 9627 |
| [102] | Wei C Z, Zhang C L, Han J, et al. Grain boundary triple junction dynamics: A continuum disconnection model [J]. SIAM J. Appl. Math., 2020, 80: 1101 |
| [103] | Annevelink E, Ertekin E, Johnson H T. Grain boundary structure and migration in graphene via the displacement shift complete lattice [J]. Acta Mater., 2019, 166: 67 |
| [104] | Song X Q, Tang L Y, Wang Y X, et al. Plastic strain-induced evolution of CSL boundaries at elevated temperature for Ni-base superalloy: Experimental and phase-field perspective [J]. J. Mater. Res. Technol., 2020, 9: 2535 |
| [105] | Zhou S Y, Hu M H, Li C, et al. Creep behavior of a Ni-based superalloy with strengthening of γ' and γ'' phases [J]. Acta Metall. Sin., 2025, 61: 226 |
| 周生玉, 胡明昊, 李 冲 等. 一种γ'/γ''相强化镍基高温合金的蠕变行为 [J]. 金属学报, 2025, 61: 226 | |
| [106] | Zhang Y, He C Y, Yu Q, et al. Nacre-like surface nanolaminates enhance fatigue resistance of pure titanium [J]. Nat. Commun., 2024, 15: 6917 |
| [107] | Zhou X Y, Ahmadian A, Gault B, et al. Atomic motifs govern the decoration of grain boundaries by interstitial solutes [J]. Nat. Commun., 2023, 14: 3535 |
| [108] | Schuh C A, Kumar M, King W E. Analysis of grain boundary networks and their evolution during grain boundary engineering [J]. Acta Mater., 2003, 51: 687 |
| [109] | Kumar M, King W E, Schwartz A J. Modifications to the microstructural topology in f.c.c. materials through thermomechanical processing [J]. Acta Mater., 2000, 48: 2081 |
| [110] | Farabi E, Tari V, Hodgson P D, et al. On the grain boundary network characteristics in a martensitic Ti-6Al-4V alloy [J]. J. Mater. Sci., 2020, 55: 15299 |
| [111] | Chen Y B, Han J, Deng H L, et al. Revealing grain boundary kinetics in three-dimensional space [J]. Acta Mater., 2024, 268: 119717 |
| [112] | Priedeman J L, Rosenbrock C W, Johnson O K, et al. Quantifying and connecting atomic and crystallographic grain boundary structure using local environment representation and dimensionality reduction techniques [J]. Acta Mater., 2018, 161: 431 |
| [113] | Palumbo G, Thorpe S J, Aust K T. On the contribution of triple junctions to the structure and properties of nanocrystalline materials [J]. Scr. Metall. Mater., 1990, 24: 1347 |
| [114] | Chen E Z, Heo T W, Wood B C, et al. Grand canonically optimized grain boundary phases in hexagonal close-packed titanium [J]. Nat. Commun., 2024, 15: 7049 |
| [115] | Yazyev O V, Louie S G. Topological defects in graphene: Dislocations and grain boundaries [J]. Phys. Rev., 2010, 81B: 195420 |
| [116] | Korbuly B, Plapp M, Henry H, et al. Topological defects in two-dimensional orientation-field models for grain growth [J]. Phys. Rev., 2017, 96E: 052802 |
| [117] | Barr C M, Leff A C, Demott R W, et al. Unraveling the origin of twin related domains and grain boundary evolution during grain boundary engineering [J]. Acta Mater., 2018, 144: 281 |
| [118] | Kinderlehrer D, Liu C. Evolution of grain boundaries [J]. Math. Models Methods Appl. Sci., 2001, 11: 713 |
| [119] | Ni?o J D, Johnson O K. Influence of grain boundary energy anisotropy on the evolution of grain boundary network structure during 3D anisotropic grain growth [J]. Comput. Mater. Sci, 2023, 217: 111879 |
| [120] | Luo M, Liao X Z, Ringer S P, et al. Grain boundary network evolution in electron-beam powder bed fusion nickel-based superalloy Inconel 738 [J]. J. Alloys Compd., 2024, 972: 172811 |
| [121] | Yang X Y, Wang P, Huang M. Grain boundary evolution during low-strain grain boundary engineering achieved by strain-induced boundary migration in pure copper [J]. Mater. Sci. Eng., 2022, A833: 142532 |
| [122] | Volovitch P, Traskine V, Barrallier L. Analysis of grain boundary network topology using grain boundary wetting [J]. Z. Metallkd., 2004, 95: 215 |
| [123] | Minich R W, Schuh C A, Kumar M. Role of topological constraints on the statistical properties of grain boundary networks [J]. Phys. Rev., 2002, 66B: 052101 |
| [124] | Rohrer G S, Miller H M. Topological characteristics of plane sections of polycrystals [J]. Acta Mater., 2010, 58: 3805 |
| [125] | Liu T G, Xia S, Zhou B X, et al. Three-dimensional geometrical and topological characteristics of grains in conventional and grain boundary engineered 316L stainless steel [J]. Micron, 2018, 109: 58 |
| [126] | Li X Y, Jin Z H, Zhou X, et al. Constrained minimal-interface structures in polycrystalline copper with extremely fine grains [J]. Science, 2020, 370: 831 |
| [127] | Rollett A D, Lee S B, Campman R, et al. Three-dimensional characterization of microstructure by electron back-scatter diffraction [J]. Annu. Rev. Mater. Res., 2007, 37: 627 |
| [128] | Christopher W A, Oliver K J. A decision transformer approach to grain boundary network optimization [J]. Comput. Mater. Sci., 2025, 253: 113852 |
| [129] | Irukuvarghula S, Hassanin H, Cayron C, et al. Evolution of grain boundary network topology in 316L austenitic stainless steel during powder hot isostatic pressing [J]. Acta Mater., 2017, 133: 269 |
| [130] | Patala S, Mason J K, Schuh C A. Improved representations of misorientation information for grain boundary science and engineering [J]. Prog. Mater. Sci., 2012, 57: 1383 |
| [131] | Johnson O K, Lund J M, Critchfield T R. Spectral graph theory for characterization and homogenization of grain boundary networks [J]. Acta Mater., 2018, 146: 42 |
| [132] | Valiev R Z, Langdon T G. Principles of equal-channel angular pressing as a processing tool for grain refinement [J]. Prog. Mater. Sci., 2006, 51: 881 |
| [133] | Winning M, Gottstein G, Shvindlerman L S. On the mechanisms of grain boundary migration [J]. Acta Mater., 2002, 50: 353 |
| [134] | Voyiadjis G Z. Grain boundary migration in metals: Thermodynamics, kinetics, applications [J]. J. Eng. Mech., 2000, 126: 888 |
| [135] | Jia H R, Duan S Y, Zhang Z, et al. Homogenization-based topology optimization for self-supporting additive-manufactured lattice-infilled structure [J]. Mater. Des., 2024, 245: 113264 |
| [136] | Rohrer G S. Measuring and interpreting the structure of grain-boundary networks [J]. J. Am. Ceram. Soc., 2011, 94: 633 |
| [137] | Barr C M, Thomas S, Hart J L, et al. Tracking the evolution of intergranular corrosion through twin-related domains in grain boundary networks [J]. npj Mater. Degrad., 2018, 2: 14 |
| [138] | Liu T G, Xia S, Li H, et al. The highly twinned grain boundary network formation during grain boundary engineering [J]. Mater. Lett., 2014, 133: 97 |
| [139] | Zhu X J, Fan Q B, Liu X, et al. Microstructure evolution and mechanical properties of a hot-rolled Ti alloy [J]. Prog. Nat. Sci.: Mater. Int., 2021, 31: 105 |
| [140] | Johnson O K, Schuh C A. The triple junction hull: Tools for grain boundary network design [J]. J. Mech. Phys. Solids, 2014, 69: 2 |
| [141] | Frary M, Schuh C A. Connectivity and percolation behaviour of grain boundary networks in three dimensions [J]. Philos. Mag., 2005, 85: 1123 |
| [142] | Liang C G, Yin Y, Wang W X, et al. A thermodynamically consistent non-isothermal phase-field model for selective laser sintering [J]. Int. J. Mech. Sci., 2023, 259: 108602 |
| [143] | Zhang B B, Tang Y G, Mei Q S, et al. Inhibiting creep in nanograined alloys with stable grain boundary networks [J]. Science, 2022, 378: 659 |
| [144] | Bhattacharya A, Shen Y F, Hefferan C M, et al. Grain boundary velocity and curvature are not correlated in Ni polycrystals [J]. Science, 2021, 374: 189 |
| [145] | Lin B, Jin Y, Hefferan C M, et al. Observation of annealing twin nucleation at triple lines in nickel during grain growth [J]. Acta Mater., 2015, 99: 63 |
| [146] | Liu T G, Xia S, Zhou B X, et al. Three-dimensional characteristics of the grain boundary networks of conventional and grain boundary engineered 316L stainless steel [J]. Mater. Charact., 2017, 133: 60 |
| [147] | Wanner T, Fuller E R, Saylor D M. Homology metrics for microstructure response fields in polycrystals [J]. Acta Mater., 2010, 58: 102 |
| [148] | Kobayashi S, Tsurekawa S, Watanabe T. A new approach to grain boundary engineering for nanocrystalline materials [J]. Beilstein J. Nanotechnol., 2016, 7: 1829 |
| [149] | Yang D, Bai Q, Hu Y, et al. Fractal analysis of the effect of grain boundary character on Te-induced brittle cracking in GH3535 alloy [J]. Acta Metall. Sin., 2023, 59: 248 |
| 杨 杜, 白 琴, 胡 悦 等. GH3535合金中晶界特征对碲致脆性开裂影响的分形分析 [J]. 金属学报, 2023, 59: 248 | |
| [150] | Zhu S Y. In silico grain boundary engineering by analysis on discrete complexes [D]. Manchester: The University of Manchester, 2023 |
| [151] | Hatcher A. Algebraic Topology [M]. Beijing: Tsinghua University, 2005: 1 |
| [152] | Salnikov V, Cassese D, Lambiotte R. Simplicial complexes and complex systems [J]. Eur. J. Phys., 2018, 40: 014001 |
| [153] | Zhu S Y, Gao W J, Yi M, et al. Integrated discrete cell complexes and finite element analysis for microstructure topology evolution during severe plastic deformation [J]. Comput. Mater. Contin., 2025, 85: 657 |
/
| 〈 |
|
〉 |