金属塑性成形的应变路径效应:机制、表征与应用
收稿日期: 2025-09-29
修回日期: 2025-11-26
网络出版日期: 2026-01-28
基金资助
国家自然科学基金项目(52130507);国家自然科学基金项目(U24B2055)
Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
Received date: 2025-09-29
Revised date: 2025-11-26
Online published: 2026-01-28
Supported by
National Natural Science Foundation of China(52130507);National Natural Science Foundation of China(U24B2055)
应变路径是决定塑性成形金属构件形状、组织和性能等成形质量的重要因素。为提升成形质量,通常需要设计非线性的复杂应变路径。复杂应变路径必然引起更复杂的多尺度变形行为,因此,其机制分析和表征成为塑性成形领域研究的前沿和热点。本文系统探讨了复杂应变路径下的宏观力学响应、损伤行为以及显微组织和织构演化规律,总结了路径历史在多尺度变形机制中的作用特征。梳理了基于应变路径效应的材料成形有限元建模思路和方法,包括材料本构模型、极限预测与损伤模型和微观组织演化模型,阐述了其在提升变形预测精度和工艺模拟效果方面的价值。分析了工程应用中面向成形性和服役性能优化的路径设计策略,突出了其在形性调控方面的潜力。最后,对金属塑性成形的应变路径效应未来的研究方向进行了展望。
樊晓光 , 肖云腾 , 詹梅 , 马飞 , 高鹏飞 , 郑泽邦 , 张昕 , 邵光大 , 伍寓铭 . 金属塑性成形的应变路径效应:机制、表征与应用[J]. 金属学报, 2026 , 62(5) : 975 -992 . DOI: 10.11900/0412.1961.2025.00294
Strain path is a critical factor governing the forming quality of metallic components, including their geometry, microstructure, and service performance. Achieve high-quality forming often requires the use of nonlinear and complex strain paths, which inevitably give rise to multiscale deformation behaviors. Understanding and characterizing these mechanisms has therefore become a frontier topic in the field of plastic forming. This review synthesizes recent advances in the investigation of macroscopic mechanical responses, damage behavior, and microstructural and textural evolutions under complex strain paths, emphasizing the central role of stress path history in shaping multiscale deformation mechanisms. Finite element modeling strategies that account for strain path effects are discussed, including constitutive models, limit prediction and damage models, as well as microstructure evolution models, with particular attention to their roles in improving predictive accuracy and process simulation capabilities. Engineering-oriented approaches to strain path design are also summarized, highlighting their potential for optimizing formability and service performance. Finally, perspectives on future research directions are presented.
| [1] | Yang H. Local Loading Control of Nonuniform Deformation and Precise Plastic Forming: Principles and Techniques [M]. Beijing: Science Press, 2014: 1 |
| 杨 合. 局部加载控制不均匀变形与精确塑性成形: 原理和技术 [M]. 北京: 科学出版社, 2014: 1 | |
| [2] | Lin Z Q, Huang Q X, Yuan S J, et al. Major breakthrough and progress in metal forming technology and equipment of China in the last 30 years [J]. J. Plast. Eng., 2024, 31(4): 2 |
| 林忠钦, 黄庆学, 苑世剑 等. 中国塑性成形技术和装备30年的重大突破与进展 [J]. 塑性工程学报, 2024, 31(4): 2 | |
| [3] | Schmitt J H, Shen E L, Raphanel J L. A parameter for measuring the magnitude of a change of strain path: Validation and comparison with experiments on low carbon steel [J]. Int. J. Plast., 1994, 10: 535 |
| [4] | Dunand M, Maertens A P, Luo M, et al. Experiments and modeling of anisotropic aluminum extrusions under multi-axial loading—Part I: Plasticity [J]. Int. J. Plast., 2012, 36: 34 |
| [5] | Shi B D, Shi R, Zhao H, et al. Review on deformation behavior of sheet metal during biaxial compression [J]. Forg. Stamp. Technol., 2024, 49(7): 19 |
| 石宝东, 石 瑞, 赵 辉 等. 金属板材双轴压缩变形行为研究进展 [J]. 锻压技术, 2024, 49(7): 19 | |
| [6] | Jiang X Q, Fan X G, Zhan M, et al. Research progress on plastic flow instability during hot deformation of metal materials [J]. J. Plast. Eng., 2020, 27(7): 33 |
| 姜雪琦, 樊晓光, 詹 梅 等. 金属材料热变形中的塑性流动失稳研究进展 [J]. 塑性工程学报, 2020, 27(7): 33 | |
| [7] | Gautam P C, Al-Samman T, Thangaraju S, et al. Effect of ECAP strain path on deformation behaviour, microstructure, texture evolution, and mechanical properties in magnesium [J]. Mater. Sci. Eng., 2024, A913: 147077 |
| [8] | Bharti A, Dey R, Sivaprasad S, et al. Deformation response and microstructure evolution in 304LN stainless steel subjected to multiaxial fatigue loading under different strain paths [J]. Int. J. Press. Vessels Pip., 2025, 214: 105452 |
| [9] | Dhara S, Taylor S, Figiel ?, et al. Development of a novel testing methodology for in-situ microstructural characterisation during continuous strain path change [J]. Mater. Charact., 2022, 183: 111610 |
| [10] | Jiang X Q. Study on the correlation between strain localization and microstructure of TA15 titanium alloy and its prediction [D]. Xi’an: Northwestern Polytechnical University, 2021 |
| 姜雪琦. TA15钛合金应变局部化的组织相关性与预测研究 [D]. 西安: 西北工业大学, 2021 | |
| [11] | Xie Z X, Fan X G, Wang L, et al. Stepwise cooling spinning to achieve isotropic strength-ductility synergy of titanium alloy tube [J]. J. Mater. Sci. Technol., 2026, 244: 156 |
| [12] | Li H W, Gao J, Sun X X, et al. Research developments on multiscale modeling and simulation towards high-performance plastic forming [J]. J. Mech. Eng., 2024, 60(1): 27 |
| 李宏伟, 高 佳, 孙新新 等. 面向高性能塑性成形的多尺度建模仿真研究进展 [J]. 机械工程学报, 2024, 60(1): 27 | |
| [13] | Zhao T Z, Zhang S H, Cheng M, et al. Development of strain path effects on the mechanical behaviors of metals [J]. Forg. Stamp. Technol., 2016, 41(10): 1 |
| 赵天章, 张士宏, 程 明 等. 金属力学行为中应变路径效应的研究进展 [J]. 锻压技术, 2016, 41(10): 1 | |
| [14] | Boger R K, Wagoner R H, Barlat F, et al. Continuous, large strain, tension/compression testing of sheet material [J]. Int. J. Plast., 2005, 21: 2319 |
| [15] | Liao J, Xue X, Lee M G, et al. Constitutive modeling for path-dependent behavior and its influence on twist springback [J]. Int. J. Plast., 2017, 93: 64 |
| [16] | Van Petegem S, Wagner J, Panzner T, et al. In-situ neutron diffraction during biaxial deformation [J]. Acta Mater., 2016, 105: 404 |
| [17] | Zhan M, Dong Y D, Zhai Z L, et al. Review on fast numerical simulation method for plastic forming [J]. J. Mech. Eng., 2022, 58(16): 2 |
| 詹 梅, 董赟达, 翟卓蕾 等. 塑性成形快速数值仿真方法的研究进展 [J]. 机械工程学报, 2022, 58(16): 2 | |
| [18] | Guo S Q, Yan S L, Huang L, et al. A strain-path dependent unified constitutive model of titanium alloy coupling coarse grain subdivision and recrystallization: Application to multi-directional hot deformation [J]. Int. J. Plast., 2025, 186: 104248 |
| [19] | Fan R L, Chen M H, Wu D P, et al. Research progress of forming limit of sheet metal under nonlinear loading path [J]. J. Plast. Eng., 2024, 31(2): 1 |
| 范荣磊, 陈明和, 吴迪鹏 等. 非线性加载路径下金属薄板成形极限研究进展 [J]. 塑性工程学报, 2024, 31(2): 1 | |
| [20] | Yang B, Zhang W G, Lin Z Q, et al. The study of loading path optimization for tube hydroforming process [J]. J. Plast. Eng., 2006, 13(4): 10 |
| 杨 兵, 张卫刚, 林忠钦 等. 管件液压成形中加载路径的优化设计方法研究 [J]. 塑性工程学报, 2006, 13(4): 10 | |
| [21] | Sharma R, Sargeant D, Daroju S, et al. Multi-strain path deformation behavior of AA6016-T4: Experiments and crystal plasticity modeling [J]. Int. J. Solids Struct., 2022, 244-245: 111536 |
| [22] | Daroju S, Kuwabara T, Sharma R, et al. Experimental characterization and crystal plasticity modeling for predicting load reversals in AA6016-T4 and AA7021-T79 [J]. Int. J. Plast., 2022, 153: 103292 |
| [23] | Li F, Zhang H Y, He W W, et al. Compression and tensile consecutive deformation behavior of Mn18Cr18N austenite stainless steel [J]. Acta Metall. Sin., 2016, 52: 956 |
| 李 飞, 张华煜, 何文武 等. Mn18Cr18N奥氏体不锈钢的压缩拉伸连续加载变形行为 [J]. 金属学报, 2016, 52: 956 | |
| [24] | Xu S, Liu T M, Ding X Z, et al. Reducing the anisotropy of a pre-twinned hot-rolled Mg-3Al-1Zn alloy by plane-strain compression [J]. Mater. Sci. Eng., 2014, A592: 230 |
| [25] | Shi B D, Peng Y, Yang C, et al. Loading path dependent distortional hardening of Mg alloys: Experimental investigation and constitutive modeling [J]. Int. J. Plast., 2017, 90: 76 |
| [26] | Zhang Z X, Qu S J, Feng A H, et al. Microstructural mechanisms during multidirectional isothermal forging of as-cast Ti-6Al-4V alloy with an initial lamellar microstructure [J]. J. Alloys Compd., 2019, 773: 277 |
| [27] | Hama T, Nagao H, Kobuki A, et al. Work-hardening and twinning behaviors in a commercially pure titanium sheet under various loading paths [J]. Mater. Sci. Eng., 2015, A620: 390 |
| [28] | Wroński M, Kumar M A, McCabe R J, et al. Deformation behavior of CP-titanium under strain path changes: Experiment and crystal plasticity modeling [J]. Int. J. Plast., 2022, 148: 103129 |
| [29] | Hou Y, Lee M G, Lin J P, et al. Experimental characterization and modeling of complex anisotropic hardening in quenching and partitioning (Q&P) steel subject to biaxial non-proportional loadings [J]. Int. J. Plast., 2022, 156: 103347 |
| [30] | Benzerga A A, Surovik D, Keralavarma S M. On the path-dependence of the fracture locus in ductile materials-Analysis [J]. Int. J. Plast., 2012, 37: 157 |
| [31] | Cortese L, Nalli F, Rossi M. A nonlinear model for ductile damage accumulation under multiaxial non-proportional loading conditions [J]. Int. J. Plast., 2016, 85: 77 |
| [32] | Zhang R, Xu Z T, Deng Y J, et al. Characterizing the back stress of ultra-thin metallic sheet via pre-strain tension/bending process [J]. J. Mater. Process. Technol., 2020, 279: 116560 |
| [33] | Fincato R, Tsutsumi S. Numerical modeling of the evolution of ductile damage under proportional and non-proportional loading [J]. Int. J. Solids Struct., 2019, 160: 247 |
| [34] | Itoh T, Yang T. Material dependence of multiaxial low cycle fatigue lives under non-proportional loading [J]. Int. J. Fatigue, 2011, 33: 1025 |
| [35] | Yu J W, Fan X G, Wang L, et al. Mechanism of the high elongation but low formability of high-strength aluminum alloy in W-temper [J]. J. Mater. Process. Technol., 2025, 345: 119068 |
| [36] | Wollenweber M A, Medghalchi S, Guimar?es L R, et al. On the damage behaviour in dual-phase DP800 steel deformed in single and combined strain paths [J]. Mater. Des., 2023, 231: 112016 |
| [37] | Marcadet S J, Mohr D. Effect of compression-tension loading reversal on the strain to fracture of dual phase steel sheets [J]. Int. J. Plast., 2015, 72: 21 |
| [38] | Yu K, Yoon J W. Characterization of compressive fracture strain based on bilinear strain paths [J]. Int. J. Plast., 2024, 183: 104168 |
| [39] | Sanderson S G, Najmabad S I, Sharma R, et al. Observation and modeling of strain gradients in AA6016—Influence of length-scale, microstructure, and strain path [J]. Mater. Charact., 2025, 222: 114843 |
| [40] | Wang Z S, Wang T, Guan Y J, et al. Effect of strain path on microstructure and mechanical properties of AZ31 magnesium alloy sheets processed by constrained groove pressing [J]. Mater. Sci. Eng., 2021, A804: 140794 |
| [41] | Poths R M, Angella G, Wynne B P, et al. Effect of strain reversal on the dynamic spheroidization of Ti-6Al-4V during hot deformation [J]. Metall. Mater. Trans., 2004, 35A: 2993 |
| [42] | Zhao A M, Yang H, Fan X G, et al. The flow behavior and microstructure evolution during (α + β) deformation of β wrought TA15 titanium alloy [J]. Mater. Des., 2016, 109: 112 |
| [43] | Wang L, Fan X G, Zhan M, et al. Experimental characterization and physical modeling of strain path dependent microstructure evolution: A case study of primary hot working of titanium alloy [J]. Int. J. Plast., 2022, 158: 103450 |
| [44] | Huang Z, Luo S, Wang G Y, et al. Mechanistic exploration of high strain-hardening and TWIP effects in Fe-15.5Mn-0.6C-1.4Al steel under compression-tensile loading [J]. Int. J. Plast., 2025, 188: 104292 |
| [45] | Xin Y C, Jiang J, Chapuis A, et al. Plastic deformation behavior of AZ31 magnesium alloy under multiple passes cross compression [J]. Mater. Sci. Eng., 2012, A532: 50 |
| [46] | Yang H, Zhou G W, Wang H M, et al. Experimental and numerical study on strain path and crystal orientation dependences of phase transformation behaviors of QP1180 steel [J]. Int. J. Plast., 2023, 160: 103499 |
| [47] | Sahoo S K, Sabat R K, Sahni S, et al. Texture and microstructure evolution of commercially pure titanium during hot rolling: Role of strain-paths [J]. Mater. Des., 2016, 91: 58 |
| [48] | Gupta A, Khatirkar R K, Dandekar T, et al. Texture development during multi-step cross rolling of a β titanium alloy: Experiments and simulation [J]. J. Alloys Compd., 2021, 850: 156824 |
| [49] | Fan J K, Zhao D, Chen Z S, et al. Tailoring texture in a near-α titanium alloy: Insights from strain paths and cooling rate influences [J]. J. Mater. Res. Technol., 2024, 30: 1388 |
| [50] | Tang L Q, Jiang F L, Teng J, et al. Strain path dependent evolutions of microstructure and texture in AZ80 magnesium alloy during hot deformation [J]. J. Alloys Compd., 2019, 806: 292 |
| [51] | Li Y Y, Han T Z, Chu Z B, et al. Effect of strain path on mechanical behavior of AZ31 magnesium alloy [J]. Rare Met. Mater. Eng., 2022, 51: 2785 |
| [52] | Wu W J, Chen W Z, Wang X Y, et al. Texture adjustment approach of magnesium alloys via variable strain path calculated by an integrated finite element-viscoplastic self-consistent model [J]. J. Mater. Sci. Technol., 2024, 184: 15 |
| [53] | El-Danaf E A. Mechanical properties, microstructure and micro-texture evolution for 1050AA deformed by equal channel angular pressing (ECAP) and post ECAP plane strain compression using two loading schemes [J]. Mater. Des., 2012, 34: 793 |
| [54] | Dhara S, Hughes D J, Huband S, et al. An X-ray diffraction study of the influence of linear and changing strain paths on strain and texture evolution in AA6111-T4 aluminium alloy sheets [J]. Materialia, 2024, 38: 102305 |
| [55] | Zeng X, Fan X G, Li H W, et al. Grain refinement in hot working of 2219 aluminium alloy: On the effect of deformation mode and loading path [J]. Mater. Sci. Eng., 2020, A794: 139905 |
| [56] | Collins D M, Erinosho T, Dunne F P E, et al. A synchrotron X-ray diffraction study of non-proportional strain-path effects [J]. Acta Mater., 2017, 124: 290 |
| [57] | Akbarian S H, Zarei-Hanzaki A, Anoushe A S, et al. Step-by-step texture modification through strain path change toward improvement of the hardening capacity in a twinning-induced-plasticity steel [J]. Mater. Sci. Eng., 2021, A799: 140269 |
| [58] | Shaabani A, Jamaati R, Hosseinipour S J. Effect of strain path and short-term post-annealing on the microstructure, texture, and mechanical anisotropy of low-carbon steel [J]. Mater. Charact., 2024, 215: 114148 |
| [59] | Fan X G, Jiang X Q, Zeng X, et al. Modeling the anisotropy of hot plastic deformation of two-phase titanium alloys with a colony microstructure [J]. Int. J. Plast., 2018, 104: 173 |
| [60] | Chen F, Tian X, Liu Z X, et al. A novel continuous dynamic recrystallization model to reveal grain refinement mechanism in constraining ring rolling of thin-walled conical structure with inner ribs [J]. Int. J. Mach. Tools Manuf., 2025, 206: 104255 |
| [61] | Wei D L, Cui Z S, Chen J. Optimization and tolerance prediction of sheet metal forming process using response surface model [J]. Comput. Mater. Sci., 2008, 42: 228 |
| [62] | Yang H, Tang W Q, Li D Y. Development and verification of crystal plasticity finite element model considering phase transformation [J]. J. Plast. Eng., 2025, 32(4): 169 |
| 杨 浩, 唐伟琴, 李大永. 考虑相变的晶体塑性有限元模型开发及验证 [J]. 塑性工程学报, 2025, 32(4): 169 | |
| [63] | Liu R X, Li K, Zhou G W, et al. Simulation of strain induced abnormal grain growth in aluminum alloy by coupling crystal plasticity and phase field methods [J]. Trans. Nonferrous Met. Soc. China, 2022, 32: 3873 |
| [64] | Barlat F, Brem J C, Yoon J W, et al. Plane stress yield function for aluminum alloy sheets—part 1: Theory [J]. Int. J. Plast., 2003, 19: 1297 |
| [65] | Yoon J W, Barlat F, Dick R E, et al. Plane stress yield function for aluminum alloy sheets-part II: FE formulation and its implementation [J]. Int. J. Plast., 2004, 20: 495 |
| [66] | Deng N X, Kuwabara T, Korkolis Y P. On the non-linear unloading behavior of a biaxially loaded dual-phase steel sheet [J]. Int. J. Mech. Sci., 2018, 138-139: 383 |
| [67] | Hou Y, Min J Y, Guo N, et al. Investigation of evolving yield surfaces of dual-phase steels [J]. J. Mater. Process. Technol., 2021, 287: 116314 |
| [68] | Chaboche J L. Constitutive equations for cyclic plasticity and cyclic viscoplasticity [J]. Int. J. Plast., 1989, 5: 247 |
| [69] | Haddag B, Balan T, Abed-Meraim F. Investigation of advanced strain-path dependent material models for sheet metal forming simulations [J]. Int. J. Plast., 2007, 23: 951 |
| [70] | Barlat F, Ha J J, Grácio J J, et al. Extension of homogeneous anisotropic hardening model to cross-loading with latent effects [J]. Int. J. Plast., 2013, 46: 130 |
| [71] | Yang Y F, Balan T. Prediction of the yield surface evolution and some apparent non-normality effects after abrupt strain-path change using classical plasticity [J]. Int. J. Plast., 2019, 119: 331 |
| [72] | Choi H, Yoon J W. A new simplified distortional hardening model for nonlinear strain paths [J]. Int. J. Plast., 2023, 165: 103617 |
| [73] | Zhang H M, Xu S, Li Q, et al. Progress of crystal plasticity theory and simulations [J]. J. Plast. Eng., 2020, 27(5): 12 |
| 章海明, 徐 帅, 李 倩 等. 晶体塑性理论及模拟研究进展 [J]. 塑性工程学报, 2020, 27(5): 12 | |
| [74] | Zecevic M, Korkolis Y P, Kuwabara T, et al. Dual-phase steel sheets under cyclic tension-compression to large strains: Experiments and crystal plasticity modeling [J]. J. Mech. Phys. Solids, 2016, 96: 65 |
| [75] | Kim H, Barlat F, Lee Y, et al. A crystal plasticity model for describing the anisotropic hardening behavior of steel sheets during strain-path changes [J]. Int. J. Plast., 2018, 111: 85 |
| [76] | Xu Z T, Zhang R, Peng L F, et al. Crystal plasticity-based analysis and modelling of grain size and strain path dependent micro-scaled deformation mechanisms of ultra-thin sheet metals [J]. Int. J. Plast., 2023, 168: 103696 |
| [77] | Iftikhar C M A, Li Y L, Kohar C P, et al. Evolution of subsequent yield surfaces with plastic deformation along proportional and non-proportional loading paths on annealed AA6061 alloy: Experiments and crystal plasticity finite element modeling [J]. Int. J. Plast., 2021, 143: 102956 |
| [78] | Zhou C, Deng J J, Zhang W T, et al. A mixed hardening model for TRIP steel considering strain path change [J]. J. Plast. Eng., 2018, 25(4): 129 |
| 周 驰, 邓军杰, 张文涛 等. 一种考虑应变路径变化的TRIP钢组合硬化模型 [J]. 塑性工程学报, 2018, 25(4): 129 | |
| [79] | Li J Z, Guan Z P, Chen J R, et al. A long short-term memory-based constitutive modeling framework for capturing strain path dependence in plastic deformation [J]. Mech. Mater., 2025, 205: 105325 |
| [80] | Morand L, Helm D. A mixture of experts approach to handle ambiguities in parameter identification problems in material modeling [J]. Comput. Mater. Sci., 2019, 167: 85 |
| [81] | Gorji M B, Mozaffar M, Heidenreich J N, et al. On the potential of recurrent neural networks for modeling path dependent plasticity [J]. J. Mech. Phys. Solids, 2020, 143: 103972 |
| [82] | Zhang A N, Mohr D. Using neural networks to represent von Mises plasticity with isotropic hardening [J]. Int. J. Plast., 2020, 132: 102732 |
| [83] | Jang D P, Fazily P, Yoon J W. Machine learning-based constitutive model for J2- plasticity [J]. Int. J. Plast., 2021, 138: 102919 |
| [84] | Gu B, He J, Li S H, et al. Research progress on anisotropic fracture models and fracture tests for sheet metals [J]. J. Plast. Eng., 2019, 26(1): 1 |
| 顾 彬, 何 霁, 李淑慧 等. 金属板料各向异性断裂模型及断裂实验研究进展 [J]. 塑性工程学报, 2019, 26(1): 1 | |
| [85] | Yoshida K, Kuwabara T, Kuroda M. Path-dependence of the forming limit stresses in a sheet metal [J]. Int. J. Plast., 2007, 23: 361 |
| [86] | Nurcheshmeh M, Green D E. Prediction of sheet forming limits with Marciniak and Kuczynski analysis using combined isotropic-nonlinear kinematic hardening [J]. Int. J. Mech. Sci., 2011, 53: 145 |
| [87] | Fincato R, Tsutsumi S, Momii H, et al. Ductile damage evolution under cyclic non-proportional loading paths [J]. Procedia Struct. Integr., 2018, 9: 136 |
| [88] | Fan R L, Chen M H, Wu D P, et al. Prediction of damage and hot forming limit of TA32 titanium alloy based on crystal plasticity model [J]. Acta Metall. Sin., 2025, 61: 1293 |
| 范荣磊, 陈明和, 吴迪鹏 等. 基于晶体塑性模型预测TA32钛合金损伤及高温成形极限 [J]. 金属学报, 2025, 61: 1293 | |
| [89] | Nguyen N T, Tran M T, Nguyen X M, et al. Physics-guided machine learning for forming-limit assessments of advanced high-strength steels [J]. Int. J. Mech. Sci., 2025, 287: 109959 |
| [90] | Pandya K S, Roth C C, Mohr D. Strain rate and temperature dependent fracture of aluminum alloy 7075: Experiments and neural network modeling [J]. Int. J. Plast., 2020, 135: 102788 |
| [91] | Schowtjak A, Gerlach J, Muhammad W, et al. Prediction of ductile damage evolution based on experimental data using artificial neural networks [J]. Int. J. Solids Struct., 2022, 257: 111950 |
| [92] | Qiao H, Guo X Q, Hong S G, et al. Modeling of {10-12}-{10-12} secondary twinning in pre-compressed Mg alloy AZ31 [J]. J. Alloys Compd., 2017, 725: 96 |
| [93] | Barrett T J, McCabe R J, Brown D W, et al. Predicting deformation behavior of α-uranium during tension, compression, load reversal, rolling, and sheet forming using elasto-plastic, multi-level crystal plasticity coupled with finite elements [J]. J. Mech. Phys. Solids, 2020, 138: 103924 |
| [94] | Upadhyay M V, Capek J, Panzner T, et al. Microstructure evolution of stainless steel subjected to biaxial load path changes: In-situ neutron diffraction and multi-scale modeling [J]. Int. J. Plast., 2019, 122: 49 |
| [95] | Kitayama K, Tomé C N, Rauch E F, et al. A crystallographic dislocation model for describing hardening of polycrystals during strain path changes. Application to low carbon steels [J]. Int. J. Plast., 2013, 46: 54 |
| [96] | Zhang Z, Shen F H, Münstermann S. Crystal plasticity modeling of prior austenite orientation effects on deformation behaviors of martensitic steels under different strain paths [J]. Mater. Des., 2024, 245: 113280 |
| [97] | Ibragimova O, Brahme A, Muhammad W, et al. A new ANN based crystal plasticity model for FCC materials and its application to non-monotonic strain paths [J]. Int. J. Plast., 2021, 144: 103059 |
| [98] | Chen X F, Yu Z Q, Hou B, et al. A theoretical and experimental study on forming limit diagram for a seamed tube hydroforming [J]. J. Mater. Process. Technol., 2011, 211: 2012 |
| [99] | Dhara S, Basak S, Panda S K, et al. Formability analysis of pre-strained AA5754-O sheet metal using Yld96 plasticity theory: Role of amount and direction of uni-axial pre-strain [J]. J. Manuf. Process., 2016, 24: 270 |
| [100] | Leotoing L, Guines D. Investigations of the effect of strain path changes on forming limit curves using an in-plane biaxial tensile test [J]. Int. J. Mech. Sci., 2015, 99: 21 |
| [101] | Schlosser F, Signorelli J, Leonard M, et al. Influence of the strain path changes on the formability of a zinc sheet [J]. J. Mater. Process. Technol., 2019, 271: 101 |
| [102] | Guo J, Zhan M, Yang H. Advances in rolling-spinning technique of titanium tubes [J]. Mater. China, 2016, 35: 275 |
| 郭 靖, 詹 梅, 杨 合. 钛合金筒形件轧-旋成形研究进展 [J]. 中国材料进展, 2016, 35: 275 | |
| [103] | Wang X X, Zhan M, Gao P F, et al. Micromechanical behaviour of TA15 alloy cylindrical parts processed by multi-pass flow forming [J]. Mater. Sci. Eng., 2018, A737: 328 |
| [104] | Yang B, Zhang W G, Lin Z Q. A method to design the loading path for tube hydroforming process [J]. J. Shanghai Jiao Tong Univ., 2006, 40: 893 |
| 杨 兵, 张卫刚, 林忠钦. 一种管件液压成形加载路径的设计方法 [J]. 上海交通大学学报, 2006, 40: 893 | |
| [105] | Teng B G, Li K, Yuan S J. Optimization of loading path in hydroforming T-shape using fuzzy control algorithm [J]. Int. J. Adv. Manuf. Technol., 2013, 69: 1079 |
| [106] | Imaninejad M, Subhash G, Loukus A. Loading path optimization of tube hydroforming process [J]. Int. J. Mach. Tools Manuf., 2005, 45: 1504 |
| [107] | Zhang C, Liu W, Huang L R, et al. Process analysis of biconvex tube hydroforming based on loading path optimization by response surface method [J]. Int. J. Adv. Manuf. Technol., 2021, 112: 2609 |
| [108] | Salandari-Rabori A, Zarei-Hanzaki A, Fatemi S M, et al. Microstructure and superior mechanical properties of a multi-axially forged WE magnesium alloy [J]. J. Alloys Compd., 2017, 693: 406 |
| [109] | Wang L. Study on the high-performance forming mechanism of TB6 titanium alloy shaped charge liner through controllable strain path forging [D]. Xi'an: Northwestern Polytechnical University, 2024 |
| 王 俐. TB6钛合金药型罩可控应变路径锻造高性能成形机理研究 [D]. 西安: 西北工业大学, 2024 | |
| [110] | Fan X G, Wang L, Jiang X Q, et al. Method for pre-treating and matching reversing large deformation refined titanium alloy microstructure [P]. Chin Pat, 202210099026.0, 2022 |
| 樊晓光, 王 俐, 姜雪琦 等. 一种预处理匹配换向大变形细化钛合金微观组织的方法 [P]. 中国专利, 202210099026.0, 2022) | |
| [111] | Chen X H, Yu Z Q, Chen W, et al. Study on generating rolling method for manufacturing cylindrical parts with external cross ribs [J]. J. Manuf. Process., 2024, 111: 1 |
| [112] | Gao L Y, Fan Q B, Xu S, et al. Comparative investigation of deformation mechanisms in Ti-6Mo-3.5Cr-1Zr metastable β titanium alloy subject to cold rolling strain paths [J]. Mater. Sci. Eng., 2025, A941: 148661 |
| [113] | Li W Y, Chen Z Y, Liu J R, et al. Rolling texture and its effect on tensile property of a near-α titanium alloy Ti60 plate [J]. J. Mater. Sci. Technol., 2019, 35: 790 |
| [114] | Rouzbeh A, Sedighi M, Hashemi R. Effects of strain path on the microstructure, tensile properties, and formability of Al/Mg roll-bonded sheets [J]. J. Mater. Res. Technol., 2023, 23: 5318 |
| [115] | Zhang Z M, Li G J, Wang Q, et al. Multi-directional loading rotary extrusion forming technology and equipment [J]. J. Mech. Eng., 2023, 59(12): 264 |
| 张治民, 李国俊, 王 强 等. 多向加载旋转挤压成形技术及装备 [J]. 机械工程学报, 2023, 59(12): 264 | |
| [116] | Mills K, Li H J, Luzin V, et al. Influence of ECAP deformation routes on grain refinement, mechanical properties and texture of zinc [J]. Mater. Sci. Eng., 2025, A945: 149066 |
/
| 〈 |
|
〉 |