综述

先进导电铜基复合材料设计与制备研究进展

  • 姜伊辉 ,
  • 张兴德 ,
  • 石浩 ,
  • 曹飞 ,
  • 马文君 ,
  • 王艳芳 ,
  • 梁淑华
展开
  • 1 西安理工大学 材料科学与工程学院 西安 710048
    2 西安理工大学 导电材料与复合技术教育部工程研究中心 西安 710048
    3 西安理工大学 陕西省电工材料与熔渗技术重点实验室 西安 710048
姜伊辉,男,1985年生,教授,博士
梁淑华,liangsh@xaut.edu.cn,主要从事导电材料成型技术、难熔金属及粉末冶金技术等方面的研究

收稿日期: 2025-02-24

  修回日期: 2025-05-28

  网络出版日期: 2025-06-20

基金资助

国家自然科学基金项目(52322409);国家自然科学基金项目(52127802);国家自然科学基金项目(52271137)

Research Progress in the Design and Preparation of Advanced Conductive Copper Matrix Composites

  • JIANG Yihui ,
  • ZHANG Xingde ,
  • SHI Hao ,
  • CAO Fei ,
  • MA Wenjun ,
  • WANG Yanfang ,
  • LIANG Shuhua
Expand
  • 1 School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
    2 Engineering Research Center of Conducting Materials and Composite Technology, Ministry of Education, Xi'an University of Technology, Xi'an 710048, China
    3 Shaanxi Province Key Laboratory of Electrical Materials and Infiltration Technology, Xi'an University of Technology, Xi'an 710048, China
LIANG Shuhua, professor, Tel: (029)82312185, E-mail: liangsh@xaut.edu.cn

Received date: 2025-02-24

  Revised date: 2025-05-28

  Online published: 2025-06-20

Supported by

National Natural Science Foundation of China(52322409);National Natural Science Foundation of China(52127802);National Natural Science Foundation of China(52271137)

摘要

铜基复合材料具有高强度、高导电、高导热、耐高温、耐磨、耐电弧烧蚀等优良性能,有望成为未来苛刻服役环境下的关键基础导电材料之一。本文对导电型铜基复合材料的典型材料体系、主要制备技术以及组织性能等进行了归纳和总结,分析了原位制备方法的基本原理和特点,阐述了多种类型高强高导铜基复合材料组织特征与综合性能的关系规律,并展望了未来研究所面临的问题及挑战。

本文引用格式

姜伊辉 , 张兴德 , 石浩 , 曹飞 , 马文君 , 王艳芳 , 梁淑华 . 先进导电铜基复合材料设计与制备研究进展[J]. 金属学报, 2026 , 62(2) : 289 -308 . DOI: 10.11900/0412.1961.2025.00047

Abstract

Copper matrix composites are expected to be essential conductive materials for harsh service environments in the future, due to their remarkable properties, including high strength, excellent electrical and thermal conductivity, and their resistance to high temperatures, wear, and arc ablation. This paper summarizes the typical materials, primary preparation techniques, microstructures, and properties of conductive copper matrix composites. It further analyzes the basic principles and characteristics of in situ preparation methods. Finally, the relationship between microstructures and the overall properties of various high-strength and high-conductivity copper matrix composites is discussed, and the problems and challenges that future research may face are considered.

参考文献

[1] Xiao Z, Ding Y J, Wang Z J, et al. Research and development of advanced copper matrix composites [J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 3789
[2] Zhang X H, Zhang Y, Tian B H, et al. Review of nano-phase effects in high strength and conductivity copper alloys [J]. Nanotechnol. Rev., 2019, 8: 383
[3] Zhang X H, Li X X, Chen H, et al. Investigation on microstructure and properties of Cu-Al2O3 composites fabricated by a novel in-situ reactive synthesis [J]. Mater. Des., 2016, 92: 58
[4] Minneci R P, Lass E A, Bunn J R, et al. Copper-based alloys for structural high-heat-flux applications: A review of development, properties, and performance of Cu-rich Cu-Cr-Nb alloys [J]. Int. Mater. Rev., 2021, 66: 394
[5] Chen M X, Li X P, Ji G, et al. Novel composite powders with uniform TiB2 nano-particle distribution for 3D printing [J]. Appl. Sci., 2017, 7: 250
[6] Kini A R, Maischner D, Weisheit A, et al. In-situ synthesis via laser metal deposition of a lean Cu-3.4Cr-0.6Nb (at%) conductive alloy hardened by Cr nano-scale precipitates and by Laves phase micro-particles [J]. Acta Mater., 2020, 197: 330
[7] Zhang Z, Chen D L. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: A model for predicting their yield strength [J]. Scr. Mater., 2006, 54: 1321
[8] Zhou M Y, Ren L B, Fan L L, et al. Progress in research on hybrid metal matrix composites [J]. J. Alloys Compd., 2020, 838: 155274
[9] Guo Q, Li Z Q, Zhao L, et al. Metal matrix composites with microstructural architectures [J]. Mater. China, 2016, 35: 641
  郭 强, 李志强, 赵 蕾 等. 金属材料的构型复合化 [J]. 中国材料进展, 2016, 35: 641
[10] Zou C, Kang H, Li R, et al. The effect of rotating magnetic field on the microstructure of in situ TiB2/Cu composites [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2016, 117: 012043
[11] Arunachalam R, Krishnan P K, Muraliraja R. A review on the production of metal matrix composites through stir casting—Furnace design, properties, challenges, and research opportunities [J]. J. Manuf. Processes, 2019, 42: 213
[12] Wang T M, Zou C L, Chen Z N, et al. In situ synthesis of TiB2 particulate reinforced copper matrix composite with a rotating magnetic field [J]. Mater. Des., 2015, 65: 280
[13] Feng J, Liang S H, Song K X, et al. Micro-nano dual-scale particle-reinforced TiB2/Cu-0.5Cr composites prepared by vacuum arc melting [J]. J. Mater. Eng. Perform., 2020, 29: 3353
[14] Pan S H, Zheng T Q, Yao G C, et al. High-strength and high-conductivity in situ Cu-TiB2 nanocomposites [J]. Mater. Sci. Eng., 2022, A831: 141952
[15] Guo M X, Shen K, Wang M P. Effect of in situ reaction conditions on the microstructure changes of Cu-TiB2 alloys by combining in situ reaction and rapid solidification [J]. Mater. Chem. Phys., 2012, 131: 589
[16] Lee A K, Sanchez-Caldera L E, Chun J H, et al. Material with novel compositions and fine Microstructljres produced via the mixalloy process [J]. MRS Online Proc. Libr., 1988, 132: 87
[17] Guo M X, Shen K, Wang M P. Relationship between microstructure, properties and reaction conditions for Cu-TiB2 alloys prepared by in situ reaction [J]. Acta Mater., 2009, 57: 4568
[18] Liang S H, Li W Z, Jiang Y H, et al. Microstructures and properties of hybrid copper matrix composites reinforced by TiB whiskers and TiB2 particles [J]. J. Alloys Compd., 2019, 797: 589
[19] Cao F, Zhang X D, Jiang Y H, et al. Effect of different rare earths on microstructures and tensile strength of in situ hybrid reinforced (TiB2p + TiBw)/Cu composites [J]. Mater. Charact., 2022, 184: 111624
[20] Lee J, Kim N J, Jung J Y, et al. The influence of reinforced particle fracture on strengthening of spray formed Cu-TiB2 composite [J]. Scr. Mater., 1998, 39: 1063
[21] Lee J, Jung J Y, Lee E S, et al. Microstructure and properties of titanium boride dispersed Cu alloys fabricated by spray forming [J]. Mater. Sci. Eng., 2000, A277: 274
[22] Chen D, Jiang Y H, Li Y F, et al. In situ TiB2/Cu composites fabricated by spray deposition using solid-liquid and liquid-liquid reactions [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1849
[23] Tu J P, Wang N Y, Yang Y Z, et al. Preparation and properties of TiB2 nanoparticle reinforced copper matrix composites by in situ processing [J]. Mater. Lett., 2002, 52: 448
[24] Zheng R G, Zhan Z J, Wang W K. Wear behavior of Cu-La2O3 composite with or without electrical current [J]. Wear, 2010, 268: 72
[25] Jeyaprakash N, Saravana Kumar M, Yang C H. Enhanced nano-level mechanical responses on additively manufactured Cu-Cr-Zr copper alloy containing Cu2O nano precipitates [J]. J. Alloys Compd., 2023, 930: 167425
[26] Liu Y G, Zhang J Q, Sun Q, et al. Laser powder bed fusion of copper matrix iron particle reinforced nanocomposite with high strength and high conductivity [J]. J. Mater. Sci. Technol., 2023, 134: 50
[27] Liu Y A, Zhang J Q, Niu R M, et al. Manufacturing of high strength and high conductivity copper with laser powder bed fusion [J]. Nat. Commun., 2024, 15: 1283
[28] Wang G, Ouyang H, Fan C, et al. The origin of high-density dislocations in additively manufactured metals [J]. Mater. Res. Lett., 2020, 8(8): 283
[29] Sta?i? J, Bo?i? D. Obtaining of reinforced Cu-Ti, Cu-Ti-TiB2 foils through green compact laser sintering [J]. J. Alloys Compd., 2018, 762: 231
[30] Tang X P, Chen X H, Sun F J, et al. The current state of CuCrZr and CuCrNb alloys manufactured by additive manufacturing: A review [J]. Mater. Des., 2022, 224: 111419
[31] Teasley T, Gradl P, Garcia M B, et al. Extreme environment hot fire durability of post processed additively manufactured GRCop-alloy combustion chambers [A]. Proceedings of the AIAA Propulsion and Energy 2021 Forum [C]. AIAA (August 9-11, 2021, Virtual Event), 2021: 3233
[32] Seltzman A H, Wukitch S J. Fracture characteristics and heat treatment of laser powder bed fusion additively manufactured GRCop-84 copper [J]. Mater. Sci. Eng., 2021, A827: 141690
[33] Wang L Q, Qu S, Fu H L, et al. Additively manufactured copper alloy with heterogeneous nanoprecipitates-dislocation architecture for superior strength-ductility-conductivity synergy [J]. Addit. Manuf., 2024, 84: 104100
[34] Cao F, Dong G Z, Jiang Y H, et al. Effect of La addition on microstructures and properties of TiB2(-TiB)/Cu hybrid composites prepared by in situ reaction [J]. Mater. Sci. Eng., 2020, A789: 139605
[35] Zhang S R, Kang H J, Li R G, et al. Microstructure evolution, electrical conductivity and mechanical properties of dual-scale Cu5Zr/ZrB2 particulate reinforced copper matrix composites [J]. Mater. Sci. Eng., 2019, A762: 138108
[36] Zou C L, Kang H J, Wang W, et al. Effect of La addition on the particle characteristics, mechanical and electrical properties of in situ Cu-TiB2 composites [J]. J. Alloys Compd., 2016, 687: 312
[37] Zhai Q M, Xu W Q, Wang J H, et al. Study status of in-situ reaction copper matrix composite [J]. Mater. Heat Treat., 2006, 35(14): 58
  翟启明, 徐文清, 王冀恒 等. 原位反应铜基复合材料的研究现状 [J]. 热加工工艺, 2006, 35(14): 58
[38] Guo M X, Wang M P, Li Z, et al. The studies of TiB2/Cu metal matrix composites [J]. Mater. Rep., 2004, 18(8): 39
  郭明星, 汪明朴, 李 周 等. TiB2/Cu金属基复合材料的研究 [J]. 材料导报, 2004, 18(8): 39
[39] Yan Y F, Kou S Q, Yang H Y, et al. Ceramic particles reinforced copper matrix composites manufactured by advanced powder metallurgy: preparation, performance, and mechanisms [J]. Int. J. Extrem. Manuf., 2023, 5: 032006
[40] Saheb N, Iqbal Z, Khalil A, et al. Spark plasma sintering of metals and metal matrix nanocomposites: A review [J]. J. Nanomater., 2012, 2012: 983470
[41] Jiang X S, Liu W X, Li Y J, et al. Microstructures and mechanical properties of Cu/Ti3SiC2/C/graphene nanocomposites prepared by vacuum hot-pressing sintering and hot isostatic pressing [J]. Composites, 2018, 141B: 203
[42] Tian B H, Liu P, Song K X, et al. Microstructure and properties at elevated temperature of a nano-Al2O3 particles dispersion-strengthened copper base composite [J]. Mater. Sci. Eng., 2006, A435-436: 705
[43] Zhuo H O, Tang J C, Ye N. A novel approach for strengthening Cu-Y2O3 composites by in situ reaction at liquidus temperature [J]. Mater. Sci. Eng., 2013, A584: 1
[44] Xiang Z Q, Li Z, Lei Q, et al. High temperature mechanical behavior of alumina dispersion strengthened copper alloy with high content of alumina [J]. Trans. Nonferrous Met. Soc. China, 2015, 25: 444
[45] Lan T, Jiang Y H, Zhang X J, et al. Competitive precipitation behavior of hybrid reinforcements in copper matrix composites fabricated by powder metallurgy [J]. Int. J. Miner. Metall. Mater., 2021, 28: 1090
[46] Jiang Y H, Wang C, Liang S H, et al. TiB2(-TiB)/Cu in-situ composites prepared by hot-press with the sintering temperature just beneath the melting point of copper [J]. Mater. Charact., 2016, 121: 76
[47] Guo X F, Jia L, Lu Z L, et al. Preparation of Cu/CrB2 composites with well-balanced mechanical properties and electrical conductivity by ex-situ powder metallurgy [J]. J. Mater. Res. Technol., 2022, 17: 1605
[48] Jiang Y H, Shi Y Y, Zhang X J, et al. Copper matrix composite with bimodal microstructures fabricated by liquid nitrogen temperature rolling [J]. Mater. Sci. Technol., 2022, 38: 654
[49] Zhang X K, Lei Q, Liu B, et al. Enhanced softening resistance and mechanical properties of Mo2C particle-reinforced Cu-matrix composites [J]. Compos. Struct., 2023, 305: 116503
[50] Ren J Q, Liang S H, Jiang Y H, et al. Research on the microstructure and properties of in situ (TiB2-TiB)/Cu composites [J]. Acta Metall. Sin., 2019, 55: 126
  任建强, 梁淑华, 姜伊辉 等. 原位(TiB2-TiB)/Cu复合材料组织与性能研究 [J]. 金属学报, 2019, 55: 126
[51] Huang F, Wang H, Yang B, et al. Uniformly dispersed Y2O3 nanoparticles in nanocrystalline copper matrix via multi-step ball milling and reduction process [J]. Mater. Lett., 2019, 242: 119
[52] Guo M X, Wang M P. The relationship among microstructure evolution, mechanical property and in situ reaction mechanisms in preparing Cu-1.6wt% TiB2 alloys [J]. Mater. Chem. Phys., 2013, 138: 95
[53] Li T J, Wang Y Q, Yang M, et al. High strength and conductivity copper matrix composites reinforced by in-situ graphene through severe plastic deformation processes [J]. J. Alloys Compd., 2021, 851: 156703
[54] Wei X, Tao J M, Hu Y, et al. Enhancement of mechanical properties and conductivity in carbon nanotubes (CNTs)/Cu matrix composite by surface and intratube decoration of CNTs [J]. Mater. Sci. Eng., 2021, A816: 141248
[55] Zhao N Q, Guo S Y, Zhang X, et al. Progress on graphene/copper composites focusing on reinforcement configuration design: A review [J]. Acta Metall. Sin., 2021, 57: 1087
  赵乃勤, 郭斯源, 张 翔 等. 基于增强相构型设计的石墨烯/Cu复合材料研究进展 [J]. 金属学报, 2021, 57: 1087
[56] Chen Y K, Zhang X, Liu E Z, et al. Fabrication of three-dimensional graphene/Cu composite by in-situ CVD and its strengthening mechanism [J]. J. Alloys Compd., 2016, 688: 69
[57] Zhang X, Zhao N Q, He C N. The superior mechanical and physical properties of nanocarbon reinforced bulk composites achieved by architecture design—A review [J]. Prog. Mater Sci., 2020, 113: 100672
[58] Jiang L, Li Z Q, Fan G L, et al. The use of flake powder metallurgy to produce carbon nanotube (CNT)/aluminum composites with a homogenous CNT distribution [J]. Carbon, 2012, 50: 1993
[59] Li Z, Wang H T, Guo Q, et al. Regain strain-hardening in high-strength metals by nanofiller incorporation at grain boundaries [J]. Nano Lett., 2018, 18(10): 6255
[60] Shukla A K, Samuel M G, Suresh Kumar R, et al. Effect of powder oxidation on densification and properties of vacuum hot pressed Cu-Cr-Nb alloy [J]. Mater. Sci. Eng., 2013, A561: 452
[61] Shi H, Cao F, Wang T L, et al. A well-balanced strength and electrical conductivity in rolled composite prepared by in-situ TiB2p/Cu composite powder [J]. J. Mater. Res. Technol., 2023, 27: 1
[62] Shi H, Zhao Y, Gao H B, et al. In-situ spherical TiB2/Cu composite powder: A new method of liquid phase reaction coupled with gas atomization [J]. Mater. Charact., 2022, 191: 112096
[63] Shi H, Cao F, Zhang H D, et al. Densification behavior, mechanical and electrical properties of in-situ TiB2p/Cu composite powder via vacuum hot pressing [J]. Mater. Charact., 2023, 202: 113004
[64] Wang L, Zheng C, Kombaiah B, et al. Contrasting roles of Laves_Cr2Nb precipitates on the creep properties of novel CuCr-NbZr alloys [J]. Mater. Sci. Eng., 2020, A779: 139110
[65] Lv X Q, Liu Z M, Lei T, et al. Effect of heat treatment on Cr2Nb phase and properties of spark plasma sintered Cu-2Cr-1Nb alloy [J]. Materials, 2020, 13: 2860
[66] Cao F, Zhang X D, Cai P T, et al. Effect of reaction temperature and heat treatment time on electrical and mechanical performance of TiB2 particles and TiB whiskers reinforced copper matrix composites [J]. Metals, 2022, 12: 592
[67] Zai X F, Chen S Q, Wu H, et al. Preparation of spherical high-purity Zr powders by gas atomization without crucible [J]. Chin. J. Rare Met., 2018, 42: 864
  宰雄飞, 陈仕奇, 吴 宏 等. 无坩埚熔炼气雾化技术制备高纯球形锆粉 [J]. 稀有金属, 2018, 42: 864
[68] Fu J W, Nie Q Q, Qiu W X, et al. Morphology, orientation relationships and formation mechanism of TiN in Fe-17Cr steel during solidification [J]. Mater. Charact., 2017, 133: 176
[69] Bahador A, Umeda J, Yamanoglu R, et al. Deformation mechanism and enhanced properties of Cu-TiB2 composites evaluated by the in-situ tensile test and microstructure characterization [J]. J. Alloys Compd., 2020, 847: 156555
[70] Chen Z, Qiu M L, Yang J J, et al. Thermal stability and grain growth kinetics of ultrafine-grained W with various amount of La2O3 addition [J]. Metall. Mater. Trans., 2020, 51A: 4113
[71] Pan S H, Guan Z Y, Yao G C, et al. Study on electrical behaviour of copper and its alloys containing dispersed nanoparticles [J]. Curr. Appl. Phys., 2019, 19: 452
[72] Zou C L, Chen Z N, Guo E Y, et al. A nano-micro dual-scale particulate-reinforced copper matrix composite with high strength, high electrical conductivity and superior wear resistance [J]. RSC Adv., 2018, 8: 30777
[73] Jin B, Chen G Y, He Y Y, et al. Lubrication properties of graphene under harsh working conditions [J]. Mater. Today Adv., 2023, 18: 100369
[74] Zhang S R, Kang H J, Wang Z C, et al. Microstructure and properties of dual-scale particulate reinforced copper matrix composites with superior comprehensive properties [J]. J. Alloys Compd., 2021, 860: 157888
[75] Jin B, Zhao J, He Y Y, et al. High-quality ultra-flat reduced graphene oxide nanosheets with super-robust lubrication performances [J]. Chem. Eng. J., 2022, 438: 135620
[76] Luan T Y, Gao T C, Zhao J M, et al. Properties and microstructure characterisation of high-strength, high-conductivity and high-resistance to arc ablation Cu-0.6Te-0.3Cr-0.15Zr-0.008P alloy [J]. Mater. Charact., 2024, 214: 114110
[77] Dong L L, Li L, Li X, et al. Enhancing mechanisms of arc-erosion resistance for copper tungsten electrical contact using reduced graphene oxides in situ modified by copper nanoparticles [J]. Int. J. Refract. Met. Hard Mater., 2022, 108: 105934
[78] Fu Q Q, Li B, Gao M Q, et al. Quantitative mechanisms behind the high strength and electrical conductivity of Cu-Te alloy manufactured by continuous extrusion [J]. J. Mater. Sci. Technol., 2022, 121: 9
[79] Li S L, Guo X H, Zhang S L, et al. Arc erosion behavior of TiB2/Cu composites with single-scale and dual-scale TiB2 particles [J]. Nanotechnol. Rev., 2019, 8: 619
[80] Feng J, Liang S H, Guo X H, et al. Electrical conductivity anisotropy of copper matrix composites reinforced with SiC whiskers [J]. Nanotechnol. Rev., 2019, 8: 285
[81] Liu J B, Zeng Y W, Meng L. Crystal structure and morphology of a rare-earth compound in Cu-12wt.% Ag [J]. J. Alloys Compd., 2009, 468: 73
[82] Li J, Liu B, Fang Q H, et al. Atomic-scale strengthening mechanism of dislocation-obstacle interaction in silicon carbide particle-reinforced copper matrix nanocomposites [J]. Ceram. Int., 2017, 43: 3839
[83] Liu N, Zhang Q Q, Zhang H Y, et al. Experimental verification and numerical analysis on plastic deformation and mechanical properties of the in-situ TiB2 homogeneous composites and TiB2/Cu network composites prepared by powder metallurgy [J]. J. Alloys Compd., 2022, 920: 165897
[84] Zhang X X, Yuan Y L, Zhao S Q, et al. Microstructure stability, softening temperature and strengthening mechanism of pure copper, CuCrZr and Cu-Al2O3 up to 1000 oC [J]. Nucl. Mater. Energy, 2022, 30: 101123
[85] Li Z, Zhang D. The self-stimulation effect for high-performance metal matrix composites [J]. Mater. China, 2023, 42: 605
  李 赞, 张 荻. 金属基复合材料的内源性效应 [J]. 中国材料进展, 2023, 42: 605
[86] Ke J G, Liu R, Xie Z M, et al. Ultrahigh strength, thermal stability and high thermal conductivity in hierarchical nanostructured Cu-W alloy [J]. Acta Mater., 2024, 264: 119547
[87] Li N Y, Chang Y Q, Li M Y, et al. Enhanced mechanical property by introducing bimodal grains structures in Cu-Ta alloys fabricated by mechanical alloying [J]. J. Mater. Sci. Technol., 2024, 172: 104
[88] Zhang X H, Xiong D B, Liu Y Z, et al. Multilayer graphene interface enabled ultrahigh extensibility for high performance bulk nanostructured copper [J]. Acta Mater., 2024, 267: 119710
[89] Cao F, Zhang X D, Dong G Z, et al. Microstructures and properties of in situ (TiB2p + TiBw)/Cu composites with different Ce content [J]. Adv. Eng. Mater., 2022, 24: 2200251
[90] Zhou D S, Wang X K, Zeng W, et al. Doping Ti to achieve microstructural refinement and strength enhancement in a high volume fraction Y2O3 dispersion strengthened Cu [J]. J. Alloys Compd., 2018, 753: 18
[91] Jia Y L, Zhou K, Sun W T, et al. Enhancement mechanisms of mechanical, electrical and thermal properties of carbon nanotube-copper composites: A review [J]. J. Mater. Res. Technol., 2024, 32: 1395
[92] Zeng W, Xie J W, Zhou D S, et al. Bulk Cu-NbC nanocomposites with high strength and high electrical conductivity [J]. J. Alloys Compd., 2018, 745: 55
[93] Xie J W, Zeng W, Zhou D S, et al. Microstructure and properties of a nanocrystalline Cu-Al-NbC composite with high strength and good conductivity [J]. Mater. Lett., 2018, 214: 174
[94] Cao J M, Li F J, Yang Q C, et al. A review on interfacial structure optimization and its mechanism on the properties of carbon reinforced metal-matrix composites [J]. Compos. Interfaces, 2023, 30(5): 543
[95] Pan Y, Xiao S Q, Lu X, et al. Fabrication, mechanical properties and electrical conductivity of Al2O3 reinforced Cu/CNTs composites [J]. J. Alloys Compd., 2019, 782: 1015
[96] Zhang X D, Jiang Y H, Cao F, et al. Hybrid effect on mechanical properties and high-temperature performance of copper matrix composite reinforced with micro-nano dual-scale particles [J]. J. Mater. Sci. Technol., 2024, 172: 94
[97] Zhou T, Chen W, Jiang Y B, et al. Microstructure, properties and reaction kinetics of a Cu-Al2O3-TiB2 alloy prepared by a new liquid phase in-situ reaction technology [J]. J. Mater. Res. Technol., 2023, 26: 4024
[98] Long F, Guo X H, Song K X, et al. An internal-oxidation-based strategy induced high-density alumina in-situ nanoprecipitation and carbon nanotube interface optimization for co-reinforcing copper matrix composites [J]. Composites, 2022, 229B: 109455
[99] Xu K, Chen X H, Zhou H L, et al. Preparation and formation mechanism of CNTs/Cu-Al2O3 composite powders by in situ CVD using internally-oxidized Cu-Al alloy powders [J]. Mater. Lett., 2019, 254(1): 390
[100] Nageswaran G, Natarajan S, Ramkumar K R. Synthesis, structural characterization, mechanical and wear behaviour of Cu-TiO2-Gr hybrid composite through stir casting technique [J]. J. Alloys Compd., 2018, 768: 733
[101] Fan G L, Guo Z Q, Tan Z Q, et al. Architecture design strategies and strengthening-toughening mechanisms of metal matrix composites [J]. Acta Metall. Sin., 2022, 58: 1416
  范根莲, 郭峙岐, 谭占秋 等. 金属材料的构型化复合与强韧化 [J]. 金属学报, 2022, 58: 1416
[102] Wegst U G K, Bai H, Saiz E, et al. Bioinspired structural material [J]. Nat. Mater., 2015, 14: 23
[103] Zhao L, Zheng W S, Hu Y, et al. Heterostructured metal matrix composites for structural applications: A review [J]. J. Mater. Sci., 2024, 59: 9768
[104] Cao M, Xiong D B, Yang L, et al. Ultrahigh electrical conductivity of graphene embedded in metals [J]. Adv. Funct. Mater., 2019, 29: 1806792
[105] Han F, Jiang Y H, Cao F, et al. Role of gradient heterogeneous interfaces in synergetic strengthening and toughening of layered CuCrZr/Cu composites [J]. Mater. Sci. Eng., 2023, A885: 145613
[106] Cao F, Cai L, Han F, et al. Effects of the layer thickness ratio on the microstructure and mechanical properties of Cu-TiB2/Cu layered composites [J]. Foundry Technol., 2024, 45: 61
  曹 飞, 蔡 磊, 韩 非 等. 层厚比对Cu-TiB2/Cu层状复合材料微观组织和力学性能的影响 [J]. 铸造技术, 2024, 45: 61
[107] Xiong D B, Cao M, Guo Q, et al. Graphene-and-copper artificial nacre fabricated by a preform impregnation process: Bioinspired strategy for strengthening-toughening of metal matrix composite [J]. ACS Nano, 2015, 9: 6934
[108] Yang Z Y, Wang L D, Cui Y, et al. High strength and ductility of graphene-like carbon nanosheet/copper composites fabricated directly from commercial oleic acid coated copper powders [J]. Nanoscale, 2018, 10: 16990
[109] Zhang X, Shi C S, Liu E Z, et al. Achieving high strength and high ductility in metal matrix composites reinforced with a discontinuous three-dimensional graphene-like network [J]. Nanoscale, 2017, 9: 11929
[110] Jiang Y H, Han L, Xu Y Q, et al. Arc erosion behaviour of in-situ TiB2/Cu composites with a three-dimensional network structure [J]. Mater. Res. Express, 2022, 9: 046503
文章导航

/