研究论文

Zn-Pb偏晶合金微量界面活性元素选取

  • 杨林洁 ,
  • 张丽丽 ,
  • 赵九洲 ,
  • 江鸿翔 ,
  • 何杰
展开
  • 1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016
    2.中国科学技术大学 材料科学与工程学院 沈阳 110016
杨林洁,男,1997年生,博士生
张丽丽,llzhang@imr.ac.cn,主要从事合金凝固过程及组织调控研究;
赵九洲,jzzhao@imr.ac.cn,主要从事合金凝固理论及新材料研究

收稿日期: 2024-04-08

  修回日期: 2024-07-20

  网络出版日期: 2025-02-20

基金资助

国家重点研发计划项目(2021YFA0716303);中国载人空间站项目(KJZ-YY-NCL-1-02);中国载人空间站项目(KJZ-YY-NCL-1-06);辽宁省自然科学基金项目(2023-MS-023)

Selection of Trace Interface Active Element for Zn-Pb Monotectic Alloy

  • YANG Linjie ,
  • ZHANG Lili ,
  • ZHAO Jiuzhou ,
  • JIANG Hongxiang ,
  • HE Jie
Expand
  • 1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
ZHANG Lili, associate professor, Tel: (024)23971905, E-mail: llzhang@imr.ac.cn;
ZHAO Jiuzhou, professor, Tel: (024)23971918, E-mail: jzzhao@imr.ac.cn

Received date: 2024-04-08

  Revised date: 2024-07-20

  Online published: 2025-02-20

Supported by

National Key Research and Development Program of China(2021YFA0716303);China Manned Space Station Project(KJZ-YY-NCL-1-02);China Manned Space Station Project(KJZ-YY-NCL-1-06);Natural Science Foundation of Liaoning Province(2023-MS-023)

摘要

为了选取有效的Zn-Pb偏晶合金微量界面活性元素,调控Zn-Pb合金液-液相变过程,促进Zn-Pb合金形成弥散型凝固组织,本工作通过实验和理论计算研究了微量元素对Zn-4.0%Pb (质量分数)偏晶合金凝固组织的影响。实验结果表明,微量元素Sn、In能够显著细化凝固组织中的富Pb相粒子,而微量元素Cu、Bi对富Pb相粒子尺寸影响较小。建立了描述Zn-Pb合金液-液相变过程中微量元素在Zn基体与富Pb液滴间液/液界面处偏析行为的理论模型,计算并分析了微量元素在液/液界面处的偏析行为。计算结果表明,微量元素Cu、Bi不能作为Zn-Pb合金的界面活性元素,而微量元素Sn、In倾向于在液/液界面处富集,可作为Zn-Pb合金的界面活性元素。微量元素的偏析行为取决于各组元间的相互作用,仅当其与Zn原子和Pb原子间相互作用(吸引或排斥)均较弱时才可作为界面活性元素。

本文引用格式

杨林洁 , 张丽丽 , 赵九洲 , 江鸿翔 , 何杰 . Zn-Pb偏晶合金微量界面活性元素选取[J]. 金属学报, 2026 , 62(3) : 532 -540 . DOI: 10.11900/0412.1961.2024.00101

Abstract

Zn-Pb alloy is an excellent electrochemical material, provided that Pb-rich particles are well dispersed within the Zn-based matrix. When used as the anode in Zn-MnO2 batteries, the Zn-Pb alloy effectively inhibits hydrogen evolution corrosion, enhances cycling stability, and improves Coulombic efficiency, thus significantly increasing the battery's durability. However, Zn-Pb alloy is a typical monotectic alloy, characterized by liquid-liquid phase transformation during solidification. In this transformation, a homogeneous monotectic alloy melt separates into two liquid phases, resulting in a phase-segregated microstructure that limits the alloy's application. Extensive research has been conducted on the solidification of monotectic alloys. The use of external fields such as ultrasound, electric fields, magnetic fields, and composite electric-magnetic fields to control the solidification structure has been explored. Studies have also investigated the impact of nucleating agents on the solidification process and microstructure. In addition, alloying with a third element to control the solidification process has proven effective. Results indicate that the microstructure evolution during the liquid-liquid phase transition involves complex kinetic behaviors, including nucleation, growth, Ostwald ripening, motion, collision-coagulation of minority phase droplets, and their interaction with the solidification front. The nucleation and migration of minority phase droplets have a dominant influence on the solidification microstructure of monotectic alloys. Adding interface active elements to the alloy melt reduces the liquid/liquid interfacial energy, increasing the nucleation rate and reducing the Marangoni migration velocity of minority phase droplets. This promotes the formation of a well-dispersed microstructure in Zn-Pb alloys. According to the Gibbs isothermal adsorption equation, an element can act as an interface active element if it segregates at the interface between the two liquid phases at the onset of the liquid-liquid phase transition. In this study, solidification experiments were conducted with Zn-4.0%Pb (mass fraction) alloy micro-alloyed with different trace elements to evaluate their effects on the liquid-liquid phase transition. The results indicate that trace elements Sn and In significantly refine Pb-rich particles, while the effects of Cu and Bi are negligible. An analytical model was developed to calculate the segregation behavior of trace elements at the Zn-rich liquid/Pb-rich liquid interface in the Zn-Pb alloy. Calculations reveal that Sn and In segregate to the liquid/liquid interface and act as interface active elements, facilitating effective refinement of Pb-rich particles. In contrast, Cu and Bi cannot act as interface active elements. The segregation behavior of trace elements is closely related to their interactions with Zn and Pb; trace elements can only act as interface active elements if they exhibit weak attraction or repulsion toward both Zn and Pb.

参考文献

[1] Ratke L, Diefenbach S. Liquid immiscible alloys [J]. Mater. Sci. Eng., 1995, R15: 263
[2] Zhao J Z, Jiang H X. Progress in the solidification of monotectic alloys [J]. Acta Metall. Sin., 2018, 54: 682
  赵九洲, 江鸿翔. 偏晶合金凝固过程研究进展 [J]. 金属学报, 2018, 54: 682
[3] Ruan P C, Chen X H, Qin L P, et al. Achieving highly proton-resistant Zn-Pb anode through low hydrogen affinity and strong bonding for long-life electrolytic Zn//MnO2 battery [J]. Adv. Mater., 2023, 35: 2300577
[4] Dong B W, Jie J C, Dong Z Z, et al. Novel insight into mechanism of secondary phase's morphology evolution in hypomonotectic Cu-Pb-Sn alloy during solidification [J]. J. Mol. Liq., 2019, 292: 111336
[5] Lu W Q, Zhang S G, Li J G. Segregation driven by collision and coagulation of minor droplets in Al-Bi immiscible alloys under aerodynamic levitation condition [J]. Mater. Lett., 2013, 107: 340
[6] Wu W H, Wang D Z, Zhai W, et al. Multiple ultrasounds assisted phase separation and monotectic solidification of liquid ternary Al81.5Cu14.7Bi3.8 immiscible alloy [J]. J. Appl. Phys., 2023, 133: 115102
[7] Zhu J, Wang T M, Cao F, et al. Real-time observation on evolution of droplets morphology affected by electric current pulse in Al-Bi immiscible alloy [J]. J. Mater. Eng. Perform., 2013, 22: 1319
[8] Zhou B F, Lin W H, Liu Y, et al. Effects of high static magnetic field on the microstructure of Zn-Bi monotectic alloys during directional solidification process [J]. J. Alloys Compd., 2021, 889: 161670
[9] Li Y Q, Jiang H X, Sun H, et al. Microstructure evolution of immiscible alloy solidified under the effect of composite electric and magnetic fields [J]. J. Mater. Sci. Technol., 2023, 162: 247
[10] Man T N, Zhang L, Xu N K, et al. Effect of rare-earth Ce on macrosegregation in Al-Bi immiscible alloys [J]. Metals, 2016, 6: 177
[11] Yang Q, Sun Z P, Wang Z M. Effects of Sn, Si, and Cu addition on the microstructure and properties of hypermonotectic Al92Bi8 alloy [J]. Mater. Sci. Eng., 2019, A756: 71
[12] Sun Q, Jiang H X, Zhao J Z, et al. Microstructure evolution during the liquid-liquid phase transformation of Al-Bi alloys under the effect of TiC particles [J]. Acta Mater., 2017, 129: 321
[13] Xie M, Zhang Y Z, Li X, et al. Effect of Si element and TiB2 nucleating agent on microstructure and magnetic properties of Cu-based immiscible composites by laser melting deposition [J]. J. Alloys Compd., 2023, 934: 167938
[14] Zhao J Z, Sun H, Zhang L L, et al. In-situ composite microstructure formation of immiscible alloy solidified in space [J]. Natl. Sci. Rev., 2023, 10: nwac261
[15] Lu W Q, Zhang S G, Zhang W, et al. A full view of the segregation evolution in Al-Bi immiscible alloy [J]. Metall. Mater. Trans., 2017, 48A: 2701
[16] Zhao J Z, Li H L, Zhang X F, et al. Nucleation determined microstructure formation in immiscible alloys [J]. Mater. Lett., 2008, 62: 3779
[17] Liu Y L, Liu S H, Du Y, et al. A general model to calculate coherent solid/solid and immiscible liquid/liquid interfacial energies [J]. Calphad, 2019, 65: 225
[18] Kaban I, Hoyer W. Effect of Cu and Sn on liquid-liquid interfacial energy in ternary and quaternary Al-Bi-based monotectic alloys [J]. Mater. Sci. Eng., 2008, 495A: 3
[19] Fu X C, Shen W X, Yao T Y, et al. Physical Chemistry [M]. 5th Ed., Beijing: Higher Education Press, 2005: 326
  付献彩, 沈文霞, 姚天扬 等. 物理化学 [M]. 第5版. 北京: 高等教育出版社, 2005: 326
[20] Sun Q, Jiang H X, Zhao J Z. Effect of micro-alloying element Bi on solidification and microstructure of Al-Pb alloy [J]. Acta Metall. Sin., 2016, 52: 497
  孙 倩, 江鸿翔, 赵九洲. 微量元素Bi对Al-Pb合金凝固过程及显微组织的影响 [J]. 金属学报, 2016, 52: 497
[21] Li W, Sun Q, Jiang H X, et al. Solidification of Al-Bi alloy and influence of microalloying element Sn [J]. Acta Metall. Sin., 2019, 55: 831
  黎 旺, 孙 倩, 江鸿翔 等. Al-Bi合金凝固过程及微合金化元素Sn的影响 [J]. 金属学报, 2019, 55: 831
[22] Hao S M, Jiang M, Li H X. Materials Thermodynamics [M]. 2nd Ed., Beijing: Chemical Industry Press, 2010: 151
  郝士明, 蒋 敏, 李洪晓. 材料热力学 [M]. 第2版. 北京: 化学工业出版社, 2010: 151
[23] Dinsdale A T. SGTE data for pure elements [J]. Calphad, 1991, 15: 317
[24] Wang C L. Phase Diagrams and Its Application [M]. Beijing: Higher Education Press, 2014: 9
  王崇琳. 相图理论及其应用(修订版) [M]. 北京: 高等教育出版社, 2014: 9
[25] David N, Vassiliev V, Hertz J, et al. EMF measurements and thermodynamic description of the Pb-Sn-Zn liquid phase [J]. Int. J. Mater. Res., 2004, 95: 124
[26] Vassiliev V P, Lysenko V A, Gong W P. New EMF measurements and thermodynamic evaluation of the In-Pb-Zn system [J]. J. Alloys Compd., 2013, 564: 49
[27] Miettinen J, Gandova V, Vassilev G. Thermodynamic description of the Cu-Pb-Zn system [J]. Calphad, 2010, 34: 377
[28] Gierlotka W, Tung Y C. A new thermodynamic description of the Bi-Pb-Sn system [J]. J. Phase Equilib. Diffus., 2017, 38: 814
[29] Malakhov D V. Thermodynamic assessment of the Bi-Zn system [J]. Calphad, 2000, 24: 1
[30] Yang L J, Zhang L L, Zhao J Z, et al. A simple criterion for the selection of interfacial active element to control liquid-liquid decomposition of immiscible alloys [J]. Scr. Mater., 2024, 238: 115753
[31] Kaptay G. Modelling interfacial energies in metallic systems [J]. Mater. Sci. Forum, 2005, 473-474: 1
[32] Zhang L L, Yang L J, Zhao J Z, et al. Selection of a micro-alloying interface active component to stabilize the interface between droplets and liquid matrix in monotectic alloys [J]. Acta Mater., 2023, 250: 118823
[33] Iida T, Guthrie R I L. The Physical Properties of Liquid Metals [M]. Oxford: Clarendon Press, 1988: 71
[34] Chatain D, Vahlas C, Eustathopoulos N. Study of liquid-liquid and solid-liquid interface tensions in systems with monotectic Zn-Pb and Zn-Pb-Sn [J]. Acta Metall., 1984, 32: 227
[35] Kaptay G. On the interfacial energy of coherent interfaces [J]. Acta Mater., 2012, 60: 6804
文章导航

/