后续热处理对激光3D打印GH4099合金微观组织和高温力学性能的影响
收稿日期: 2024-06-17
修回日期: 2024-07-29
网络出版日期: 2024-11-04
基金资助
国家自然科学基金项目(U22A20172);国家自然科学基金项目(52122409);国家重点研发计划项目(2023YFB3712002)
Effects of Subsequent Heat Treatment on Microstructure and High-Temperature Mechanical Properties of Laser 3D Printed GH4099 Alloy
Received date: 2024-06-17
Revised date: 2024-07-29
Online published: 2024-11-04
Supported by
National Natural Science Foundation of China(U22A20172);National Natural Science Foundation of China(52122409);National Key Research and Development Program of China(2023YFB3712002)
激光粉末床熔融(LPBF) 3D打印技术具有跨维度多尺度成形的技术特点,同时表现出非平衡快速凝固的冶金特征,与传统制造工艺形成的微观组织存在明显差异。基于传统制造工艺发展而来的热处理工艺难以适用于LPBF制备的样品,因此,研究LPBF打印件专用的后续热处理制度对于其组织和性能调控具有重要的意义。本工作以LPBF制备的GH4099合金为研究对象,研究了后续热处理对3D打印高温合金非平衡微观组织和高温力学性能的影响。结果表明,固溶处理不仅影响打印组织的再结晶行为,而且也与碳化物和γ'相的析出行为密切相关,因而对GH4099合金的高温延伸率影响较大。LPBF制备GH4099合金中的多尺度异质结构使其组织热稳定性明显高于传统铸锻件,因此需要更高的固溶热处理温度以促进其完全再结晶。经1150 ℃固溶处理1.5 h后,GH4099打印件中柱状晶转变为等轴晶并形成大尺寸孪晶,同时晶界处M23C6碳化物的析出也受到抑制。在随后的时效热处理过程中,由于再结晶释放了3D打印晶粒内部储存的畸变能,使得基体中γ'相的析出受到了明显抑制。基于上述结果,通过优化热处理制度,GH4099合金打印件实现了高温强度和塑性的良好匹配。
赵亚楠 , 郭乾应 , 刘晨曦 , 马宗青 , 刘永长 . 后续热处理对激光3D打印GH4099合金微观组织和高温力学性能的影响[J]. 金属学报, 2025 , 61(1) : 165 -176 . DOI: 10.11900/0412.1961.2024.00208
The multi-dimensional, multi-scale forming characteristics of laser powder bed fusion (LPBF) 3D printing technology, combined with its complex non-equilibrium solidification process, result in multilayered microstructures that differ significantly from those produced by traditional manufacturing methods. However, it is challenging to apply existing heat treatment solutions, developed for conventional manufacturing processes, to LPBF. Therefore, a tailored heat treatment approach is required for LPBF-printed components to regulate their microstructure and properties effectively. This study investigated the modulation mechanism of subsequent heat treatment on the non-equilibrium microstructure and high-temperature mechanical properties of 3D-printed GH4099 superalloy produced via LPBF. The findings reveal that solution treatment influences the recrystallization behavior of the printed microstructure and the precipitation behavior of carbides and γ' phases, which play critical roles in determining the alloy's high-temperature elongation. The multi-scale heterogeneous structure in the LPBF-fabricated GH4099 alloy enhances its microstructural thermal stability beyond that of conventional castings and forgings. Consequently, a high solution heat treatment temperature is necessary to achieve complete recrystallization. Following solution treatment at 1150 oC for 1.5 h, the columnar grains in the GH4099 prints were transformed into equiaxed grains, and large size twins were formed. Additionally, the precipitation of M23C6 carbides at the grain boundaries was suppressed. During subsequent aging heat treatment, the recrystallization induced by the solution treatment mitigated the distortion energy stored in the 3D-printed grains, thereby suppressing γ' phase precipitation in the matrix. As a result, by optimizing the heat treatment process, a favorable balance between high-temperature strength and plasticity was achieved in the GH4099 alloy.
| 1 | Yang B, Shang Z, Ding J, et al. Investigation of strengthening mechanisms in an additively manufactured Haynes 230 alloy[J]. Acta Mater., 2022, 222: 117404 |
| 2 | Sun S S, Teng Q, Xie Y, et al. Two-step heat treatment for laser powder bed fusion of a nickel-based superalloy with simultaneously enhanced tensile strength and ductility[J]. Addit. Manuf., 2021, 46: 102168 |
| 3 | Hosseini E, Popovich V A. A review of mechanical properties of additively manufactured Inconel 718[J]. Addit. Manuf., 2019, 30: 100877 |
| 4 | Song B, Zhang J L, Zhang Y J, et al. Research progress of materials design for metal laser additive manufacturing[J]. Acta Metall. Sin., 2023, 59: 1 |
| 宋 波, 张金良, 章媛洁 等. 金属激光增材制造材料设计研究进展[J]. 金属学报, 2023, 59: 1 | |
| 5 | Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys[J]. Nature, 2017, 549: 365 |
| 6 | Yang X, Wang B, Gu W P, et al. Application and research status of numerical simulation of metal laser 3D printing process[J]. J. Mater. Eng., 2021, 49(4): 52 |
| 杨 鑫, 王 犇, 谷文萍 等. 金属激光3D打印过程数值模拟应用及研究现状[J]. 材料工程, 2021, 49(4): 52 | |
| 7 | Sun Z J, Tan X P, Tor S B, et al. Simultaneously enhanced strength and ductility for 3D-printed stainless steel 316L by selective laser melting[J]. npg Asia Mater., 2018, 10: 127 |
| 8 | Chen Y, Guo Y B, Xu M J, et al. Study on the element segregation and Laves phase formation in the laser metal deposited IN718 superalloy by flat top laser and Gaussian distribution laser[J]. Mater. Sci. Eng., 2019, A754: 339 |
| 9 | Nadammal N, Mishurova T, Fritsch T, et al. Critical role of scan strategies on the development of microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing[J]. Addit. Manuf., 2021, 38: 101792 |
| 10 | Liu L F, Ding Q Q, Zhong Y, et al. Dislocation network in additive manufactured steel breaks strength-ductility trade-off[J]. Mater. Today, 2018, 21: 354 |
| 11 | Voisin T, Forien J B, Perron A, et al. New insights on cellular structures strengthening mechanisms and thermal stability of an austenitic stainless steel fabricated by laser powder-bed-fusion[J]. Acta Mater., 2021, 203: 116476 |
| 12 | Zhao Y N, Guo Q Y, Ma Z Q, et al. Comparative study on the microstructure evolution of selective laser melted and wrought IN718 superalloy during subsequent heat treatment process and its effect on mechanical properties[J]. Mater. Sci. Eng., 2020, A791: 139735 |
| 13 | Kok Y, Tan X P, Wang P, et al. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: A critical review[J]. Mater. Des., 2018, 139: 565 |
| 14 | Zhao Y H, Li K, Gargani M, et al. A comparative analysis of Inconel 718 made by additive manufacturing and suction casting: Microstructure evolution in homogenization[J]. Addit. Manuf., 2020, 36: 101404 |
| 15 | Wei B, Liu Z M, Nong B Z, et al. Microstructure, cracking behavior and mechanical properties of René 104 superalloy fabricated by selective laser melting[J]. J. Alloys Compd., 2021, 867: 158377 |
| 16 | Tang Y T, Panwisawas C, Ghoussoub J N, et al. Alloys-by-design: Application to new superalloys for additive manufacturing[J]. Acta Mater., 2021, 202: 417 |
| 17 | Cloots M, Uggowitzer P J, Wegener K. Investigations on the microstructure and crack formation of IN738LC samples processed by selective laser melting using Gaussian and doughnut profiles[J]. Mater. Des., 2016, 89: 770 |
| 18 | Chang K, Ma L, Li P T, et al. Effect of heat treatment on microstructure and mechanical properties of GH4099 superalloy fabricated by selective laser melting[J]. J. Alloys Compd., 2023, 934: 167813 |
| 19 | Harte A, Atkinson M, Smith A, et al. The effect of solid solution and gamma prime on the deformation modes in Ni-based superalloys[J]. Acta Mater., 2020, 194: 257 |
| 20 | Li J, Ding R, Guo Q Y, et al. Effect of solution cooling rate on microstructure evolution and mechanical properties of Ni-based superalloy ATI 718Plus[J]. Mater. Sci. Eng., 2021, A812: 141113 |
| 21 | Zhang P, Yuan Y, Yin H, et al. Tensile properties and deformation mechanisms of Haynes 282 at various temperatures[J]. Metall. Mater. Trans., 2018, 49A: 1571 |
| 22 | Hu R, Bai G H, Li J S, et al. Precipitation behavior of grain boundary M23C6 and its effect on tensile properties of Ni-Cr-W based superalloy[J]. Mater. Sci. Eng., 2012, A548: 83 |
| 23 | Dong R F, Li J S, Zhang T B, et al. Elements segregation and phase precipitation behavior at grain boundary in a Ni-Cr-W based superalloy[J]. Mater. Charact., 2016, 122: 189 |
| 24 | Tang Y T, Panwisawas C, Jenkins B M, et al. Multi-length-scale study on the heat treatment response to supersaturated nickel-based superalloys: Precipitation reactions and incipient recrystallisation[J]. Addit. Manuf., 2023, 62: 103389 |
| 25 | Son K T, Phan T Q, Levine L E, et al. The creep and fracture properties of additively manufactured inconel 625[J]. Materialia, 2021, 15: 101021 |
| 26 | Inaekyan K, Kreitcberg A, Turenne S, et al. Microstructure and mechanical properties of laser powder bed-fused IN625 alloy[J]. Mater. Sci. Eng., 2019, A768: 138481 |
| 27 | Li Y, Kan W B, Zhang Y M, et al. Microstructure, mechanical properties and strengthening mechanisms of IN738LC alloy produced by electron beam selective melting[J]. Addit. Manuf., 2021, 47: 102371 |
| 28 | Zhang H B, Zhang K F, Jiang S S, et al. Dynamic recrystallization behavior of a γ′-hardened nickel-based superalloy during hot deformation[J]. J. Alloys Compd., 2015, 623: 374 |
| 29 | Gao Y B, Ding Y T, Chen J J, et al. Effect of twin boundaries on the microstructure and mechanical properties of Inconel 625 alloy[J]. Mater. Sci. Eng., 2019, A767: 1383611 |
| 30 | Lu Y J, Zhao W, Yang C, et al. Improving mechanical properties of selective laser melted Co29Cr9W3Cu alloy by eliminating mesh-like random high-angle grain boundary[J]. Mater. Sci. Eng., 2020, A793: 1 |
| 31 | Gao S B, Hu Z H, Duchamp M, et al. Recrystallization-based grain boundary engineering of 316L stainless steel produced via selective laser melting[J]. Acta Mater., 2020, 200: 366 |
| 32 | Zhang L, Liu H S, He X B, et al. Thermal evolution behavior of carbides and γ′ precipitates in FGH96 superalloy powder[J]. Mater. Charact., 2012, 67: 52 |
| 33 | Wang Y M, Voisin T, McKeown J T, et al. Additively manufactured hierarchical stainless steels with high strength and ductility[J]. Nat. Mater., 2018, 17: 63 |
| 34 | Bai G H, Hu R, Li J S, et al. Secondary M23C6 precipitation behavior in Ni-Cr-W based superalloy[J]. Rare Met. Mater. Eng., 2011, 40: 1737 |
| 柏广海, 胡 锐, 李金山 等. Ni-Cr-W基高温合金二次M23C6析出行为[J]. 稀有金属材料与工程, 2011, 40: 1737 | |
| 35 | Tan Y, You X G, You Q F, et al. Microstructure and deformation behavior of nickel based superalloy Inconel 740 prepared by electron beam smelting[J]. Mater. Charact., 2016, 114: 267 |
| 36 | Wang Z Y, Muránsky O, Zhu H L, et al. On the kinetics of gamma prime (γ') precipitation and its strengthening mechanism in alloy 617 during a long-term thermal aging[J]. Materialia, 2020, 11: 100682 |
| 37 | Mei Y P, Liu Y C, Liu C X, et al. Effects of cold rolling on the precipitation kinetics and the morphology evolution of intermediate phases in Inconel 718 alloy[J]. J. Alloys Compd., 2015, 649: 949 |
| 38 | Qin H L, Bi Z N, Yu H Y, et al. Influence of stress on γ″ precipitation behavior in Inconel 718 during aging[J]. J. Alloys Compd., 2018, 740: 997 |
| 39 | Bober D B, Lind J, Mulay R P, et al. The formation and characterization of large twin related domains[J]. Acta Mater., 2017, 129: 500 |
| 40 | Kumar N. An exploration of microstructural in-homogeneity in the 6082 Al alloy processed through room temperature multi-axial forging[J]. Mater. Charact., 2021, 176: 111134 |
| 41 | Chinese Society of Metals High Temperature Materials Branch. China Superalloys Handbook[M]. Beijing: China Quality Inspection Press, 2012: 599 |
| 中国金属学会高温材料分会. 中国高温合金手册[M]. 北京: 中国质检出版社, 2012: 599 | |
| 42 | Gallmeyer T G, Moorthy S, Kappes B B, et al. Knowledge of process-structure-property relationships to engineer better heat treatments for laser powder bed fusion additive manufactured Inconel 718[J]. Addit. Manuf., 2020, 31: 100977 |
| 43 | Zhang Z H, Han Q Q, Liu Z Y, et al. Influence of the TiB2 content on the processability, microstructure and high-temperature tensile performance of a Ni-based superalloy by laser powder bed fusion[J]. J. Alloys Compd., 2022, 908: 164656 |
| 44 | Du B N, Hu Z Y, Sheng L Y, et al. Tensile, creep behavior and microstructure evolution of an as-cast Ni-based K417G polycrystalline superalloy[J]. J. Mater. Sci. Technol., 2018, 34: 1805 |
| 45 | de Oliveira M M, Couto A A, Almeida G F C, et al. Mechanical behavior of Inconel 625 at elevated temperatures[J]. Metals, 2019, 9: 301 |
| 46 | Hu Y L, Li Y L, Zhang S Y, et al. Effect of solution temperature on static recrystallization and ductility of Inconel 625 superalloy fabricated by directed energy deposition[J]. Mater. Sci. Eng., 2020, A772: 138711 |
| 47 | Hu Y L, Lin X, Zhang S Y, et al. Effect of solution heat treatment on the microstructure and mechanical properties of Inconel 625 superalloy fabricated by laser solid forming[J]. J. Alloys Compd., 2018, 767: 330 |
| 48 | McCarley J, Helmink R, Goetz R, et al. Grain boundary engineering of a low stacking fault energy Ni-based Superalloy[J]. Metall. Mater. Trans., 2017, 48A: 1666 |
| 49 | Hu Z P, Guan K, Qian Z, et al. Simultaneous enhancement of strength and ductility in selective laser melting manufactured 316L alloy by employing Y2O3 coated spherical powder as precursor[J]. J. Alloys Compd., 2022, 899: 163262 |
| 50 | Németh A A N, Crudden D J, Armstrong D E J, et al. Environmentally-assisted grain boundary attack as a mechanism of embrittlement in a nickel-based superalloy[J]. Acta Mater., 2017, 126: 361 |
| 51 | Zheng L, Schmitz G, Meng Y, et al. Mechanism of intermediate temperature embrittlement of Ni and Ni-based superalloys[J]. Crit. Rev. Solid State Mater. Sci., 2012, 37: 181 |
| 52 | Bahl S, Plotkowski A, Sisco K, et al. Elevated temperature ductility dip in an additively manufactured Al-Cu-Ce alloy[J]. Acta Mater., 2021, 220: 117285 |
| 53 | Lei Y C, Aoyagi K, Aota K, et al. Critical factor triggering grain boundary cracking in non-weldable superalloy Alloy713ELC fabricated with selective electron beam melting[J]. Acta Mater., 2021, 208: 116695 |
| 54 | Hrutkay K, Kaoumi D. Tensile deformation behavior of a nickel based superalloy at different temperatures[J]. Mater. Sci. Eng., 2014, A599: 196 |
| 55 | Shin K Y, Kim J H, Terner M, et al. Effects of heat treatment on the microstructure evolution and the high-temperature tensile properties of Haynes 282 superalloy[J]. Mater. Sci. Eng., 2019, A751: 311 |
| 56 | Zhong Z H, Gu Y F, Yuan Y, et al. Tensile properties and deformation characteristics of a Ni-Fe-base superalloy for steam boiler applications[J]. Metall. Mater. Trans., 2013, 45A: 343 |
/
| 〈 |
|
〉 |