研究论文

深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺

  • 刘庚 ,
  • 单以银 ,
  • 严伟 ,
  • 苏锐 ,
  • 任毅 ,
  • 史显波
展开
  • 1.中国科学技术大学 材料科学与工程学院 沈阳 110016
    2.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016
    3.中国科学院金属研究所 沈阳材料科学国家研究中心 沈阳 110016
    4.鞍钢集团 海洋装备用金属材料及其应用全国重点实验室 鞍山 114009
刘 庚,男,1997年生,博士生
单以银,yyshan@imr.ac.cn,主要从事先进钢铁结构材料设计、制备、表征与使役行为研究

收稿日期: 2024-08-28

  修回日期: 2024-11-01

  网络出版日期: 2024-11-04

基金资助

国家自然科学基金项目(52201093);工业和信息化部专项项目(2240STCZB2346);海洋装备国家重点实验室开放基金项目(SKLMEA-K202205)

Thermal Deformation Behavior and Hot Rolling Process of X65/Inconel 625 Bimetal Composite Plate for Deep Sea Oil and Gas Field Transportation

  • LIU Geng ,
  • SHAN Yiyin ,
  • YAN Wei ,
  • SU Rui ,
  • REN Yi ,
  • SHI Xianbo
Expand
  • 1.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    2.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3.Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    4.State Key Laboratory of Metal Materials for Marine Equipment and Application, Ansteel Group Corporation, Anshan 114009, China
SHAN Yiyin, professor, Tel: (024)23971517, E-mail: yyshan@imr.ac.cn

Received date: 2024-08-28

  Revised date: 2024-11-01

  Online published: 2024-11-04

Supported by

National Natural Science Foundation of China(52201093);Special Project of Ministry of Industry and Information Technology(2240STCZB2346);Open Fund of State Key Laboratory of Marine Equipment(SKLMEA-K202205)

摘要

针对异质双金属复合材料在热轧过程中变形不协调严重影响性能和界面结合强度的问题,本工作对深海油气输送用X65/Inconel 625双金属复合板热轧工艺的精准调控进行研究。利用Gleeble-3800热模拟试验机对基材X65管线钢和内衬层Inconel 625耐蚀合金进行了热压缩实验,研究了双金属的流变应力、本构关系、热加工图、界面抗弯性能和微观组织特征等。结果表明,随着变形温度的升高和应变速率的降低,双金属的峰值应力差逐渐减小。在高温条件(≥ 950 ℃)下,X65钢的主要软化机制为动态回复,而Inconel 625合金为动态再结晶。理论分析与实验结果相结合可知,理想的双金属复合板的热轧工艺窗口为:1000 ℃终轧、70%压下量。在该参数下热轧后,界面平直且复合良好,具有较强的弯曲变形能力。复合板纵向屈服强度为469 MPa,抗拉强度为606 MPa,延伸率为30%,剪切强度为442 MPa。

本文引用格式

刘庚 , 单以银 , 严伟 , 苏锐 , 任毅 , 史显波 . 深海油气田输送用X65/Inconel 625双金属复合板热变形行为及热轧工艺[J]. 金属学报, 2026 , 62(4) : 572 -586 . DOI: 10.11900/0412.1961.2024.00303

Abstract

The service environment of deep-sea oil and gas pipelines is becoming increasingly harsh, making it difficult for traditional single-metal pipeline steels to meet the unique demands of such environments. Bimetal composite materials leverage the advantages of bimetal components to achieve properties that are not possible with single metal materials. Hot rolling, a solid-phase bonding process that joins pipeline steel substrates and stainless steel at high temperatures, is an efficient method for creating strong interfaces. This technique is particularly suitable for the large-scale industrial production of bimetal clad plates, necessitating the establishment of an industrial production line. To overcome the challenge posed by deformation inconsistencies that adversely affect the properties and interface bonding strength of heterogeneous bimetal clad materials during hot rolling, the precise control of the hot rolling process for X65/Inconel 625 bimetal composite plates intended for deep-sea oil and gas transportation was investigated. Thermal compression tests on the X65 pipeline steel and Inconel 625 corrosion-resistant alloy were carried out using a Gleeble-3800 thermal simulation testing machine. The flow stress, constitutive relationships, thermal working diagram, interface bending resistance, and microstructure characteristics of the bimetallic materials were examined. The results indicate that the peak stress difference in the bimetallic materials decreases as the deformation temperature increases and the strain rate decreases. At high temperatures (≥ 950 oC), the primary softening mechanism for X65 steel is dynamic recovery, whereas that for Inconel 625 is dynamic recrystallization. Our findings suggest that the optimal hot rolling process for the bimetal clad plate should involve a final rolling temperature of 1000 oC and a reduction of 70%, based on theoretical analysis and experimental data. The interface is straight and well-combined, and demonstrates strong bending deformation ability. The bimetal clad plate achieves a rolling direction yield strength of 469 MPa, tensile strength of 606 MPa, elongation of 30%, and shear strength of 442 MPa.

参考文献

[1] Li Z, Zhao J W, Jia F H, et al. Interfacial characteristics and mechanical properties of duplex stainless steel bimetal composite by heat treatment [J]. Mater. Sci. Eng., 2020, A787: 139513
[2] Hedayati O, Korei N, Adeli M, et al. Microstructural evolution and interfacial diffusion during heat treatment of Hastelloy/stainless steel bimetals [J]. J. Alloys Compd., 2017, 712: 172
[3] Li Z, Zhao J W, Jia F H, et al. Analysis of bending characteristics of bimetal steel composite [J]. Int. J. Mech. Sci., 2018, 148: 272
[4] Poberezhnyi L, Maruschak P, Prentkovskis O, et al. Fatigue and failure of steel of offshore gas pipeline after the laying operation [J]. Arch. Civ. Mech. Eng., 2016, 16: 524
[5] O’Grady R, Harte A. Localised assessment of pipeline integrity during ultra-deep S-lay installation [J]. Ocean Eng., 2013, 68: 27
[6] Su G X, Shi Y, Li G, et al. High-efficiency fabrication of Inconel 625 coating for AISI 1045 carbon steel through laser cladding with hot wire: Microstructure and wear resistance [J]. J. Manuf. Process., 2023, 102: 622
[7] Li H L, Liu S X, Sun F X, et al. Preliminary investigation on underwater wet welding of Inconel 625 alloy: Microstructure, mechanical properties and corrosion resistance [J]. J. Mater. Res. Technol., 2022, 20: 2394
[8] Acarer M, Gülen? B, Findik F. Investigation of explosive welding parameters and their effects on microhardness and shear strength [J]. Mater. Des., 2003, 24: 659
[9] Liu F J, Zheng J Y, Xu P, et al. Forming mechanism of double-layered tubes by internal hydraulic expansion [J]. Int. J. Press Vessels Pip., 2004, 81: 625
[10] Huang Q X, Yang X R, Ma L F, et al. Interface-correlated characteristics of stainless steel/carbon steel plate fabricated by AAWIV and hot rolling [J]. J. Iron Steel Res. Int., 2014, 21: 931
[11] Xie G M, Luo Z A, Wang G L, et al. Interface characteristic and properties of stainless steel/HSLA steel clad plate by vacuum rolling cladding [J]. Mater. Trans., 2011, 52: 1709
[12] Li L, Yin F X, Nagai K. Progress of laminated materials and clad steels production [J]. Mater. Sci. Forum, 2011, 675-677: 439
[13] Tachibana S, Kuronuma Y, Yokota T, et al. Effect of hot rolling and cooling conditions on intergranular corrosion behavior in Alloy625 clad steel [J]. Corros. Sci., 2015, 99: 125
[14] Chen C X, Guo Y, Liu B X, et al. Interfacial microstructure characteristics and mechanical properties of X65/IN625 composite plates with different interlayers [J]. Mater. Lett., 2024, 362: 136184
[15] Liu W H, Yue X M, Hu Q, et al. Effects of recrystallization and element diffusion behavior on interfacial bonding quality and mechanical properties of aluminum laminated composites [J]. J. Alloys Compd., 2024, 985: 174045
[16] Zhu Z C, He Y, Zhang X J, et al. Effect of interface oxides on shear properties of hot-rolled stainless steel clad plate [J]. Mater. Sci. Eng., 2016, A669: 344
[17] Liu B X, Yin F X, Dai X L, et al. The tensile behaviors and fracture characteristics of stainless steel clad plates with different interfacial status [J]. Mater. Sci. Eng., 2017, A679: 172
[18] Cao F R, Ding X, Xiang C, et al. Flow stress, microstructural evolution, and constitutive analysis during high-temperature deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y alloy [J]. Acta Metall. Sin., 2021, 57: 860
  曹富荣, 丁 鑫, 项 超 等. Mg-4.4Li-2.5Zn-0.46Al-0.74Y合金高温变形流动应力、组织演变与本构分析 [J]. 金属学报, 2021, 57: 860
[19] Li F L, Fu R, Bai Y R, et al. Effects of initial grain size and strengthening phase on thermal deformation and recrystallization behavior of GH4096 superalloy [J]. Acta Metall. Sin., 2023, 59: 855
  李福林, 付 锐, 白云瑞 等. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 [J]. 金属学报, 2023, 59: 855
[20] Zhou G, Wang C, Li J L, et al. Structure evolution mechanism and physical modeling of Ni60Ti40 during dynamic recrystallization [J]. Mater. Charact., 2022, 190: 112028
[21] Li N, Zhao C Z, Jiang Z H, et al. Flow behavior and processing maps of high-strength low-alloy steel during hot compression [J]. Mater. Charact., 2019, 153: 224
[22] Chen L, Zhang B, Yang Y, et al. Evolution of hot processing map and microstructure of as-forged nickel-based superalloy during hot deformation [J]. J. Mater. Res. Technol., 2023, 24: 7638
[23] Jonas J J, Sellars C M, Tegart W J M. Strength and structure under hot-working conditions [J]. Int. Mater. Rev., 1969, 14: 1
[24] Ma X, Zeng W D, Tian F, et al. Optimization of hot process parameters of Ti-6.7Al-2Sn-2.2Zr-2.1Mo-1W-0.2Si alloy with lamellar starting microstructure based on the processing map [J]. Mater. Sci. Eng., 2012, A545: 132
[25] Peng X N, Guo H Z, Shi Z F, et al. Constitutive equations for high temperature flow stress of TC4-DT alloy incorporating strain, strain rate and temperature [J]. Mater. Des., 2013, 50: 198
[26] Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Mater. Trans., 1984, 15A: 1883
[27] Hernandez C A, Medina S F, Ruiz J. Modelling austenite flow curves in low alloy and microalloyed steels [J]. Acta Mater., 1996, 44: 155
[28] Tan Y B, Ma Y H, Zhao F. Hot deformation behavior and constitutive modeling of fine grained Inconel 718 superalloy [J]. J. Alloys Compd., 2018, 741: 85
[29] Li J S, Cheng G J, Yen H W, et al. Microstrain and boundary misorientation evolution for recrystallized super DSS after deformation [J]. Mater. Chem. Phys., 2020, 246: 122815
[30] Lin Y C, He M, Zhou M, et al. New constitutive model for hot deformation behaviors of Ni-based superalloy considering the effects of initial δ phase [J]. J. Mater. Eng. Perform., 2015, 24: 3527
文章导航

/