Cr对FeWB块体金属玻璃热稳定性和耐腐蚀性能的影响
收稿日期: 2024-05-17
修回日期: 2024-09-09
网络出版日期: 2024-10-31
基金资助
国家自然科学基金项目(52071276)
Effect of Chromium on Thermal Stability and Corrosion Resistance in FeWB Bulk Metallic Glasses
Received date: 2024-05-17
Revised date: 2024-09-09
Online published: 2024-10-31
Supported by
National Natural Science Foundation of China(52071276)
块体金属玻璃属于热力学亚稳态合金,其非晶结构在环境温度超过玻璃转变温度时易失稳,从而导致其优异性能退化。提高非晶合金的热稳定性对于维持其综合性能至关重要。本工作在Fe59W23B18 (原子分数,%)块体金属玻璃基础上,引入Cr元素,制备了一系列(Fe1 - x Cr x )59W23B18 (x = 0、0.05、0.1、0.15、0.2、0.25)块体金属玻璃。结果表明,Cr元素显著提高了该块体金属玻璃的热稳定性,其中(Fe0.9Cr0.1)59W23B18金属玻璃的玻璃转变温度为954 K,晶化起始温度为994 K,极高的热稳定性主要源于Cr的引入使得体系更容易形成强过渡金属-类金属共价键(Cr—B键),增强了原子间的相互作用。此外,大量类Fe23B6的中程序结构也进一步提高了体系的稳定性。Cr元素进一步降低了该金属玻璃体系的自腐蚀电流密度,这主要得益于Cr促进了合金表面稳定钝化膜的形成。然而,Cr2O3的抗点蚀能力弱于WO3,导致合金的抗点蚀能力有所下降。
肖思明 , 刘天豪 , 苏辰 , 郭胜锋 . Cr对FeWB块体金属玻璃热稳定性和耐腐蚀性能的影响[J]. 金属学报, 2026 , 62(3) : 458 -466 . DOI: 10.11900/0412.1961.2024.00168
Bulk metallic glasses are thermodynamically metastable alloys with an amorphous structure that becomes increasingly unstable at temperatures above their glass transition temperature, leading to degradation of their advantageous properties. Thus, enhancing the thermal stability of bulk metallic glasses is critical for preserving their exceptional characteristics. Recently, our team successfully synthesized a Fe59W23B18 (atomic fraction, %) bulk metallic glass that exhibits high thermal stability and further developed a series of (Fe1 - x Cr x )59W23B18 (x = 0, 0.05, 0.1, 0.15, 0.2, 0.25) bulk metallic glasses by incorporating Cr in this study. Results show that Cr addition notably enhanced the thermal stability of FeWB bulk metallic glasses, with (Fe0.9Cr0.1)59W23B18 achieving a glass transition temperature of 954 K and an crystallization onset temperature of 994 K. This substantial increase in thermal stability is primarily attributed to Cr playing a role in the formation of strong metal-metalloid covalent bonds (Cr—B bonds), which enhance interatomic interactions. Additionally, the substantial presence of an Fe23B6-like medium-range order structure further stabilized the system. Furthermore, the corrosion resistance of the FeWB bulk metallic glass system was considerably improved by Cr addition, as indicated by an approximately 10-fold reduction in the corrosion current density. This enhancement can be primarily attributed to the formation of a dense Cr2O3 passivation layer on the alloy surface. However, the reduced pitting potential of Cr2O3 relative to WO3 led to a slight decrease in the pitting corrosion resistance of the FeCrWB alloys.
| [1] | Wang W H, Dong C, Shek C H. Bulk metallic glasses [J]. Mater. Sci. Eng., 2004, R44: 45 |
| [2] | Lai L M, Ding K L, Liu T H, et al. Ternary Co-W-B bulk metallic glasses with ultrahigh strength [J]. J. Non-Cryst. Solids, 2020, 544: 120194 |
| [3] | Puszkarz A, Wasiak M, Ró?ański A, et al. Structural and magnetic properties of FinemetTM doped with Ta [J]. J. Alloys Compd., 2010, 491: 495 |
| [4] | Suo Z Y, Song Y L, Yu B, et al. Fabrication of tungsten-based metallic glasses by low purity industrial raw materials [J]. Mater. Sci. Eng., 2011, A528: 2912 |
| [5] | Kim J, Kyeong J S, Ham M H, et al. Development of Mo-Ni-Si-B metallic glass with high thermal stability and H versus E ratios [J]. Mater. Des., 2016, 98: 31 |
| [6] | Li M X, Zhao S F, Lu Z, et al. High-temperature bulk metallic glasses developed by combinatorial methods [J]. Nature, 2019, 569: 99 |
| [7] | Li H X, Lu Z C, Wang S L, et al. Fe-based bulk metallic glasses: Glass formation, fabrication, properties and applications [J]. Prog. Mater. Sci., 2019, 103: 235 |
| [8] | Liu T H, Guo S F. Research progress of glass-formation rule and mechanical properties of Fe-based bulk amorphous alloys [J]. J. Mater. Eng., 2020, 48(11): 46 |
| 刘天豪, 郭胜锋. 铁基块体非晶合金的形成规律与力学性能研究进展 [J]. 材料工程, 2020, 48(11): 46 | |
| [9] | Li Y C, Zhang C, Xing W, et al. Design of Fe-based bulk metallic glasses with improved wear resistance [J]. ACS Appl. Mater. Interfaces, 2018, 10: 43144 |
| [10] | Guo S F, Qiu J L, Yu P, et al. Fe-based bulk metallic glasses: Brittle or ductile? [J]. Appl. Phys. Lett., 2014, 105: 161901 |
| [11] | Liu T H, Lai L M, Xiao S M, et al. Ternary Fe-W-B bulk metallic glasses with ultrahigh thermal stabilities [J]. Mater. Sci. Eng., 2021, A826: 142034 |
| [12] | Geng Y X, Wang Y M. Local structure-property correlation of Fe-based amorphous alloys: Based on minor alloying research [J]. Acta Metall. Sin., 2020, 56: 1558 |
| 耿遥祥, 王英敏. 铁基非晶合金局域结构与性能关联: 基于微合金化机理研究 [J]. 金属学报, 2020, 56: 1558 | |
| [13] | Xu T, Pang S J, Li H F, et al. Corrosion resistant Cr-based bulk metallic glasses with high strength and hardness [J]. J. Non-Cryst. Solids, 2015, 410: 20 |
| [14] | Kim D H, Park J M, Kim D H, et al. Development of quaternary Fe-B-Y-Nb bulk glassy alloys with high glass-forming ability [J]. J. Mater. Res., 2007, 22: 471 |
| [15] | Lai L M, Liu T H, Cai X H, et al. High-temperature Mo-based bulk metallic glasses [J]. Scr. Mater., 2021, 203: 114095 |
| [16] | Meng D, Yi J, Zhao D Q, et al. Tantalum based bulk metallic glasses [J]. J. Non-Cryst. Solids, 2011, 357: 1787 |
| [17] | Madge S V, Caron A, Gralla R, et al. Novel W-based metallic glass with high hardness and wear resistance [J]. Intermetallics, 2014, 47: 6 |
| [18] | Takeuchi A, Inoue A. Calculations of mixing enthalpy and mismatch entropy for ternary amorphous alloys [J]. Mater. Trans., JIM, 2000, 41: 1372 |
| [19] | Kalescky R, Kraka E, Cremer D. Identi?cation of the strongest bonds in chemistry [J]. J. Phys. Chem., 2013, 117A: 8981 |
| [20] | Li Q, Li J F, Gong P, et al. Formation of bulk magnetic ternary Fe80P13C7 glassy alloy [J]. Intermetallics, 2012, 26: 62 |
| [21] | Liu D Y, Sun W S, Wang A M, et al. Preparation, thermal stability, and magnetic properties of Fe-Co-Zr-Mo-W-B bulk metallic glass [J]. J. Alloys Compd., 2004, 370: 249 |
| [22] | Ma R D, Zhang H F, Yu H S, et al. The effect of Al substitution on thermal and mechanical properties of Fe-based bulk metallic glass [J]. J. Alloys Compd., 2008, 454: 370 |
| [23] | Guo S F, Wu Z Y, Liu L. Preparation and magnetic properties of FeCoHfMoBY bulk metallic glasses [J]. J. Alloys Compd., 2009, 468: 54 |
| [24] | Pan J, Chen Q, Li N, et al. Formation of centimeter Fe-based bulk metallic glasses in low vacuum environment [J]. J. Alloys Compd., 2008, 463: 246 |
| [25] | Shi M J, Pang S J, Zhang T. Towards improved integrated properties in FeCrPCB bulk metallic glasses by Cr addition [J]. Intermetallics, 2015, 61: 16 |
| [26] | Jia Y Z, Zeng S Y, Shan S F, et al. Effect of copper addition on the glass forming ability of a Fe-Co based alloy [J]. J. Alloys Compd., 2007, 440: 113 |
| [27] | Xu T, Jian Z Y, Chang F G, et al. Synthesis of Fe75Cr5(PBC)20 bulk metallic glasses with a combination of desired merits using industrial ferro-alloys without high-purity materials [J]. J. Alloys Compd., 2017, 699: 92 |
| [28] | Chen Q J, Zhang D L, Shen J, et al. Effect of yttrium on the glass-forming ability of Fe-Cr-Mo-C-B bulk amorphous alloys [J]. J. Alloys Compd., 2007, 427: 190 |
| [29] | Yang W M, Wan C, Liu H S, et al. Fluxing induced boron alloying in Fe-based bulk metallic glasses [J]. Mater. Des., 2017, 129: 63 |
| [30] | Xu M, Quan M X, Hu Z Q, et al. Thermal stability and magnetic properties of amorphous Fe-based alloys with significant supercooled liquid region [J]. J. Alloys Compd., 2002, 334: 238 |
| [31] | Shen J, Chen Q J, Sun J F, et al. Exceptionally high glass-forming ability of an FeCoCrMoCBY alloy [J]. Appl. Phys. Lett., 2005, 86: 151907 |
| [32] | Chen Q, Zhang D, Shen J, et al. Effect of yttrium on the glass-forming ability of Fe-Cr-Mo-C-B bulk amorphous alloys [J]. J. Alloys Compd., 2007, 427: 190 |
| [33] | Pang S J, Zhang T, Asami K, et al. Bulk glassy Fe-Cr-Mo-C-B alloys with high corrosion resistance [J]. Corros. Sci., 2002, 44: 1847 |
| [34] | Huang X M, Chang C T, Chang Z Y, et al. Glass forming ability, mechanical and magnetic properties in Fe-W-Y-B alloys [J]. Mater. Sci. Eng., 2010, A527: 1952 |
| [35] | Liang D D, Wei X S, Chang C T, et al. Effect of W addition on the glass forming ability and mechanical properties of Fe-based metallic glass [J]. J. Alloys Compd., 2018, 731: 1146 |
| [36] | Suryanarayana C, Inoue A. Iron-based bulk metallic glasses [J]. Int. Mater. Rev., 2013, 58: 131 |
| [37] | Guan P F, Sun S J. Atomic-level study in the structure and its instability of metallic glasses [J]. Acta Metall. Sin., 2021, 57: 501 |
| 管鹏飞, 孙胜君. 金属玻璃结构及其失稳的原子层次研究 [J]. 金属学报, 2021, 57: 501 | |
| [38] | Hirata A, Hirotsu Y, Amiya K, et al. Fe23B6-type quasicrystal-like structures without icosahedral atomic arrangement in an Fe-based metallic glass [J]. Phys. Rev., 2009, 80B:140201(R) |
| [39] | Gu X J, Poon S J, Shiflet G J, et al. Ductility improvement of amorphous steels: Roles of shear modulus and electronic structure [J]. Acta Mater. 2008, 56: 88 |
| [40] | Shen B L, Inoue A, Chang C T. Superhigh strength and good soft-magnetic properties of (Fe,Co)-B-Si-Nb bulk glassy alloys with high glass-forming ability [J]. Appl. Phys. Lett., 2004, 85: 4911 |
| [41] | Lu Z P, Liu C T, Thompson J R, et al. Structural amorphous steels [J]. Phys. Rev. Lett., 2004, 92: 245503 |
| [42] | Zhang J W, Su C, Zhang X P, et al. Fe-based bulk metallic glass with high thermal stability and corrosion resistance [J]. J. Non-Cryst. Solids, 2024, 643:123176 |
| [43] | Qu R T, Liu Z Q, Wang R F, et al. Yield strength and yield strain of metallic glasses and their correlations with glass transition temperature [J]. J. Alloys Compd., 2015, 637: 44 |
| [44] | Bi J Z, Wei X Q, Liu X B, et al. OsCo-based high-temperature bulk metallic glasses with robust mechanical properties [J]. Scr. Mater., 2023, 228: 115336 |
| [45] | Yang X D, Gao M, Liu Y H, et al. Superior corrosion resistance of high-temperature Ir-Ni-Ta-(B) amorphous alloy in sulfuric acid solution [J]. Corros. Sci., 2022, 200: 110227 |
| [46] | Zhang L M, Zhang S D, Ma A L, et al. Thermally induced structure evolution on the corrosion behavior of Al-Ni-Y amorphous alloys [J]. Corros. Sci., 2018, 144: 172 |
| [47] | Gan Z, Zhang C, Zhang Z R, et al. Crystallization-dependent transition of corrosion resistance of an Fe-based bulk metallic glass under hydrostatic pressures [J]. Corros. Sci., 2021, 179: 109098 |
| [48] | Xu T, Li X, Zhuo L C, et al. Synthesis of Cr50Fe6Co7Mo14C15B6Y2 bulk metallic glass with integrated merits by high-content solvent element substitution and the structural origin [J]. J. Mater. Res. Technol., 2021, 14: 220 |
| [49] | Liu D Y, Zhang H F, Hu Z Q, et al. Magnetic and corrosion properties of Fe56Co7 M2Mo5Zr10B20 (M = W or Ni) bulk metallic glasses [J]. J. Alloys Compd., 2006, 422: 28 |
| [50] | Guo S F, Chan K C, Xie S H, et al. Novel centimeter-sized Fe-based bulk metallic glass with high corrosion resistance in simulated acid rain and seawater [J]. J. Non-Cryst. Solids, 2013, 369: 29 |
| [51] | Zhang X P, Lai L M, Xiao S M, et al. Effect of W on the thermal stability, mechanical properties and corrosion resistance of Fe-based bulk metallic glass [J]. Intermetallics, 2021, 143: 107485 |
| [52] | Li J W, Yang L J, Ma H R, et al. Improved corrosion resistance of novel Fe-based amorphous alloys [J]. Mater. Des., 2016, 95: 225 |
/
| 〈 |
|
〉 |