研究论文

Fe7(CoNiMn)80B13 共晶高熵合金的深过冷非平衡凝固行为及微观组织演变

  • 王叶青 ,
  • 付珂 ,
  • 赵永柱 ,
  • 苏礼季 ,
  • 陈正
展开
  • 中国矿业大学 材料与物理学院 徐州 221116
王叶青,女,1991年生,博士
陈 正,chenzheng1218@163.com,主要从事金属非平衡凝固与材料成型加工研究

收稿日期: 2024-04-16

  修回日期: 2024-07-25

  网络出版日期: 2024-08-26

基金资助

国家自然科学基金项目(52201055);国家自然科学基金项目(52274401)

Non-Equilibrium Solidification Behavior and Microstructure Evolution of Undercooled Fe7(CoNiMn)80B13 Eutectic High-Entropy Alloy

  • WANG Yeqing ,
  • FU Ke ,
  • ZHAO Yongzhu ,
  • SU Liji ,
  • CHEN Zheng
Expand
  • School of Material Science and Physics, China University of Mining and Technology, Xuzhou 221116, China
CHEN Zheng, professor, Tel: 13655207199, E-mail: chenzheng1218@163.com

Received date: 2024-04-16

  Revised date: 2024-07-25

  Online published: 2024-08-26

Supported by

National Natural Science Foundation of China(52201055);National Natural Science Foundation of China(52274401)

摘要

Fe7(CoNiMn)80B13共晶高熵合金在非平衡凝固过程中存在复杂的相变及微观组织演变行为。为了揭示其非平衡凝固特征及组织演变机理,本工作采用熔融玻璃包覆法对Fe7(CoNiMn)80B13共晶高熵合金进行了深过冷凝固,研究了该共晶高熵合金的深过冷凝固行为及微观组织演变特征。结果表明,Fe7(CoNiMn)80B13共晶高熵合金在深过冷凝固过程中的凝固路径及凝固组织可以分为5类。在小过冷度下(ΔT < 57 K),冷却曲线只有一次再辉现象,对应的凝固组织为初生富B相+ α-(Fe, Co, Ni, Mn)包晶相+共晶组织。在中等过冷度下(ΔT = 57~111 K),冷却曲线上出现2次再辉现象,对应的凝固组织可以分为2种:第一种为初生M23B6枝晶+次生α-(Fe, Co, Ni, Mn)晕圈+规则共晶;第二种为初生α-(Fe, Co, Ni, Mn)枝晶+规则共晶。在大过冷度下(ΔT = 139~198 K),冷却曲线再次表现出单再辉现象,对应的凝固组织也可以分为2种:第一种为富B相 + M23B6 + α-(Fe, Co, Ni, Mn),3相各自存在;第二种为M23B6 + α-(Fe, Co, Ni, Mn)的反常共晶。随着过冷度的增加,初生相的种类发生了2次转变:富B相→M23B6相→α-(Fe, Co, Ni, Mn)相。另外,小过冷度下获得的规则共晶中共晶2相的取向关系与大过冷度下获得的反常共晶中共晶2相的取向关系一致。

本文引用格式

王叶青 , 付珂 , 赵永柱 , 苏礼季 , 陈正 . Fe7(CoNiMn)80B13 共晶高熵合金的深过冷非平衡凝固行为及微观组织演变[J]. 金属学报, 2025 , 61(1) : 143 -153 . DOI: 10.11900/0412.1961.2024.00111

Abstract

Eutectic high-entropy alloys show excellent properties, such as casting property, mechanical properties, corrosion resistance properties, and so on. They are usually consisted of two kinds of phases, which would be compete with each other in the non-equilibrium solidification process. Fe7(CoNiMn)80B13 eutectic high-entropy alloy has complex phase transition and microstructure evolution behavior during the non-equilibrium solidification process. In order to reveal the non-equilibrium solidification characteristics and microstructure evolution mechanism, Fe7(CoNiMn)80B13 eutectic high-entropy alloy was undercooled by the molten glass fluxing method in this work. The results show that the solidification path and microstructure of undercooled Fe7(CoNiMn)80B13 eutectic high-entropy alloy can be divided into 5 categories. At low undercooling (ΔT < 57 K), the cooling curve has only one recalescence phenomenon. The corresponding solidification microstructure is primary B-rich phase + peritectic α-(Fe, Co, Ni, Mn) phase + eutectic structure. At medium undercooling (ΔT = 57~111 K), there are two recalescence phenomena on the cooling curve. The corresponding solidification microstructure can be divided into two types: the first is primary M23B6 dendrite + secondary α-(Fe, Co, Ni, Mn) halo + regular eutectic; the second is primary α-(Fe, Co, Ni, Mn) dendrite + regular eutectic. At high undercooling (ΔT = 139~198 K), the cooling curve shows a single recalescence phenomenon again. The corresponding solidification microstructure can be divided into two types: the first is a mixture of B-rich phase + M23B6 + α-(Fe, Co, Ni, Mn) three phases, and the second is M23B6 + α-(Fe, Co, Ni, Mn) anomalous eutectic. Note that the type of primary phase transited for twice with the increase of undercooling: B-rich phase→M23B6 phase→α-(Fe, Co, Ni, Mn) phase. In addition, the orientation relationship of two eutectic phases in regular eutectic at low undercooling is consistent with that of two phases in anomalous eutectic at high undercooling.

参考文献

1 Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys[J]. Sci. Rep., 2014, 4: 6200
2 Jiao W N, Lu Y P, Cao Z Q, et al. Progress and prospect of eutectic high entropy alloys[J]. Spec. Cast. Nonferrous Alloys, 2022, 42: 265
  焦文娜, 卢一平, 曹志强 等. 共晶高熵合金的研究进展及展望[J]. 特种铸造及有色合金, 2022, 42: 265
3 Wu P H, Liu N, Yang W, et al. Microstructure and solidification behavior of multicomponent CoCrCu x FeMoNi high-entropy alloys[J]. Mater. Sci. Eng., 2015, A642: 142
4 Shukla S, Wang T H, Cotton S, et al. Hierarchical microstructure for improved fatigue properties in a eutectic high entropy alloy[J]. Scr. Mater., 2018, 156: 105
5 Wang M L, Lu Y P, Wang T M, et al. A novel bulk eutectic high-entropy alloy with outstanding as-cast specific yield strengths at elevated temperatures[J]. Scr. Mater., 2021, 204: 114132
6 Jiang H, Han K M, Gao X X, et al. A new strategy to design eutectic high-entropy alloys using simple mixture method[J]. Mater. Des., 2018, 142: 101
7 Jiang H, Qiao D X, Lu Y P, et al. Direct solidification of bulk ultrafine-microstructure eutectic high-entropy alloys with outstanding thermal stability[J]. Scr. Mater., 2019, 165: 145
8 Rogal ?, Morgiel J, ?wi?tek Z, et al. Microstructure and mechanical properties of the new Nb25Sc25Ti25Zr25 eutectic high entropy alloy[J]. Mater. Sci. Eng., 2016, A651: 590
9 Ye X C, Xiong J Y, Wu X, et al. A new infinite solid solution strategy to design eutectic high entropy alloys with B2 and BCC structure[J]. Scr. Mater., 2021, 199: 113886
10 Wang F J, Zhang Y, Chen G L, et al. Cooling rate and size effect on the microstructure and mechanical properties of AlCoCrFeNi high entropy alloy[J]. J. Eng. Mater. Technol., 2009, 131: 034501
11 Li J S, Jia W J, Wang J, et al. Enhanced mechanical properties of a CoCrFeNi high entropy alloy by supercooling method[J]. Mater. Des., 2016, 95: 183
12 Cao L G, Zhu L, Zhang L L, et al. Microstructure evolution and mechanical properties of rapid solidified AlCoCrFeNi2.1 eutectic high entropy alloy[J]. Chin. J. Mater. Res., 2019, 33: 650
  曹雷刚, 朱 琳, 张磊磊 等. 快速凝固AlCoCrFeNi2.1共晶高熵合金的微观组织演变和力学性能[J]. 材料研究学报, 2019, 33: 650
13 Zhao K, Wu S, Jiang S Y, et al. Microstructural refinement and anomalous eutectic structure induced by containerless solidification for high-entropy Fe-Co-Ni-Si-B alloys[J]. Intermetallics, 2020, 122: 106812
14 Yan P X, Chang J, Wang W L, et al. Eutectic growth kinetics and microscopic mechanical properties of rapidly solidified CoCrFeNiMo0.8 high entropy alloy[J]. Acta Mater., 2022, 237: 118149
15 Nassar A, Mullis A, Cochrane R, et al. Rapid solidification of AlCoCrFeNi2.1 high-entropy alloy[J]. J. Alloys Compd., 2022, 900: 163350
16 Guo Y N, Su H J, Zhou H T, et al. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting[J]. J. Mater. Sci. Technol., 2022, 111: 298
17 Su J, Chen S Q, Ding Z Y, et al. Solidification behavior of eutectic high entropy alloy fabricated by selective laser melting[J]. Chin. J. Nonferrous Met., 2022, 32: 658
  苏 捷, 陈仕奇, 丁正阳 等. 选区激光熔化共晶高熵合金凝固行为[J]. 中国有色金属学报, 2022, 32: 658
18 Liang X Y, Chen J, Yao Y H, et al. A novel nano-spaced coherent FCC1/FCC2 eutectic high entropy alloy[J]. Mater. Lett., 2023, 337: 133952
19 Qi T L, Li Y H, Takeuchi A, et al. Soft magnetic Fe25Co25Ni25(B, Si)25 high entropy bulk metallic glasses[J]. Intermetallics, 2015, 66: 8
20 Zhang Z Q, Song K K, Guo S, et al. Optimizing mechanical properties of Fe26.7Co26.7Ni26.7Si8.9B11 high entropy alloy by inducing hypoeutectic to quasi-duplex microstructural transition[J]. Sci. Rep., 2019, 9: 360
21 Fu K, Yin B J, Zhao Y Z, et al. Effect of boron content on microstructure evolution and crystallization behavior of Fe7(CoNi)93 - x B x (x = 15, 18, 21) eutectic high-entropy alloys[J]. Intermetallics, 2024, 165: 108131
22 Gao J R, Kao A, Bojarevics V, et al. Modeling of convection, temperature distribution and dendritic growth in glass-fluxed nickel melts[J]. J. Cryst. Growth, 2017, 471: 66
23 Wang Y Q, Shan C X, Wang L, et al. A new complex-regular eutectic in the Fe7(CoNiMn)93 - x B x high entropy alloys[J]. J. Mater. Res. Technol., 2024, 30: 4521
24 Yang C L, Liu F, Yang G C, et al. Structure evolution upon non-equilibrium solidification of bulk undercooled Fe-B system[J]. J. Cryst. Growth, 2009, 311: 404
25 Wang Y Q, Gao J R, Kolbe M, et al. Metastable solidification of hypereutectic Co2Si-CoSi composition: Microstructural studies and in-situ observations[J]. Acta Mater., 2018, 142: 172
26 Zhao R J, Wang Y Q, Gao J R, et al. In situ and ex situ studies of anomalous eutectic formation in undercooled Ni-Sn alloys[J]. Acta Mater., 2020, 197: 198
27 Miettinen J, Vassilev G. Thermodynamic description of ternary Fe-B-X systems. Part 2: Fe-B-Ni[J]. Arch. Metall. Mater., 2014, 59: 609
28 van Loo F J J, van Beek J A. Reactions and phase relations in the systems Fe-Ni-B and Fe-Co-B[J]. Z. Metallkd., 1989, 80: 245
29 Miettinen J, Lilova K, Vassilev G. Thermodynamic description of ternary Fe-B-X systems. Part 3: Fe-B-Mn[J]. Arch. Metall. Mater., 2014, 59: 1481
30 Jackson K A, Hunt J D. Lamellar and rod eutectic growth[A]. Dynamics of Curved Fronts[M]. Pittsburgh: Academic Press, 1988: 363
31 Wang Y Q, Gao J R, Shahani A J. Effects of Al substitution for Zn on the non-equilibrium solidification behavior of Zn-3Mg alloys[A]. Materials Processing Fundamentals 2020[M]. Cham: Springer, 2020: 23
32 Kattamis T Z, Flemings M C. Structure of undercooled Ni-Sn eutectic[J]. Metall. Trans., 1970, 1B: 1449
33 Wu Y, Piccone T J, Shiohara Y, et al. Dendritic growth of undercooled nickel-tin: Part III[J]. Metall. Trans., 1988, 19A: 1109
34 Jones B L. Growth mechanisms in undercooled eutectics[J]. Metall. Trans., 1971, 2: 2950
35 Tewari S N. Effect of undercooling on the microstructure of Ni-35 at. pct Mo (eutectic) and Ni-38 at. pct Mo (hypereutectic) alloys[J]. Metall. Trans., 1987, 18A: 525
36 Zhao S, Li J F, Liu L, et al. Eutectic growth from cellular to dendritic form in the undercooled Ag-Cu eutectic alloy melt[J]. J. Cryst. Growth, 2009, 311: 1387
37 Liu L, Li J F, Zhou Y H. Solidification interface morphology pattern in the undercooled Co-24.0at.% Sn eutectic melt[J]. Acta Mater., 2011, 59: 5558
38 Goetzinger R, Barth M, Herlach D M. Mechanism of formation of the anomalous eutectic structure in rapidly solidified Ni-Si, Co-Sb and Ni-Al-Ti alloys[J]. Acta Metall., 1998, 46: 1647
39 Lai C, Wang H F, Pu Q, et al. Phase selection and re-melting-induced anomalous eutectics in undercooled Ni-38 wt% Si alloys[J]. J. Mater. Sci., 2016, 51: 10990
文章导航

/