增材制造AlSi10Mg合金存在显著的残余应力,对零件的形状尺寸精度、服役安全性和抗腐蚀性能等产生不利影响。在实际应用中,对残余应力敏感的应用需采用去应力退火以消除残余应力。然而,目前对增材制造AlSi10Mg合金退火后力学特性的理解还停留在宏观层面。为了更深入地揭示其微观力学行为与内在机制,本工作利用同步辐射X射线衍射技术,对合金进行原位变形研究,分析Al和Si相的晶格应变应力演化,明确各物相对合金加工硬化率的具体贡献,并对位错密度的演变进行了量化分析,从而阐明了退火热处理对增材制造AlSi10Mg合金载荷传递行为与位错行为的影响。
关键词: 同步辐射X射线衍射; 原位变形; 增材制造; AlSi10Mg合金; 热处理
张星星 , LUTZ Andreas , 甘为民 , MAAWAD Emad , KRIELE Armin . 退火热处理对增材制造AlSi10Mg合金宏观和微观变形行为的影响[J]. 金属学报, 2024 , 60(8) : 1091 -1099 . DOI: 10.11900/0412.1961.2024.00116
The additively manufactured AlSi10Mg alloy demonstrates considerable residual stresses, adversely affecting the dimensional accuracy, operational safety, and corrosion resistance of the parts. In practical applications, stress relief annealing is necessary to eliminate residual stresses in residual stress-sensitive applications. However, the current understanding of the mechanical properties of the additively manufactured AlSi10Mg alloy after annealing is still limited to the macroscopic level. To further investigate the micromechanical behavior and intrinsic mechanisms of the alloy, this study employed synchrotron X-ray diffraction technology to conduct in situ deformation analysis. This study thoroughly examined the lattice strain and stress evolutions of the Al and Si phases and clarified the individual contribution of each phase to the strain hardening rate of the alloy. In addition, this study quantitatively assessed the evolution of dislocation density and elucidated the influences of annealing heat treatment on the load transfer and dislocation behavior of the additively manufactured AlSi10Mg alloy.
| 1 | Aboulkhair N T, Simonelli M, Parry L, et al. 3D printing of aluminium alloys: Additive manufacturing of aluminium alloys using selective laser melting [J]. Prog. Mater Sci., 2019, 106: 100578 |
| 2 | Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys [J]. Nature, 2017, 549: 365 |
| 3 | Fiocchi J, Tuissi A, Biffi C A. Heat treatment of aluminium alloys produced by laser powder bed fusion: A review [J]. Mater. Des., 2021, 204: 109651 |
| 4 | Zhao L, Macías J G S, Dolimont A, et al. Comparison of residual stresses obtained by the crack compliance method for parts produced by different metal additive manufacturing techniques and after friction stir processing [J]. Addit. Manuf., 2020, 36: 101499 |
| 5 | Schr?der J, Evans A, Mishurova T, et al. Diffraction-based residual stress characterization in laser additive manufacturing of metals [J]. Metals, 2021, 11: 1830 |
| 6 | Fang Z C, Wu Z L, Huang C G, et al. Review on residual stress in selective laser melting additive manufacturing of alloy parts [J]. Opt. Laser Technol., 2020, 129: 106283 |
| 7 | Laleh M, Sadeghi E, Revilla R I, et al. Heat treatment for metal additive manufacturing [J]. Prog. Mater Sci., 2023, 133: 101051 |
| 8 | Huang N, Luo Q X, Bartles D L, et al. Effect of heat treatment on microstructure and mechanical properties of AlSi10Mg fabricated using laser powder bed fusion [J]. Mater. Sci. Eng., 2024, A895: 146228 |
| 9 | Takata N, Kodaira H, Sekizawa K, et al. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments [J]. Mater. Sci. Eng., 2017, A704: 218 |
| 10 | Chen S Q, Tan Q Y, Gao W Q, et al. Effect of heat treatment on the anisotropy in mechanical properties of selective laser melted AlSi10Mg [J]. Mater. Sci. Eng., 2022, A858: 144130 |
| 11 | Zhang C C, Zhu H H, Liao H L, et al. Effect of heat treatments on fatigue property of selective laser melting AlSi10Mg [J]. Int. J. Fatigue, 2018, 116: 513 |
| 12 | Tridello A, Fiocchi J, Biffi C A, et al. Influence of the annealing and defects on the VHCF behavior of an SLM AlSi10Mg alloy [J]. Fatigue Fract. Eng. Mater. Struct., 2019, 42: 2794 |
| 13 | Xie Q G, Lian J H, Sidor J J, et al. Crystallographic orientation and spatially resolved damage in a dispersion-hardened Al alloy [J]. Acta Mater., 2020, 193: 138 |
| 14 | Zhang X X, Lutz A, Andr? H, et al. Evolution of microscopic strains, stresses, and dislocation density during in-situ tensile loading of additively manufactured AlSi10Mg alloy [J]. Int. J. Plast., 2021, 139: 102946 |
| 15 | Takata N, Liu M L, Hirata M, et al. Microstructural origins of high strength of Al-Si alloy manufactured by laser powder bed fusion: In-situ synchrotron radiation X-ray diffraction approach [J]. J. Mater. Sci. Technol., 2024, 178: 80 |
| 16 | Li C, Zhang W X, Yang H O, et al. Microstructural origin of high strength and high strain hardening capability of a laser powder bed fused AlSi10Mg alloy [J]. J. Mater. Sci. Technol., 2024, 197: 194 |
| 17 | Hong Y Y, Gao J, Liu X Q, et al. Investigation of the high-temperature fatigue mechanism related to altered local short-range order in AL6XN austenitic stainless steel [J]. Mater. Des., 2023, 236: 112504 |
| 18 | Masumura T, Inami K, Matsuda K, et al. Quantitative evaluation of dislocation density in as-quenched martensite with tetragonality by X-ray line profile analysis in a medium-carbon steel [J]. Acta Mater., 2022, 234: 118052 |
| 19 | Ribárik G, Jóni B, Ungár T. Global optimum of microstructure parameters in the CMWP line-profile-analysis method by combining Marquardt-Levenberg and Monte-Carlo procedures [J]. J. Mater. Sci. Technol., 2019, 35: 1508 |
| 20 | Zhang X X, Bauer P P, Lutz A, et al. Microplasticity and macroplasticity behavior of additively manufactured Al-Mg-Sc-Zr alloys: In-situ experiment and modeling [J]. Int. J. Plast., 2023, 166: 103659 |
| 21 | Zhang X X, Lutz A, Andr? H, et al. An additively manufactured and direct-aged AlSi3.5Mg2.5 alloy with superior strength and ductility: Micromechanical mechanisms [J]. Int. J. Plast., 2021, 146: 103083 |
| 22 | Li Y, Yu J Y, Li S L, et al. The influence of post-aging treatment on the microstructure and micromechanical behaviors of additively manufactured maraging steel investigated by in situ high-energy X-ray diffraction [J]. J. Mater. Sci. Technol., 2024, 200: 1 |
| 23 | Zhang X X, Knoop D, Andr? H, et al. Multiscale constitutive modeling of additively manufactured Al-Si-Mg alloys based on measured phase stresses and dislocation density [J]. Int. J. Plast., 2021, 140: 102972 |
| 24 | Harjo S, Tsuchida N, Abe J, et al. Martensite phase stress and the strengthening mechanism in TRIP steel by neutron diffraction [J]. Sci. Rep., 2017, 7: 15149 |
| 25 | Zhang X X, Lutz A, Andr? H, et al. Strain hardening behavior of additively manufactured and annealed AlSi3.5Mg2.5 alloy [J]. J. Alloys Compd., 2022, 898: 162890 |
| 26 | Santos Macías J G, Douillard T, Zhao L, et al. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg [J]. Acta Mater., 2020, 201: 231 |
| 27 | Dan C Y, Cui Y C, Wu Y, et al. Achieving ultrahigh fatigue resistance in AlSi10Mg alloy by additive manufacturing [J]. Nat. Mater., 2023, 22: 1182 |
/
| 〈 |
|
〉 |