研究论文

先进镍基粉末高温合金FGH4108在不同应力条件下的蠕变行为

  • 李新宇 ,
  • 白佳铭 ,
  • 张浩鹏 ,
  • 李晓鲲 ,
  • 贾建 ,
  • 刘常升 ,
  • 刘建涛 ,
  • 张义文
展开
  • 1 东北大学 材料科学与工程学院 沈阳 110819
    2 钢铁研究总院 高温材料研究所 北京 100081
    3 北京钢研高纳科技股份有限公司 北京 100081
李新宇,男,1991年生,博士生
刘建涛,ljtsuperalloys@sina.com,主要从事粉末高温合金的研究;
张义文,yiwen64@cisri.cn,主要从事粉末高温合金的研究

收稿日期: 2023-04-06

  修回日期: 2023-11-03

  网络出版日期: 2023-12-25

基金资助

国家科技重大专项项目(2017-VI-0008-0078);北京钢研高纳科技股份有限公司项目(KZKJ02-GN0J-22012)

Creep Behavior of Advanced Powder Metallurgy Nickel-Based Superalloys FGH4108 Under Different Stress Conditions

  • LI Xinyu ,
  • BAI Jiaming ,
  • ZHANG Haopeng ,
  • LI Xiaokun ,
  • JIA Jian ,
  • LIU Changsheng ,
  • LIU Jiantao ,
  • ZHANG Yiwen
Expand
  • 1 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2 High Temperature Material Research Institute, Central Iron and Steel Research Institute, Beijing 100081, China
    3 Gaona Aero Material Co. Ltd., Beijing 100081, China
LIU Jiantao, professor, Tel: (010)62182925, E-mail: ljtsuperalloys@sina.com;
ZHANG Yiwen, professor, Tel: (010)62186736, E-mail: yiwen64@cisri.cn

Received date: 2023-04-06

  Revised date: 2023-11-03

  Online published: 2023-12-25

Supported by

National Science and Technology Major Project(2017-VI-0008-0078);Project of Gaona Aero Material Co. Ltd(KZKJ02-GN0J-22012)

摘要

为深入了解双组织结构的FGH4108合金的蠕变特性,通过2种不同晶粒尺寸组织研究了合金在700 ℃不同应力下的蠕变行为。利用SEM和TEM研究不同应力下2种晶粒组织的蠕变变形机制和断裂模式,分析应力对蠕变变形和断裂的影响。结果表明,在700 ℃条件下,粗晶组织在780 MPa蠕变应力下的变形组织主要为孤立层错和微孪晶,随着应力提升至900 MPa,主要的变形组织转变为扩展层错和微孪晶;对于细晶组织,在780~900 MPa蠕变应力范围内主要的变形组织为扩展层错和微孪晶。在2种尺寸的晶粒组织中,晶界对最小蠕变速率的促进作用随着加载应力的增加而降低。分析表明,合金的高应力敏感性是导致应力增加后在变形过程中容易产生孪生的原因。另外,随着蠕变应力增加,粗晶组织的沿晶断裂倾向减小,而对于细晶组织则反之。

本文引用格式

李新宇 , 白佳铭 , 张浩鹏 , 李晓鲲 , 贾建 , 刘常升 , 刘建涛 , 张义文 . 先进镍基粉末高温合金FGH4108在不同应力条件下的蠕变行为[J]. 金属学报, 2025 , 61(5) : 757 -769 . DOI: 10.11900/0412.1961.2023.00153

Abstract

Turbine discs, manufactured using powder metallurgy nickel-based superalloys, serve as critical hot-end components in aviation engines. Considering that the disc rim and hub has to function under different temperatures and stresses, their dual microstructure had been paid close attention. In this study, the coarse- and fine-grained microstructures were obtained by controlling the solution treatment temperature, and the creep behavior of the superalloy at 700 oC and under various stresses was investigated. The effect of stress on the creep deformation mechanism and fracture behavior of the alloy was investigated via SEM and TEM. In the coarse-grained microstructure, the creep deformation mechanism at 780 MPa was primarily isolated by stacking faults and microtwin shearing, while the stress increased to 900 MPa, the extended stacking fault shearing and microtwinning jointly dominated creep deformation. Nevertheless, within the stress range of 780-900 MPa, the creep deformation mechanism remained consistent in the fine-grained structure, which was characterized by the coexistence of extended stacking fault shearing and microtwinning. In addition, this study indicated that the grain boundaries exhibited a diminishing promotion effect on the minimum creep rate as the applied stress increased for both grain microstructures. The high stress sensitivity of the experimental alloy resulted in the occurrence of twinning with elevated stress levels. This phenomenon accelerated plastic deformation, resulting in an increased creep rate. Moreover, the creep fracture source zone was predominantly an intergranular fracture, whereas the propagation region was predominantly a transgranular fracture in both grain microstructures. The tendency for intergranular fracture in coarse-grained microstructures decreased with the increase in the creep stress level, vice versa was observed in fine-grained microstructures.

参考文献

1 Reed R C, Mottura A, Crudden D J. Alloys-by-design: Towards optimization of compositions of nickel-based superalloys [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Warrendale: The Minerals, Metals & Materials Society, 2016: 15
2 Bai J M, Zhang H P, Li X Y, et al. Evolution of creep rupture mechanism in advanced powder metallurgy superalloys with tantalum addition [J]. J. Alloys Compd., 2022, 925: 166713
3 Liu P, Zhang R, Yuan Y, et al. Microstructural evolution of a Ni-Co based superalloy during hot compression at γ′ sub-/super-solvus temperatures [J]. J. Mater. Sci. Technol., 2021, 77: 66
4 Panella M, Signor L, Cormier J, et al. Experimental and simulation study of the effect of precipitation distribution and grain size on the AD730TM Ni-based polycrystalline superalloy tensile behavior [A]. Superalloys 2020: Proceedings of the 14th International Symposium on Superalloys [C]. Cham: Springer, 2020: 570
5 Zhang B Y, Wang Z T, Yu H, et al. Microstructural origin and control mechanism of the mixed grain structure in Ni-based superalloys [J]. J. Alloys Compd., 2022, 900: 163515
6 Gayda J, Gabb T P, Kantzos P T. The effect of dual microstructure heat treatment on an advanced nickel-base disk alloy [A]. Superalloys 2004: Proceedings of the 10th International Symposium on Superalloys [C]. Warrendale: The Minerals, Metals & Materials Society, 2004: 323
7 Gabb T P, Kantzos P T, Telesman J, et al. Fatigue resistance of the grain size transition zone in a dual microstructure superalloy disk [J]. Int. J. Fatigue, 2011, 33: 414
8 Long H B, Liu Y N, Kong D L, et al. Shearing mechanisms of stacking fault and anti-phase-boundary forming dislocation pairs in the γ′ phase in Ni-based single crystal superalloy [J]. J. Alloys Compd., 2017, 724: 287
9 Xu L, Sun C Q, Cui C Y, et al. Effects of microstructure on the creep properties of a new Ni-Co base superalloy [J]. Mater. Sci. Eng., 2016, A678: 110
10 Ru Y, Li S S, Zhou J, et al. Dislocation network with pair-coupling structure in {111} γ/γ′ interface of Ni-based single crystal superalloy [J]. Sci. Rep., 2016, 6: 29941
11 Rai R K, Sahu J K, Pramanick A, et al. Creep deformation micro-mechanisms of CM 247 DS LC Ni-base superalloy under relevant service condition [J]. Mater. Charact., 2019, 150: 155
12 Jia C L, Li Y, Zhang F L, et al. The creep behavior of a disk superalloy under different stress conditions [J]. Met. Powder Rep., 2018, 73: 94
13 Dong K X, Yuan C, Gao S, et al. Creep properties of a powder metallurgy disk superalloy at 700 oC [J]. J. Mater. Res., 2017, 32: 624
14 Peng Z C, Liu P Y, Wang X Q, et al. Creep behavior of FGH96 superalloy at different service conditions [J]. Acta Metall. Sin., 2022, 58: 673
  彭子超, 刘培元, 王旭青 等. 不同服役条件下FGH96合金的蠕变特征 [J]. 金属学报, 2022, 58: 673
15 Liu F, Wang Z X, Tan L M, et al. Creep behaviors of fine-grained Ni-base powder metallurgy superalloys at elevated temperatures [J]. J. Alloys Compd., 2021, 867: 158865
16 Thébaud L, Villechaise P, Crozet C, et al. Is there an optimal grain size for creep resistance in Ni-based disk superalloys? [J]. Mater. Sci. Eng., 2018, A716: 274
17 Sun F, Gu Y F, Yan J B, et al. Dislocation motion in a Ni-Fe-based superalloy during creep-rupture beyond 700 oC [J]. Mater. Lett., 2015, 159: 241
18 Mannan S L, Rodriguez P. Effect of grain size on creep rate in type 316 stainless steel at 873 and 973 K [J]. Met. Sci., 1983, 17: 63
19 Fang T T, Murty K L. Grain-size-dependent creep of stainless steel [J]. Mater. Sci. Eng., 1983, 61: L7
20 Kim Y K, Kim D, Kim H K, et al. An intermediate temperature creep model for Ni-based superalloys [J]. Int. J. Plasticity, 2016, 79: 153
21 Li X Y, Zhang H P, Bai J M, et al. The evolution of γ′ precipitates and hardness response of a novel PM Ni-based superalloy during thermal exposure [J]. J. Alloys Compd., 2023, 942: 168757
22 Yue Q Z, Liu L, Yang W C, et al. Stress dependence of the creep behaviors and mechanisms of a third-generation Ni-based single crystal superalloy [J]. J. Mater. Sci. Technol., 2019, 35: 752
23 Murakumo T, Kobayashi T, Koizumi Y, et al. Creep behaviour of Ni-base single-crystal superalloys with various γ′ volume fraction [J]. Acta Mater., 2004, 52: 3737
24 Tian T, Hao Z B, Ge C C, et al. Effects of stress and temperature on creep behavior of a new third-generation powder metallurgy superalloy FGH100L [J]. Mater. Sci. Eng., 2020, A776: 139007
25 Guo J T, Ranucci D, Picco E, et al. An investigation on the creep and fracture behavior of cast nickel-base superalloy IN738LC [J]. Metall. Trans., 1983, 14A: 2329
26 Nategh S, Sajjadi S A. Dislocation network formation during creep in Ni-base superalloy GTD-111 [J]. Mater. Sci. Eng., 2003, A339: 103
27 Balikci E, Raman A, Mirshams R A. Tensile strengthening in the nickel-base superalloy IN738LC [J]. J. Mater. Eng. Perform., 2000, 9: 324
28 Zhang X, Jin T, Zhao N R, et al. Effect of strain rate on the tensile behavior of a single crystal nickel-base superalloy [J]. Mater. Sci. Eng., 2008, A492: 364
29 Guan S, Cui C Y, Yuan Y, et al. The role of phosphorus in a newly developed Ni-Fe-Cr-based wrought superalloy [J]. Mater. Sci. Eng., 2016, A662: 275
30 Cui L Q, Su H H, Yu J J, et al. The creep deformation and fracture behaviors of nickel-base superalloy M951G at 900 oC [J]. Mater. Sci. Eng., 2017, A707: 383
文章导航

/